Influence of limestone content, gypsum content and fineness on early age properties of Portland limestone cement produced by inter-grinding

被引:55
作者
Irassar, E. F. [1 ]
Violini, D. [2 ]
Rahhal, V. F. [1 ]
Milanesi, C. [2 ]
Trezza, M. A. [1 ]
Bonavetti, V. L. [1 ]
机构
[1] Univ Nacl Ctr Prov Buenos Aires, Fac Ingn, Olavarria, Argentina
[2] Cementos Avellaneda SA, Buenos Aires, DF, Argentina
关键词
Limestone filler; Hydration heat; Inter-grinding; Fineness; Early strength; SHORT-TERM HYDRATION; MINERAL ADMIXTURES; INERT MATERIALS; MORTARS; FILLER; PARAMETERS; CONCRETE; CLINKER; PASTES;
D O I
10.1016/j.cemconcomp.2010.10.001
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
This paper examines the behavior of Portland limestone cements (PLCs) made by inter-grinding clinker, gypsum and limestone in a full size-cement plant, while varying the content of limestone filler (LF - 0% and 24%), content of gypsum (GC - 2.5% and 5.0%) and PLC fineness, measured as that fraction retained on a 45 mu m sieve (R45 -5% and 18%). The influence of the combined action of these variables on the particle size distribution (PSD) and early age properties of blended cement was studied using a 2(3) experimental design. Fineness evaluated by the parameters of the Rosin-Rammler-Springer-Bennett (RRSB) distribution function shows that the uniformity index (n-parameter) depends strongly on LF content; while the characteristic diameter (x'-parameter) depends on R45 and LF content. As for the inter-grinding process, water demand is reduced by incorporation of LF and increased by reduction of R45, producing a compensation. Setting time is mainly affected by R45; LF produces a few modifications and the influence of gypsum content and gypsum-limestone interaction are not as obvious. Calorimetry studies show that LF decreases the height of the main peak and the total heat released, while gypsum content modifies the time of acceleration and the post-peak hydration, specifically for fine cements. In accordance, chemical shrinkage decreases when R45, LF content and gypsum content increase. Up to 2 days, strength is mainly governed by the R45 and the LF in PLC, which act inversely. At early ages, the influence of gypsum content on early properties increases up to 48 h. XRD analysis shows its stimulation of calcium silicate hydration during the first hours and ettringite formation after 24 h. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:192 / 200
页数:9
相关论文
共 35 条
[1]  
ADAMS LD, 1990, AM SOC TEST MATER, V1064, P41, DOI 10.1520/STP23470S
[2]  
[Anonymous], P 11 INT C CHEM CEM
[3]  
Barker AP, 1989, HEAT RELEASE CHARACT
[4]  
Baron J., 1987, WORLD CEMENT, V18, P100
[5]  
Bensted J., 1980, WORLD CEM TECHNOL, V11, P395
[6]   Modeling the influence of limestone filler on cement hydration using CEMHYD3D [J].
Bentz, DP .
CEMENT & CONCRETE COMPOSITES, 2006, 28 (02) :124-129
[7]   Limestone filler cement in low w/c concrete:: A rational use of energy [J].
Bonavetti, V ;
Donza, H ;
Menéndez, G ;
Cabrera, O ;
Irassar, EF .
CEMENT AND CONCRETE RESEARCH, 2003, 33 (06) :865-871
[8]   Studies on the carboaluminate formation in limestone filler-blended cements [J].
Bonavetti, VL ;
Rahhal, VF ;
Irasser, EF .
CEMENT AND CONCRETE RESEARCH, 2001, 31 (06) :853-859
[9]   Chemical shrinkage of cement pastes and mortars at very early age: Effect of limestone filler and granular inclusions [J].
Bouasker, M. ;
Mounanga, P. ;
Turcry, P. ;
Loukili, A. ;
Khelidj, A. .
CEMENT & CONCRETE COMPOSITES, 2008, 30 (01) :13-22
[10]  
CAMPITELI VC, 1990, P CARB ADD CEM AM SO, P30