Formation of Cr-modified silicide coatings on a Ti-Nb-Si based ultrahigh-temperature alloy by pack cementation process

被引:47
|
作者
Qiao, Yanqiang [1 ]
Guo, Xiping [1 ]
机构
[1] NW Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Peoples R China
基金
中国国家自然科学基金;
关键词
Ti-Nb-Si based ultrahigh temperature alloy; Coating structure; Phase constituents; Cr-modified silicide coating; Pack cementation process; OXIDATION-RESISTANT COATINGS; PHASE-EQUILIBRIA; MOLTEN-SALT; BEHAVIOR; NIOBIUM; MICROSTRUCTURE; COMPOSITES; AL; DEPOSITION; ADDITIONS;
D O I
10.1016/j.apsusc.2010.05.091
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Cr-modified silicide coatings were prepared on a Ti-Nb-Si based ultrahigh temperature alloy by Si-Cr co-deposition at 1250 degrees C, 1350 degrees C and 1400 degrees C for 5-20 h respectively. It was found that both coating structure and phase constituents changed significantly with increase in the co-deposition temperature and holding time. The outer layers in all coatings prepared at 1250 degrees C for 5-20 h consisted of (Ti,X)(5)Si(3) (X represents Nb, Cr and Hf elements). (Ti,X)(5)Si(4) was found as the only phase constituent in the intermediate layers in both coatings prepared at 1250 degrees C for 5 and 10 h, but the intermediate layers in the coatings prepared at 1250 degrees C for 15 and 20 h were mainly composed of (Ti,X)(5)Si(3) phase that was derived from the decomposition of (Ti,X)(5)Si(4) phase. In the coating prepared at 1350 degrees C for 5 h, single (Ti X)(5)Si(3) phase was found in its outmost layer, the same as that in the outer layers in the coatings prepared at 1250 degrees C; but in the coatings prepared at 1350 degrees C for 10-20 h, (Nb(1.95)Cr(1.05))Cr(2)Si(3) ternary phase was found in the outmost layers besides (Ti,X)(5)Si(3) phase. In the coatings prepared at 1400 degrees C for 5-20 h, (Nb(1.95)Cr(1.05))Cr(2)Si(3) ternary phase was the single phase constituent in their outmost layers. The phase transformation (Ti,X)(5)Si(4)->(Ti,X)(5)Si(3) + Si occurred in the intermediate layers of the coatings prepared at 1350 and 1400 degrees C with prolonging co-deposition time, similar to the situation in the coatings prepared at 1250 degrees C for 15 and 20 h, but this transformation has been speeded up by increase in the co-deposition temperature. The transitional layers were mainly composed of (Ti,X)(5)Si(3) phase in all coatings. The influence of co-deposition temperature on the diffusion ability of Cr atoms was greater than that of Si atoms in the Si-Cr co-deposition processes investigated. The growth of coatings obeyed inverse logarithmic laws at all three co-deposition temperatures. The Si-Cr co-deposition coating prepared at 1350 degrees C for 10 h showed a good oxidation resistance due to the formation of SiO(2) and Nb, Cr-doped TiO(2) scale after oxidation at 1250 degrees C for 10 h. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:7462 / 7471
页数:10
相关论文
共 50 条
  • [41] High-Temperature Oxidation Resistance Performance of Si-Ti-Cr Silicide Coating on Nb-Hf Alloy Surface in Constant Oxidation and Thermal Shock
    An Dongyang
    Liu Chenfei
    Zhao Shuang
    Zhang Haipeng
    Zou Yongchun
    Tang Zengwu
    Xiao Peng
    Dai Jingmin
    Wang Yaming
    RARE METAL MATERIALS AND ENGINEERING, 2023, 52 (04) : 1219 - 1226
  • [42] Investigation of scale formation and degeneration of silicide coating on Nb-Si based alloy in the temperature range from 1250 °C to 1560 °C
    Zhang, Weiping
    Qiao, Yanqiang
    Guo, Xiping
    INTERMETALLICS, 2024, 172
  • [43] Improving high temperature oxidation and hot corrosion resistance of Ni-base super alloy INC738LC with Cr-Si-RE modified aluminide coatings produced by single step pack cementation process
    Afshar, A.
    Sabour, A.
    Saremi, M.
    Ghasemi, D.
    PROTECTION OF METALS AND PHYSICAL CHEMISTRY OF SURFACES, 2012, 48 (01) : 120 - 127
  • [44] High-Temperature Thermal Shock Performance of Si-Ti-Cr Silicide Coating on Nb-Hf Alloy Surface in Atmosphere and Vacuum
    An Dongyang
    Liu Chenfei
    Zhao Shuang
    Zhang Haipeng
    Tang Zengwu
    Xiao Peng
    Dai Jingmin
    Wang Yaming
    RARE METAL MATERIALS AND ENGINEERING, 2022, 51 (11) : 3974 - 3980
  • [45] High temperature protection of a novel TiB2-modified (Nb,Mo,Cr)Si2 ceramic coating on Nb-based alloy
    Zhou, Xiaojun
    Xu, Jiawei
    Zha, Yitao
    Zhang, Yafang
    Deng, Guanzhi
    Zhao, Xiaojun
    Cai, Zhenyang
    Liu, Sainan
    Xiao, Lairong
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2024, 44 (07) : 4425 - 4436
  • [46] Morphology and phase constituents of mechanically alloyed Nb-Ti-Si based ultrahigh temperature alloy powders
    Wang Taotao
    Guo Xiping
    RARE METALS, 2011, 30 : 427 - 432
  • [47] Morphology and phase constituents of mechanically alloyed Nb-Ti-Si based ultrahigh temperature alloy powders
    Taotao Wang
    Xiping Guo
    Rare Metals, 2011, 30 : 427 - 432
  • [48] Effects of high-temperature homogenizing and aging treatments on the microstructure of Nb-Ti-Si based ultrahigh temperature alloy
    State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072, China
    Xiyou Jinshu Cailiao Yu Gongcheng, 2008, 9 (1601-1605):
  • [49] Microstructure and High Temperature Oxidation Resistance of Si-Al-Y Co-deposition Coatings Prepared on TiAl alloy by Pack Cementation Process
    Li Yong-Quan
    Xie Fa-Qin
    Wu Xiang-Qing
    Li Xuan
    JOURNAL OF INORGANIC MATERIALS, 2013, 28 (12) : 1369 - 1375
  • [50] A novel composite Si-Mo-Ti coating with Ti concentration gradient for Nb-Si based ultrahigh temperature alloy prepared by slurry sintering
    Li, Longfei
    Guo, Xiping
    Qiao, Yanqiang
    CORROSION SCIENCE, 2023, 225