Microstructure evolution and corrosion behavior of 316L stainless steel subjected to torsion

被引:6
|
作者
Zhang, Pengyan [1 ]
Han, Weixue [1 ]
Huang, Zhenyi [1 ]
Li, Guisheng [1 ]
Zhang, Mingya [1 ]
Li, Jinghui [1 ]
机构
[1] Anhui Univ Technol, Sch Met Engn, Maanshan 243002, Peoples R China
基金
中国国家自然科学基金;
关键词
316L stainless steel; torsion deformation; microstructure evolution; corrosion resistance; IMPEDANCE PLANE DISPLAYS; GRAIN-REFINEMENT; STABILITY CONDITIONS; STEADY-STATE; DEFORMATION; RESISTANCE; SURFACE; PLASTICITY; DISLOCATIONS; TEMPERATURE;
D O I
10.1088/2053-1591/ac1ecc
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructure evolution of 316L stainless steels subjected to torsion deformation and its corrosion resistance in 1 M H2SO4 solutions were studied. Microstructure evolution of the annealed and torsion-processed samples was characterized by x-ray diffraction and electron backscatter diffraction techniques. The results showed that no martensitic transformation occurred during torsion deformation, while dynamic recrystallization occurred within the samples slowing down the tendency of increasing dislocation density and storage energy. Electrochemical tests including potentiodynamic polarization tests and electrochemical impedance spectroscopy (EIS) were used in the 1 M H2SO4 solution to evaluate the corrosion resistance of the annealed and torsion-processed samples. The results illustrated that small deformation (torsion for 1 turn) could enhance the corrosion resistance of the 316L stainless steels by increasing the stability of the passive film, the medium deformation (torsion for 3 turns) will deteriorate the corrosion resistance due to high-density dislocations formed during torsion deformation, while large deformation (torsion for 5 turns) could improve the corrosion resistance compared with the medium deformation due to the occurrence of dynamic recrystallization and the high-density deformation twins formed.
引用
收藏
页数:14
相关论文
共 50 条
  • [31] Microstructure and Texture Evolution During Cold Rolling of 316L Stainless Steel
    Chunlei Zhang
    Dorte Juul Jensen
    Tianbo Yu
    Metallurgical and Materials Transactions A, 2021, 52 : 4100 - 4111
  • [32] The Research on the Corrosion Inhibitor for the 316L Stainless Steel
    Yang, Ruisong
    Li, Mingtian
    Jin, Yongzhong
    ADVANCED RESEARCH ON MATERIAL, ENERGY AND CONTROL ENGINEERING, 2013, 648 : 11 - 14
  • [33] Corrosion behavior of additively manufactured 316L stainless steel in acidic media
    Lodhi, M. J. K.
    Deen, K. M.
    Haider, Waseem
    MATERIALIA, 2018, 2 : 111 - 121
  • [34] Effect of Severe Cold or Warm Deformation on Microstructure Evolution and Tensile Behavior of a 316L Stainless Steel
    Odnobokova, Marina
    Belyakov, Andrey
    Kaibyshev, Rustam
    ADVANCED ENGINEERING MATERIALS, 2015, 17 (12) : 1812 - 1820
  • [35] Corrosion Behavior of Eutectic Molten Salt solution on Stainless Steel 316L
    Subari, Fuzieah
    Maksom, Hafizul Faiz
    Zawawi, Aiman
    WORLD CONFERENCE ON TECHNOLOGY, INNOVATION AND ENTREPRENEURSHIP, 2015, : 2699 - 2708
  • [36] Corrosion Behavior of Sintered 316L Stainless Steel Fibre Porous Felt
    Ao Qingbo
    Tang Huiping
    Wang Jianzhong
    Zhi Hao
    Ma Jun
    Li Bin
    RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (10) : 2344 - 2348
  • [37] The Influence of Corrosion on the Mechanical Behavior of AISI 316L Stainless Steel Welds
    Turkan, Murat
    Karakas, Ozler
    MECHANIKA, 2019, 25 (02): : 114 - 118
  • [38] Corrosion behavior of sintered 316L stainless steel fibre porous felt
    Tang, Huiping, 1600, Science Press (43):
  • [39] Effect of Passive Film on Cavitation Corrosion Behavior of 316L Stainless Steel
    Cao, Lifang
    Qin, Zhenbo
    Deng, Yida
    Zhong, Cheng
    Hu, Wenbin
    Wu, Zhong
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2020, 15 (01): : 628 - 638
  • [40] Effect of Hydrostatic Pressure on the Pitting Corrosion Behavior of 316L Stainless Steel
    Wang, Zhongyi
    Cong, Yuan
    Zhang, Tao
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2014, 9 (02): : 778 - 798