Characterizations of nano-crystalline diamond coating cutting tools

被引:57
|
作者
Hu, J. [1 ]
Chou, Y. K. [1 ]
Thompson, R. G. [2 ]
Burgess, J. [3 ]
Street, S. [3 ]
机构
[1] Univ Alabama, Dept Mech Engn, Tuscaloosa, AL 35487 USA
[2] Vista Engn Inc, Birmingham, AL USA
[3] Univ Alabama, Dept Chem, Tuscaloosa, AL 35487 USA
来源
SURFACE & COATINGS TECHNOLOGY | 2007年 / 202卷 / 4-7期
基金
美国国家科学基金会; 美国国家航空航天局;
关键词
diamond coating; nano-crystalline diamond; machining; material characterization; tool wear;
D O I
10.1016/j.surfcoat.2007.07.050
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Diamond coatings made by processes such as chemical vapor deposition (CVD) have been increasingly explored for cutting tools applications, in particular, for machining lightweight high-strength materials. However, most literature to date reported that the wear resistance of CVD diamond tools is still distant to the polycrystalline diamond (PCD) counterparts. Recently, a microwave plasma-assisted CVD technology was developed to increase the diamond growth rate, and by adding nitrogen gas, this process can produce nano-structured coatings which consist of nano-diamond crystals embedded into a hard amorphous diamond-like carbon matrix and have high hardness and low surface roughness. In this study, the nano-crystalline diamond (NCD) coating tools were characterized, compared to the conventional microcrystalline diamond coating (MCD) and PCD tools, in surface topography, grain sizes, carbon bonds, and mechanical properties. Moreover, the diamond tools were evaluated in machining Al-matrix composite and high-strength Al alloy. The results show that the NCD tools have smoother surfaces than the MCD tools, but rougher than the polished PCD tools. As to the diamond crystals, the NCD tools have ultrafine gains and the PCD tools have the largest grains. For the cutting edges, the PCD tools have the sharpest edge resulted from polishing and the NCD tools have larger edge rounding than the MCD counterparts. In addition to the nature-diamond peak identified in the Raman spectra, the NCD and MCD tools have additional Raman shifts associated with graphite and other disordered carbon bonds. The NCD tools have a much higher hardness, but a lower elasticity, than both the MCD and PCD tools. In machining testing, the NCD tools substantially outperform the MCD tools and are comparable to the PCD tools. For both the NCD and MCD tools, coating delamination is the major tool wear mechanism that leads to catastrophic tool failures. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:1113 / 1117
页数:5
相关论文
共 50 条
  • [21] Plasma Parameter Analysis During Nano-Crystalline Diamond Growth Using Automated Langmuir Probe
    Paosawatyanyong, B.
    Thitianan, S.
    Bhanthumnavin, B.
    Promros, N.
    Wong, C. S.
    JOURNAL OF COMPUTATIONAL AND THEORETICAL NANOSCIENCE, 2015, 12 (05) : 894 - 900
  • [22] Improving the long-term stability of Ti6Al4V abutment screw by coating micro/nano-crystalline diamond films
    Xie, Youneng
    Zhou, Jing
    Wei, Qiuping
    Yu, Z. M.
    Luo, Hao
    Zhou, Bo
    Tang, Z. G.
    JOURNAL OF THE MECHANICAL BEHAVIOR OF BIOMEDICAL MATERIALS, 2016, 63 : 174 - 182
  • [23] Depth profiling of nitrogen within 15N-incorporated nano-crystalline diamond thin films
    Garratt, E.
    AlFaify, S.
    Cassidy, D. P.
    Dissanayake, A.
    Mancini, D. C.
    Ghantasala, M. K.
    Kayani, A.
    APPLIED PHYSICS LETTERS, 2013, 103 (13)
  • [24] Nano-crystalline diamond-coated titanium dental implants - A histomorphometric study in adult domestic pigs
    Metzler, Philipp
    von Wilmoyvsky, Cornelius
    Stadlinger, Bernd
    Zemann, Wolfgang
    Schlegel, Karl Andreas
    Rosiwal, Stephan
    Rupprecht, Stephan
    JOURNAL OF CRANIO-MAXILLOFACIAL SURGERY, 2013, 41 (06) : 532 - 538
  • [25] Fabrication of Nano-Crystalline Diamond Duplex Micro-Gear by Hot Filament Chemical Vapor Deposition
    Wang, Hong-jun
    Zuo, Dun-wen
    Xu, Feng
    Lu, Wen-zhuang
    MATERIALS TRANSACTIONS, 2017, 58 (01) : 91 - 94
  • [26] Thermal conductivity of ultrathin nano-crystalline diamond films determined by Raman thermography assisted by silicon nanowires
    Anaya, Julian
    Rossi, Stefano
    Alomari, Mohammed
    Kohn, Erhard
    Toth, Lajos
    Pecz, Bela
    Kuball, Martin
    APPLIED PHYSICS LETTERS, 2015, 106 (22)
  • [27] Effect of CH4/H2 plasma ratio on ultra-low friction of nano-crystalline diamond coating deposited by MPECVD technique
    Sharma, Neha
    Kumar, N.
    Sundaravel, B.
    Panda, Kalpataru
    David, Wang
    Kamarrudin, M.
    Dash, S.
    Panigrahi, B. K.
    Tyagi, A. K.
    Lin, I-Nan
    Raj, Baldev
    TRIBOLOGY INTERNATIONAL, 2011, 44 (09) : 980 - 986
  • [28] Diamond planing of coated cutting tools
    Ya. I. Barats
    D. A. Tikhonov
    Russian Engineering Research, 2008, 28 (3) : 275 - 276
  • [29] Effect of bottom micro-crystalline diamond (MCD) layer and top nano-crystalline diamond (NCD) layer onto the tribological behavior of (MCD/NCD) bilayer film
    Luo, Yijie
    Ma, Li
    Li, Liang
    Chen, Yubo
    Zhou, Kechao
    Yi, Mingkun
    Deng, Biao
    Yang, Haohui
    Xia, Xin
    Hua, Tengyu
    Yin, Dengfeng
    Wei, Qiuping
    MATERIALS RESEARCH EXPRESS, 2020, 7 (02)
  • [30] Nano-Crystalline Diamond Films with Pineapple-Like Morphology Grown by the DC Arcjet vapor Deposition Method
    Li Bin
    Zhang Qin-Jian
    Shi Yan-Chao
    Li Jia-Jun
    Li Hong
    Lu Fan-Xiu
    Chen Guang-Chao
    CHINESE PHYSICS LETTERS, 2014, 31 (08)