Rolling contact fatigue behaviors of 25CrNi2MoV steel combined treated by discrete laser surface hardening and ultrasonic surface rolling

被引:27
作者
Hu, Xiongfeng [1 ,2 ]
Qu, Shengguan [1 ]
Chen, Zengtao [2 ]
Zhang, Peng [3 ]
Lu, Zhiyuan [3 ]
Lai, Fuqiang [4 ]
Duan, Chenfeng [1 ]
Li, Xiaoqiang [1 ]
机构
[1] South China Univ Technol, Sch Mech & Automot Engn, Guangdong Key Lab Adv Metall Mat Proc, Guangzhou 510640, Peoples R China
[2] Univ Alberta, Dept Mech Engn, Edmonton, AB T6G 1H9, Canada
[3] Inner Mongolia First Machinery Grp Co Ltd, Baotou 014032, Peoples R China
[4] Fuzhou Univ, Sch Mech Engn & Automat, Qishan Campus, Fuzhou 350108, Peoples R China
关键词
Discrete laser surface hardening; Ultrasonic surface rolling; Spot density; Rolling contact fatigue; Failure mode; RESIDUAL-STRESS; HEAT-TREATMENT; CRACK-GROWTH; WEAR-RESISTANCE; TRANSFORMATION; PROPAGATION; INITIATION; EVOLUTION;
D O I
10.1016/j.optlastec.2022.108370
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
DLSH) and ultrasonic surface rolling (USR) on the material properties (surface roughness, microstructures, microhardness and residual stress) and rolling contact fatigue (RCF) behaviors of 25CrNi2MoV steel were investigated. A continuous-wave diode laser with a maximum output power of 2 kW was used to fabricate four different types of DLSH density samples with a size of F42 mm x 6 mm. The results showed that the combined USR treatment improved the surface quality (including roughness and oxide layer) of the DLSH samples, increased surface hardness, and obtained a beneficial surface compressive residual stress of up to 1240 +/- 91 MPa. The severe plastic deformation introduced a gradient nano/ultrafine grain layer on both hardened zone (HZ) and substrate zone (SZ) surfaces of DLSH group samples, and the deformation depth decreased with the increase of DLSH density within 24.3-65.3 mu m. Accumulation of plastic deformation below and around the HZ edge resulted in a gradient drop in hardness from HZ to SZ, which helps to relieve the occurrence of stress concentration at the surface HZ edge. Benefit from favorable factors, the RCF life of combined treated samples with hardened spot densities of 28%, 50%, 79% and 100% was increased by 82.2%, 123%, 143.6% and 171.9% compared with that of the untreated samples, respectively. After USR treatment, the failure mode within the SZ changed from spalling to delamination, but it remained as spalling failure within the HZ.
引用
收藏
页数:15
相关论文
共 50 条
[41]   Rolling contact fatigue property of low-temperature bainite in surface layer of a low carbon steel [J].
Zhang, P. ;
Zhang, F. C. ;
Yan, Z. G. ;
Wang, T. S. ;
Qian, L. H. .
ADVANCED MATERIAL SCIENCE AND TECHNOLOGY, PTS 1 AND 2, 2011, 675-677 :585-588
[42]   Study of Inner Micro Cracks on Rolling Contact Fatigue of Bearing Steels Using Ultrasonic Nano-Crystalline Surface Modification [J].
Lee, Chang-Soon ;
Cho, In-Shik ;
Pyoun, Young-Shik ;
Park, In-Gyu .
FRACTURE AND STRENGTH OF SOLIDS VII, PTS 1 AND 2, 2011, 462-463 :979-984
[43]   Improved rolling contact fatigue performance of selective electron beam melted Ti6A14V with the as-built surface using induction-heating assisted ultrasonic surface rolling process [J].
Liu, Zhongqiang ;
Liu, Xiao ;
Liu, Ruiping ;
Xiao, Zhiyu ;
Sanderson, Joseph .
APPLIED SURFACE SCIENCE, 2023, 617
[44]   Influence of Ultrasonic Surface Rolling on Fatigue Behavior of 2D12 Aluminum Alloy [J].
Cong Jiahui ;
Wang Lei ;
Xu Yongzhen ;
Hui Li .
RARE METAL MATERIALS AND ENGINEERING, 2022, 51 (01) :113-118
[45]   Thermal fatigue resistance of H13 steel treated by selective laser surface melting and CrNi alloying [J].
Tong, Xin ;
Dai, Ming-jiang ;
Zhang, Zhi-hui .
APPLIED SURFACE SCIENCE, 2013, 271 :373-380
[46]   Influence of surface integrity on the fatigue performance of TiB2/Al composite treated by ultrasonic deep rolling: Experiments and simulations [J].
Li, Yugang ;
Geng, Jiwei ;
Wang, Zhiping ;
Song, Cunfeng ;
Zhang, Chengcheng ;
Chen, Dong ;
Wang, Haowei .
COMPOSITES PART B-ENGINEERING, 2024, 271
[47]   Comparison of Effects of Laser, Ultrasonic, and Combined Laser-Ultrasonic Hardening Treatments on Surface Properties of AISI 1045 Steel Parts [J].
Lesyk, Dmytro ;
Alnusirat, Walid ;
Martinez, Silvia ;
Mordyuk, Bohdan ;
Dzhemelinskyi, Vitaliy .
ADVANCED MANUFACTURING PROCESSES III, INTERPARTNER-2021, 2022, :313-322
[48]   The influence of ultrasonic surface rolling on the fatigue and wear properties of 23-8N engine valve steel [J].
Lai, Fuqiang ;
Qu, Shengguan ;
Lewis, Roger ;
Slatter, Tom ;
Fu, Wenlan ;
Li, Xiaoqiang .
INTERNATIONAL JOURNAL OF FATIGUE, 2019, 125 :299-313
[49]   Surface Integrity and Fretting Wear Behavior of Modified 17Cr2Ni2MoVNb Steel by Gas Carburizing Combined with Ultrasonic Surface Rolling [J].
Zhang, Yalong ;
Jiao, Chenjia ;
Hu, Yuhan ;
Shi, Dapeng ;
Wu, Luji ;
Liu, Le ;
Ji, Vincent ;
Xia, Yanfei .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2025,
[50]   Effect of residual stress induced by ultrasonic surface rolling on fretting fatigue behaviors of Ti-6Al-4V alloy [J].
Fan, Kaifa ;
Liu, Daoxin ;
Zhang, Xiaohua ;
Liu, Dan ;
Zhao, Weidong ;
Yang, Jing ;
Ma, Amin ;
Li, Mengyao ;
Qi, Yanan ;
Xiang, Junfeng ;
Wahab, Magd Abdel .
ENGINEERING FRACTURE MECHANICS, 2022, 259