Interfacial carbonation for efficient flame retardance of glass fiber-reinforced polyamide 6

被引:29
作者
Chen, Wenhua [1 ]
Liu, Pengju [1 ]
Liu, Yuan [1 ]
Wang, Qi [1 ]
机构
[1] Sichuan Univ, State Key Lab Polymer Mat Engn, Polymer Res Inst, Chengdu 610065, Peoples R China
基金
中国国家自然科学基金;
关键词
MELAMINE POLYPHOSPHATE; AMMONIUM POLYPHOSPHATE; THERMAL-DECOMPOSITION; CLAY NANOCOMPOSITES; POLYMERIC MATERIALS; FIRE; COMPOSITES; XPS; DEGRADATION; PERFORMANCE;
D O I
10.1039/c5py00280j
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Wicking action, a typical physicochemical phenomenon, always causes high flammability of glass fiber (GF)-reinforced thermoplastic polymer composites due to the rapid and oriented flow of the polymer melt along the GF surface to the fire zone. This paper introduces an interfacial carbonation mode to solve the global challenge of flame resistance for these composites. Unlike the conventional bulk flame resistance mode, in which a high load of phosphorus flame retardants must be added and evenly distributed in the polymer matrix and the acid sources released by the flame retardants would catalyze the resin into a continuous and compact carbonate layer (the carbonates distributed in the bulk region are uncombined with the GFs), the interfacial mode enriches flame retardants in the GF-resin interfacial regions where wicking actions occur. After the composite burns, the released phosphorus acids can effectively carbonize the interfacial resin and the formed interfacial carbonate layer combining with the GF will convert the original smooth and high-energy GF surface to an inert and rough carbonate surface. The change of interfacial properties makes the adsorption, wetting, spreading and flow of the polymer melt along the GFs much more difficult, thus greatly weakening the wicking effects and improving the flame retardance efficiency of the composites.
引用
收藏
页码:4409 / 4414
页数:6
相关论文
共 34 条
[1]   Investigation of the thermal degradation of polyurea: The effect of ammonium polyphosphate and expandable graphite [J].
Awad, Walid H. ;
Wilkie, Charles A. .
POLYMER, 2010, 51 (11) :2277-2285
[2]   Recent Advances in Clay/Polymer Nanocomposites [J].
Bitinis, N. ;
Hernandez, M. ;
Verdejo, R. ;
Kenny, J. M. ;
Lopez-Manchado, M. A. .
ADVANCED MATERIALS, 2011, 23 (44) :5229-5236
[3]   XPS study of an intumescent coating .2. Application to the ammonium polyphosphate pentaerythritol ethylenic terpolymer fire retardant system with and without synergistic agent [J].
Bourbigot, S ;
LeBras, M ;
Delobel, R ;
Gengembre, L .
APPLIED SURFACE SCIENCE, 1997, 120 (1-2) :15-29
[4]   Fire retardant polymers: recent developments and opportunities [J].
Bourbigot, Serge ;
Duquesne, Sophie .
JOURNAL OF MATERIALS CHEMISTRY, 2007, 17 (22) :2283-2300
[5]   Flame retardancy mechanisms of aluminium phosphinate in combination with melamine polyphosphate and zinc borate in glass-fibre reinforced polyamide 6,6 [J].
Braun, Ulrike ;
Schartel, Bernhard ;
Fichera, Mario A. ;
Jaeger, Christian .
POLYMER DEGRADATION AND STABILITY, 2007, 92 (08) :1528-1545
[6]   Hydrotalcites Catalyze the Acidolysis Polymerization of Phenolic Acid to Create Highly Heat-Resistant Bioplastics [J].
Chauzar, Manu ;
Tateyama, Seiji ;
Ishikura, Takanori ;
Matsumoto, Keitaro ;
Kaneko, Daisaku ;
Ebitani, Kohki ;
Kaneko, Tatsuo .
ADVANCED FUNCTIONAL MATERIALS, 2012, 22 (16) :3438-3444
[7]   Preparation, properties and characterizations of halogen-free nitrogen-phosphorous flame-retarded glass fiber reinforced polyamide 6 composite [J].
Chen, Yinghong ;
Wang, Qi .
POLYMER DEGRADATION AND STABILITY, 2006, 91 (09) :2003-2013
[8]   Fibre reinforced nanocomposites: Mechanical properties of PA6/clay and glass fibre/PA6/clay nanocomposites [J].
Clifford, Mike J. ;
Wan, Tong .
POLYMER, 2010, 51 (02) :535-539
[9]   Recent developments in the fire retardancy of polymeric materials [J].
Dasari, Aravind ;
Yu, Zhong-Zhen ;
Cai, Gui-Peng ;
Mai, Yiu-Wing .
PROGRESS IN POLYMER SCIENCE, 2013, 38 (09) :1357-1387
[10]   Processing degradation of polyamide 6/montmorillonite clay nanocomposites and clay organic modifier [J].
Davis, RD ;
Gilman, JW ;
VanderHart, DL .
POLYMER DEGRADATION AND STABILITY, 2003, 79 (01) :111-121