Microstructure, kinetic analysis and hardness of Sn-Ag-Cu-1 wt% nano-ZrO2 composite solder on OSP-Cu pads

被引:85
作者
Gain, Asit Kumar [1 ]
Fouzder, Tama [1 ]
Chan, Y. C. [1 ]
Yung, Winco K. C. [2 ]
机构
[1] City Univ Hong Kong, Dept Elect Engn, Kowloon Tong, Hong Kong, Peoples R China
[2] Hong Kong Polytech Univ, Dept Ind & Syst Engn, Kowloon, Hong Kong, Peoples R China
关键词
Nano doping; Microstructure; Kinetics analysis; Hardness; MECHANICAL-PROPERTIES; INTERFACIAL REACTIONS; SHEAR-STRENGTH; SN-9ZN SOLDER; RARE-EARTH; SN; ALLOY; CREEP; WETTABILITY; JOINT;
D O I
10.1016/j.jallcom.2010.12.048
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Nano-sized, nonreacting, noncoarsening ZrO2 particle-reinforced Sn-Ag-Cu composite solders were prepared by mechanically dispersing ZrO2 nano-particles into Sn-Ag-Cu solder and the interfacial morphology between the solder and organic solderability preservative (OSP)-Cu pads were characterized metallographically. At their interfaces, island-shaped Cu6Sn5 and Cu3Sn intermetallic compound (IMC) layers were found in solder joints with and without the ZrO2 particles and the IMC layer thickness was substantially increased with reaction time and temperature. In the solder ball region, needle-shaped Ag3Sn and spherically-shaped Cu6Sn5 IMC particles were found to be uniformly distributed in the beta-Sn matrix. However, after the addition of ZrO2 nano-particles, Ag3Sn and Cu6Sn5 IMC particles appeared with a fine microstructure and retarded the growth rate of the IMC layers at their interfaces. From a kinetic analysis, the calculated activation energies for the total (Cu6Sn5+Cu3Sn) IMC layers for Sn-Ag-Cu and Sn-Ag-Cu-1 wt% ZrO2 composite solder joints on OSP-Cu pads were about 53.2 and 59.5 kJ/mol, respectively. In addition, solder joints containing ZrO2 nano-particles displayed higher hardness due to the uniform distribution of ZrO2 nano-particles as well as the refined IMC particles. The hardness values of the plain Sn-Ag-Cu solder joint and solder joints containing 1 wt% of ZrO2 nano-particles after 5 min reaction at 250 degrees C were about 15.0 Hv and 17.1 Hv, respectively. On the other hand, their hardness values after 30 min reaction were about 13.7 Hv and 15.5 Hv, respectively. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:3319 / 3325
页数:7
相关论文
共 26 条
[1]  
[Anonymous], 1992, SCANNING ELECT MICRO
[2]   The effects of solder volume and Cu concentration on the consumption rate of Cu pad during reflow soldering [J].
Chang, C. C. ;
Lin, Y. W. ;
Wang, Y. W. ;
Kao, C. R. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 492 (1-2) :99-104
[3]   Interaction behavior between the additives and Sn in Sn-3.0Ag-0.5Cu-based solder alloys and the relevant joint solderability [J].
Cheng, Fangjie ;
Gao, Feng ;
Nishikawa, Hiroshi ;
Takemoto, Tadashi .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 472 (1-2) :530-534
[4]   Effect of nano Al2O3 additions on the microstructure, hardness and shear strength of eutectic Sn-9Zn solder on Au/Ni metallized Cu pads [J].
Fouzder, Tama ;
Gain, Asit Kumar ;
Chan, Y. C. ;
Sharif, A. ;
Yung, Winco K. C. .
MICROELECTRONICS RELIABILITY, 2010, 50 (12) :2051-2058
[5]   Effect of small Sn-3.5Ag-0.5Cu additions on the structure and properties of Sn-9Zn solder in ball grid array packages [J].
Gain, Asit Kumar ;
Chan, Y. C. ;
Sharif, Ahmed ;
Yung, Winco K. C. .
MICROELECTRONIC ENGINEERING, 2009, 86 (11) :2347-2353
[6]   Electrochemical composite deposition of Sn-Ag-Cu alloys [J].
Han, Chunfen ;
Liu, Qi ;
Ivey, Douglas G. .
MATERIALS SCIENCE AND ENGINEERING B-ADVANCED FUNCTIONAL SOLID-STATE MATERIALS, 2009, 164 (03) :172-179
[7]   Effect of rare earth element addition on the microstructure of Sn-Ag-Cu solder joint [J].
Li, B ;
Shi, YW ;
Lei, YP ;
Guo, F ;
Xia, ZD ;
Zong, B .
JOURNAL OF ELECTRONIC MATERIALS, 2005, 34 (03) :217-224
[8]   High temperature synthesis of Sn-3.5Ag-0.5Zn alloy nanoparticles by chemical reduction method [J].
Lin, C. Y. ;
Mohanty, U. S. ;
Chou, J. H. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 501 (02) :204-210
[9]   Interfacial reactions between Sn-8Zn-3Bi-xAg lead-free solders and Cu substrate [J].
Liu, Lijuan ;
Zhou, Wei ;
Li, Baoling ;
Wu, Ping .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 482 (1-2) :90-98
[10]   Evolutions of the interface and shear strength between SnAgCu-xNi solder and Cu substrate during isothermal aging at 150°C [J].
Liu, Ping ;
Yao, Pei ;
Liu, Jim .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 486 (1-2) :474-479