Freezing of polarization dynamics in relaxor ferroelectric (1-x)Pb(Mg1/3Nb2/3)O3-xBi(Zn1/2Ti1/2)O3 solid solution

被引:9
|
作者
Tailor, H. N.
Bokov, A. A.
Ye, Z. -G. [1 ]
机构
[1] Simon Fraser Univ, Dept Chem, 8888 Univ Dr, Burnaby, BC V5A 1S6, Canada
关键词
Ferroelectric relaxor; Dielectrics spectroscopy; Relaxation; Polarization dynamics; LEAD MAGNESIUM NIOBATE; PEROVSKITE; PHASE;
D O I
10.1016/j.cap.2011.03.023
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ceramics of a the binary solid solution (1-x)Pb(Mg1/3Nb2/3)O-3-xBi(Zn1/2Ti1/2)O-3 [(1-x)PMN-xBZT] have been prepared with x = 0.10 and 0.15 and examined by dielectric spectroscopy to reveal the temperature dependences of the relaxor ferroelectric behavior. Both compositions studied show a broad and diffuse peak in the temperature dependence of dielectric permittivity epsilon'(T), the temperature of which increases with increasing measurement frequency, indicating the typical relaxor behavior. Detailed analysis of the dielectric response shows that it involves the same types of polarization contributions as the prototypical relaxor Pb(Mg1/3Nb2/3)O-3. One of the contribution to the permittivity arises from the conventional relaxor polarization, chi(CR)*, which can be described by the Kohlrausch-Williams-Watts (KWW) law, P proportional to exp[-(t/tau)(beta)]. It is found that the beta and tau parameters both follow the Vogel-Fulcher law, with the freezing temperature T-f decreasing with increasing BZT content. The change in diffuseness and freezing temperature can be attributed to the increase in chemical disorder because the addition of BZT end member introduces two more heterovalent cations (Zn2+ and Ti4+) on the perovskite octahedral B-site and the Bi3+ cations on the perovskite A-site of PMN. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:S175 / S179
页数:5
相关论文
共 50 条
  • [1] Synthesis and Dielectric Characterization of a New Relaxor Solid Solution of (1-x)Pb(Mg1/3Nb2/3)O3-xBi(Zn1/2Ti1/2)O3
    Tailor, H. N.
    Bokov, A. A.
    Ye, Z. -G.
    FERROELECTRICS, 2010, 405 : 67 - 75
  • [2] Synthesis, structure, dielectric properties and relaxor behavior of a novel solid solution (1-x)Pb(Mg1/3Nb2/3)O3-xBi(Zn2/3Nb1/3)O3
    Liu, Z.
    Yuan, Y.
    Jaimeewong, P.
    Wu, H.
    Ren, W.
    Ye, Z. -G
    FERROELECTRICS, 2018, 534 (01) : 42 - 49
  • [3] Resistivity Enhancement and Transport Mechanisms in (1-x)BaTiO3-xBi(Zn1/2Ti1/2)O3 and (1-x)SrTiO3-xBi(Zn1/2Ti1/2)O3
    Kumar, Nitish
    Cann, David P.
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2015, 98 (08) : 2548 - 2555
  • [4] Absence of tetragonal distortion in (1-x)SrTiO3-xBi(Zn1/2Ti1/2)O3 solid solution
    Pandey, Rishikesh
    Pillutla, Ravi Kiran
    Shankar, Uma
    Singh, Akhilesh Kumar
    JOURNAL OF APPLIED PHYSICS, 2013, 113 (18)
  • [5] Two Components of the Macroscopic Polarization in Pb(Mg1/3Nb2/3)O3 Relaxor Ferroelectric
    Deguchi, Kiyoshi
    JOURNAL OF THE PHYSICAL SOCIETY OF JAPAN, 2015, 84 (07)
  • [6] Growth and characterization of piezo-/ferroelectric Pb(Mg1/3Nb2/3)O3-PbTiO3-Bi(Zn1/2Ti1/2)O3 ternary single crystals
    Belan, Reagan A.
    Tailor, Hamel N.
    Long, Xifa
    Bokov, Alexei A.
    Ye, Zuo-Guang
    JOURNAL OF CRYSTAL GROWTH, 2011, 318 (01) : 839 - 845
  • [7] Anelastic relaxor behavior of Pb(Mg1/3Nb2/3)O3
    Ursic, Hana
    Damjanovic, Dragan
    APPLIED PHYSICS LETTERS, 2013, 103 (07)
  • [8] Effect of Pb(Zn1/3Nb2/3)O3 substitution on dielectric properties of Pb[(Zn1/3Ta2/3),(Mg1/3Nb2/3)]O3 multiple-octahedral system ceramics
    Chae, MC
    Lim, SM
    Kim, NK
    FERROELECTRICS, 2000, 247 (04) : 355 - 365
  • [9] Characterizations of epitaxial Bi(Mg1/2Ti1/2)O3-Bi(Zn1/2Ti1/2)O3 solid solution films grown by pulsed laser deposition
    Oikawa, Takahiro L.
    Yasui, Shintaro
    Watanabe, Takayuki
    Yabuta, Hisato
    Kobayashi, Takeshi
    Miura, Kaoru
    Funakubo, Hiroshi
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2014, 53 (05)
  • [10] The problem of phase transitions in PZT based solid solutions, Pb(Mg1/3Nb2/3)O3, Pb(In1/2Nb1/2)O3 and "Relaxor ferroelectricity." -: 2.: Analysis of experimental results and phase diagrams for Pb(Mg1/3Nb2/3)O3, Pb(B′1/2B"1/2)O3
    Ishchuk, VM
    FERROELECTRICS, 2003, 289 : 33 - 51