Microstructural extremes and the transition from fatigue crack initiation to small crack growth in a polycrystalline nickel-base superalloy

被引:169
作者
Miao, Jiashi [1 ]
Pollock, Tresa M. [2 ]
Jones, J. Wayne [1 ]
机构
[1] Univ Michigan, Dept Mat Sci & Engn, Ann Arbor, MI 48109 USA
[2] Univ Calif Santa Barbara, Dept Mat, Santa Barbara, CA 93106 USA
关键词
Fatigue crack initiation; Superalloy; Small crack growth; Grain cluster; Sigma 3 Twin boundary; GRAIN-BOUNDARIES; CYCLE FATIGUE; DEFORMATION; MECHANISMS; EXTRUSIONS; INTRUSIONS; BEHAVIOR; FEATURES; WASPALOY;
D O I
10.1016/j.actamat.2012.01.049
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The fatigue behavior of the nickel-base superalloy Rene 88 DT has been investigated at room temperature with fully reversed loading in an ultrasonic fatigue apparatus operating at a frequency close to 20 kHz. A characterization protocol based on the electron backscatter diffraction technique has been developed to identify the combination of microstructural features within crack initiation sites and surrounding neighborhoods that leads to the transition from initiation to early small crack growth. Surface grains that were more than three times the average grain size, that were favorably oriented for cyclic slip localization and that also contained Sigma 3 twin boundaries inclined to the loading axis were most favorable for fatigue crack initiation. Fatigue cracks subsequently grew in grain clusters within which grains are misoriented by less than 20 degrees relative to the initiation grains. More highly misoriented neighboring grains resulted in crack arrest. The material characteristics that promote crack initiation and small crack growth exist only at the extreme tails of the microstructural distributions. The implications for modeling of fatigue life and fatigue life variability are discussed. (C) 2012 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:2840 / 2854
页数:15
相关论文
共 40 条
[1]  
Antolovich S.D., 1989, SUPERALLOYS SUPERCOM, P363
[2]   Twin boundaries as crack nucleation sites [J].
Blochwitz, C ;
Tirschler, W .
CRYSTAL RESEARCH AND TECHNOLOGY, 2005, 40 (1-2) :32-41
[3]   SHORT FATIGUE-CRACK PATH DETERMINANTS IN POLYCRYSTALLINE NI-BASE SUPERALLOYS [J].
BOYDLEE, A ;
KING, JE .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1994, 17 (01) :1-14
[4]   STRUCTURE OF HIGH-ANGLE GRAIN BOUNDARIES [J].
BRANDON, DG .
ACTA METALLURGICA, 1966, 14 (11) :1479-&
[5]  
Brogdon ML, 2008, SUPERALLOYS 2008, P583, DOI 10.7449/2008/Superalloys_2008_583_588
[6]  
Caton MJ, 2004, SUPERALLOYS 2004, P305, DOI 10.7449/2004/Superalloys_2004_305_312
[7]   Fatigue crack initiation in WASPALOY at 20 °C [J].
Davidson, D. L. ;
Tryon, R. G. ;
Oja, M. ;
Matthews, R. ;
Chandran, K. S. Ravi .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2007, 38A (13) :2214-2225
[8]   A MODEL OF EXTRUSIONS AND INTRUSIONS IN FATIGUED METALS .1. POINT-DEFECT PRODUCTION AND THE GROWTH OF EXTRUSIONS [J].
ESSMANN, U ;
GOSELE, U ;
MUGHRABI, H .
PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES, 1981, 44 (02) :405-426
[9]   MONITORING FATIGUE OF A NICKEL-BASE SUPERALLOY AT POSITIVE AND NEGATIVE STRESS RATIOS USING AN OPTICAL-SYSTEM [J].
HEALY, JC ;
GRABOWSKI, L ;
BEEVERS, CJ .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1992, 15 (03) :309-321
[10]   CRACK INITIATION DURING HIGH CYCLE FATIGUE OF AN AUSTENITIC STEEL [J].
HEINZ, A ;
NEUMANN, P .
ACTA METALLURGICA ET MATERIALIA, 1990, 38 (10) :1933-1940