Fatigue propagation of long cracks in ferritic thin wall ductile iron castings

被引:0
|
作者
Caldera, M. [1 ]
Chapetti, M. [1 ]
Massone, J. M. [1 ]
Sikora, J. A. [1 ]
机构
[1] Natl Univ Mar del Plata, Fac Engn, INTEMA, CONICET, Mar Del Plata, Buenos Aires, Argentina
关键词
Ductile iron; Thin wall; Nodule count; Grain size; Fatigue crack propagation; Fracture surface; MECHANICAL-PROPERTIES; CARBIDES; PLATES;
D O I
10.1179/174328409X433822
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The present work focuses on the fatigue propagation of long cracks in ferritic ductile iron parts of varied thickness. Samples were taken from thin wall ductile iron plates and standard 'Y' blocks with nodule counts ranging from 250 to 2200 nod/mm(2) and ferrite grain sizes from 70 to 150 mu m. Fatigue crack propagation threshold Delta K-th and Paris law constants C and m were measured, and the influence of the microstructure refinement (established through nodule count and grain size) on the characteristics of the fatigue fracture surface was analysed. The results show that, once the crack is initiated, the fatigue crack growth threshold diminishes as the microstructure is refined, while the rate of growth remains practically unaltered. The crack path preferentially intersects graphite nodules and is mostly transgranular through the ferrite grains. Nevertheless, at low levels of Delta K, a low percentage of intergranular fracture was also observed.
引用
收藏
页码:1102 / 1107
页数:6
相关论文
共 50 条
  • [31] Production of carbide-free thin ductile iron castings
    M. Ashraf Sheikh
    Journal of University of Science and Technology Beijing, 2008, (05) : 552 - 555
  • [32] Production of carbide-free thin ductile iron castings
    Sheikh, M. Ashraf
    JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING, 2008, 15 (05): : 552 - 555
  • [33] The morphology of solidification of thin-section ductile iron castings
    Yeung, CF
    Zhao, H
    Lee, WB
    MATERIALS CHARACTERIZATION, 1998, 40 (4-5) : 201 - 208
  • [34] Surface reactivity of thin wall ferritic ductile iron.: The effect of nodule count and grinding variables
    Sosa, A. D.
    Echeverria, M. D.
    Moncada, O. J.
    Simison, S. N.
    MATERIALS LETTERS, 2008, 62 (01) : 100 - 102
  • [35] Propagation of Long Fatigue Cracks under Remote Modes II and III in Ferritic-Pearlitic Steel
    Vojtek, T.
    Pokluda, J.
    Hohenwarter, A.
    Pippan, R.
    ACTA PHYSICA POLONICA A, 2015, 128 (04) : 611 - 614
  • [36] Effects of Antimony and Wall Thickness on Graphite Morphology in Ductile Iron Castings
    Zoran Glavas
    Anita Strkalj
    Kresimir Maldini
    Metallurgical and Materials Transactions B, 2016, 47 : 2487 - 2497
  • [37] Effects of Antimony and Wall Thickness on Graphite Morphology in Ductile Iron Castings
    Glavas, Zoran
    Strkalj, Anita
    Maldini, Kresimir
    METALLURGICAL AND MATERIALS TRANSACTIONS B-PROCESS METALLURGY AND MATERIALS PROCESSING SCIENCE, 2016, 47 (04): : 2487 - 2497
  • [38] Short fatigue cracks in austempered ductile cast iron (ADI)
    Marrow, T.J.
    Çetinel, H.
    Fatigue and Fracture of Engineering Materials and Structures, 2000, 23 (05): : 425 - 434
  • [39] Short fatigue cracks in austempered ductile cast iron (ADI)
    Marrow, TJ
    Çetinel, H
    FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2000, 23 (05) : 425 - 434
  • [40] Overload effects on fatigue cracks in a ferritized ductile cast iron
    Iacoviello, Francesco
    Di Cocco, Vittorio
    Bellini, Costanzo
    INTERNATIONAL JOURNAL OF FATIGUE, 2019, 127 : 376 - 381