Preparation of Li1.03Mn1.97O4 and Li1.06Mn1.94O4 by the Polymer Precursor Method and X-ray, Neutron Diffraction and Electrochemical Studies

被引:22
作者
Reddy, M. V. [1 ]
Raju, M. J. Silvister [1 ]
Sharma, N. [2 ]
Quan, P. Y. [1 ,3 ]
Nowshad, S. H. [1 ,3 ]
Emmanuel, H. E. -C. [1 ,3 ]
Peterson, V. K. [2 ]
Chowdari, B. V. R. [1 ]
机构
[1] Natl Univ Singapore, Dept Phys, Singapore 117542, Singapore
[2] Australian Nucl Sci & Technol Org, Bragg Inst, Kirrawee Dc, NSW 2232, Australia
[3] NUS High Sch Math & Sci, Singapore 129957, Singapore
关键词
LITHIUM-ION BATTERIES; IMPROVED CAPACITY RETENTION; EMULSION DRYING METHOD; MN-O SPINEL; LI-ION; CATHODE MATERIALS; POSITIVE ELECTRODE; MANGANESE OXIDE; PERFORMANCE; LIMN2O4;
D O I
10.1149/2.074111jes
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The compounds, Li1.03Mn1.97O4 and Li1.06Mn1.94O4 were prepared by the polymer precursor method followed by heat treatment at 650 degrees C for 6 hours in air. X-ray and neutron diffraction, scanning electron microscopy, and the Brunauer-Emmett-Teller surface area and density determination techniques were used to characterise the compounds. The lattice parameters obtained using neutron diffraction data of Li1.03Mn1.97O4 and Li1.06Mn1.94O4 are smaller than the parent LiMn2O4 at a = 8.20717(17) and 8.22899(13) A degrees, respectively. Cyclic voltammetry studies were carried out in the potential range of 3.5-4.4V at scan rate of 0.058 mV/sec. Li-doped LiMn2O4 showed the main cathodic and anodic redox peaks at similar to 3.9/4.0 and similar to 4.1/4.15V, respectively. The reversible charge capacities of Li1.03Mn1.97O4 with an applied current rate of 360 mA g(-1) at the end of 2(nd) and 230(th) cycle are 88 and 83 (+/- 3) mAh g(-1), respectively. At a current rate of 600 mA g(-1) these charge capacities are 67 and 61 (+/- 3) mAh g(-1), respectively. Li1.06Mn1.94O4 shows a capacity of 64 and 62 (+/- 3) mAh g(-1) at the end of 2(nd) and 100(th) cycles, respectively, at a current rate of 360 mA g(-1). (C) 2011 The Electrochemical Society. [DOI: 10.1149/2.074111jes] All rights reserved.
引用
收藏
页码:A1231 / A1236
页数:6
相关论文
共 44 条
[11]   Positive Electrode Materials for Li-Ion and Li-Batteries [J].
Ellis, Brian L. ;
Lee, Kyu Tae ;
Nazar, Linda F. .
CHEMISTRY OF MATERIALS, 2010, 22 (03) :691-714
[12]   Recent developments in cathode materials for lithium ion batteries [J].
Fergus, Jeffrey W. .
JOURNAL OF POWER SOURCES, 2010, 195 (04) :939-954
[13]   IMPROVED CAPACITY RETENTION IN RECHARGEABLE 4V LITHIUM LITHIUM MANGANESE OXIDE (SPINEL) CELLS [J].
GUMMOW, RJ ;
DEKOCK, A ;
THACKERAY, MM .
SOLID STATE IONICS, 1994, 69 (01) :59-67
[14]   LI METAL-FREE RECHARGEABLE LIMN2O4/CARBON CELLS - THEIR UNDERSTANDING AND OPTIMIZATION [J].
GUYOMARD, D ;
TARASCON, JM .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1992, 139 (04) :937-948
[15]   Synthesis of Ordered Mesoporous Li-Mn-O Spinel as a Positive Electrode for Rechargeable Lithium Batteries [J].
Jiao, Feng ;
Bao, Jianli ;
Hill, Adrian H. ;
Bruce, Peter G. .
ANGEWANDTE CHEMIE-INTERNATIONAL EDITION, 2008, 47 (50) :9711-9716
[16]   Electrochemical characteristics and manganese dissolution of spinel Li1.05M0.2Mn1.75O4 (M = Al, Co, and Cr) cathode for rechargeable lithium ion batteries [J].
Komaba, S ;
Sasaki, T ;
Miki, Y ;
Chikui, M ;
Sasaki, T ;
Kumagai, N .
ELECTROCHEMISTRY, 2003, 71 (12) :1236-1239
[17]  
Larson A.C., 1994, Los Alamos National Laboratory Report LAUR 86-748, P86
[18]  
Li GH, 1996, J ELECTROCHEM SOC, V143, P178, DOI 10.1149/1.1836405
[19]   Synthesis and Characterization of Li(Co0.5Ni0.5)PO4 Cathode for Li-Ion Aqueous Battery Applications [J].
Minakshi, Manickam ;
Sharma, Neeraj ;
Ralph, David ;
Appadoo, Dominique ;
Nallathamby, Kalaiselvi .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2011, 14 (06) :A86-A89
[20]   Enhanced structural stability and cyclability of Al-doped LiMn2O4 spinel synthesized by the emulsion drying method [J].
Myung, ST ;
Komaba, S ;
Kumagai, N .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2001, 148 (05) :A482-A489