Microstructure and stress corrosion cracking of a SA508-309L/308L-316L dissimilar metal weld joint in primary pressurized water reactor environment

被引:42
作者
Dong, Lijin [1 ,2 ]
Ma, Cheng [1 ]
Peng, Qunjia [1 ]
Han, En-Hou [1 ]
Ke, Wei [1 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Key Lab Nucl Mat & Safety Assessment, Shenyang 110016, Peoples R China
[2] Southwest Petr Univ, Sch Mat & Engn, Chengdu 610500, Peoples R China
来源
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY | 2020年 / 40卷
基金
中国国家自然科学基金;
关键词
Dissimilar metal weld joint; Stress corrosion cracking; Microstructure; Primary pressurized water reactor environment; Slow strain rate tension; LOW-ALLOY STEEL; AUSTENITIC STAINLESS-STEELS; HEAT-AFFECTED ZONE; FUSION BOUNDARY REGION; BEHAVIOR; TRANSITION; SUSCEPTIBILITY; CHEMISTRY;
D O I
10.1016/j.jmst.2019.08.035
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Stress corrosion cracking (SCC) of an SA508-309 L/308 L-316 L dissimilar metal weld joint in primary pressurized water reactor environment was investigated by the interrupted slow strain rate tension tests following a microstructure characterization. The 308 L weld metal shows a higher content of delta ferrite than the 309 L weld metal. In addition, no obvious Cr-depletion but carbides precipitation at gamma/delta phase boundaries was observed in both 308 L and 309 L weld metals. The slow strain rate tension tests showed that the SCC susceptibility of the base and weld metals of the dissimilar metal weld joint follows the order of SA508 < 308 L weld metal < the heat affected zone of 316 L base metal < 309 L weld metal. The higher SCC susceptibility of 309 L weld metal than that of 308 L weld metal is likely due to the lower content of 8 ferrite. In addition, a preferential SCC initiation in the 309 L weld metal adjacent to 308 L weld metal is attributed to few carbides in this region. (C) 2019 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
引用
收藏
页码:1 / 14
页数:14
相关论文
共 42 条
[1]   Role of δ-ferrite in stress corrosion cracking retardation near fusion boundary of 316NG welds [J].
Abe, Hiroshi ;
Watanabe, Yutaka .
JOURNAL OF NUCLEAR MATERIALS, 2012, 424 (1-3) :57-61
[2]   Stress corrosion cracking of stainless steels and nickel alloys in high-temperature water [J].
Andresen, P. L. ;
Morra, M. M. .
CORROSION, 2008, 64 (01) :15-29
[3]   Stress Corrosion Cracking of Current Structural Materials in Commercial Nuclear Power Plants [J].
Andresen, Peter L. .
CORROSION, 2013, 69 (10)
[4]  
[Anonymous], 2019, CRACK WELD AR REACT
[5]  
Arai T., 2009, P 14 C ENV DEGR MAT
[6]   Influence of carbide precipitation and rolling direction on intergranular stress corrosion cracking of austenitic stainless steels in hydrogenated high-temperature water [J].
Arioka, K. ;
Yamada, T. ;
Terachi, T. ;
Chiba, G. .
CORROSION, 2006, 62 (07) :568-575
[7]   Intergranular stress corrosion cracking behavior of austenitic stainless steels in hydrogenated high-temperature water [J].
Arioka, K ;
Yamada, T ;
Terachi, T ;
Staehle, RW .
CORROSION, 2006, 62 (01) :74-83
[8]   Understanding the effect of surface finish on stress corrosion crack initiation in warm-forged stainless steel 304L in high-temperature water [J].
Chang, Litao ;
Burke, M. Grace ;
Scenini, Fabio .
SCRIPTA MATERIALIA, 2019, 164 :1-5
[9]   Microstructure and Stress Corrosion Cracking Behavior of the Weld Metal in Alloy 52-A508 Dissimilar Welds [J].
Chung, Wei-Chih ;
Huang, Jiunn-Yuan ;
Tsay, Leu-Wen ;
Chen, Chun .
MATERIALS TRANSACTIONS, 2011, 52 (01) :12-19
[10]   Microstructure and intergranular stress corrosion cracking susceptibility of a SA508-52M-316L dissimilar metal weld joint in primary water [J].
Dong, Lijin ;
Peng, Qunjia ;
Han, En-Hou ;
Ke, Wei ;
Wang, Lei .
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2018, 34 (08) :1281-1292