Effect of microwave sintering on the properties of copper oxide doped Y-TZP ceramics

被引:10
作者
Ramesh, S. [1 ,5 ]
Lee, K. Y. Sara [1 ,2 ]
Tan, C. Y. [1 ]
Wong, Y. H. [1 ]
Alengaram, U. Johnson [3 ]
Tarlochan, F. [4 ]
Ramesh, S. [1 ,5 ]
Teng, W. D. [6 ]
Sutharsini, U. [7 ]
Sarhan, Ahmed A. D. [8 ]
机构
[1] Univ Malaya, Fac Engn, Dept Mech Engn, Ctr Adv Mfg & Mat Proc, Kuala Lumpur 50603, Malaysia
[2] Tunku Abdul Rahman Univ Coll, Fac Engn & Technol, Dept Mech Engn, Kuala Lumpur 53300, Malaysia
[3] Univ Malaya, Fac Engn, Dept Civil Engn, CICT, Kuala Lumpur 50603, Malaysia
[4] Qatar Univ, Coll Engn, Mech & Ind Engn Dept, Doha, Qatar
[5] Univ Malaya, Fac Sci, Dept Phys, Ctr Ion, Kuala Lumpur 50603, Malaysia
[6] SIRIM Berhad, Ceram Technol Grp, Shah Alam 40911, Malaysia
[7] Univ Jaffna, Dept Phys, Jaffna 40000, JA, Sri Lanka
[8] King Fahd Univ Petr & Minerals, Dept Mech Engn, Dhahran 31261, Saudi Arabia
关键词
Copper oxide; Sintering additive; Y-TZP; Microwave sintering; Mechanical properties; YTTRIA-STABILIZED ZIRCONIA; LOW-TEMPERATURE DEGRADATION; MANGANESE OXIDE; HYDROTHERMAL DEGRADATION; FRACTURE-TOUGHNESS; 3Y-TZP CERAMICS; GRAIN-GROWTH; HOLDING TIME; BEHAVIOR; DENSIFICATION;
D O I
10.1016/j.ceramint.2018.07.215
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of various amounts of copper oxide (CuO) up to 1 wt% on the densification behaviour and mechanical properties of 3 mol% yttria-tetragonal zirconia polycrystal (Y-TZP) were studied by using microwave (MW) sintering method. The MW sintering was performed at temperatures between 1100 degrees C and 1400 degrees C, with a heating rate of 30 degrees C/min. and holding time of 5 min. The beneficial effect of MW in enhancing densification was also compared for the undoped and 0.2 wt% CuO-doped Y-TZP when subjected to conventional sintering (CS) method. The results showed that significant enhancement in the relative density and Vickers hardness were observed for the undoped Y-TZP when MW-sintered between 1100 degrees C and 1250 degrees C. It was revealed that the 0.2 wt% CuO-doped Y-TZP and MW sintered at 1250-1300 degrees C could attain >= 99.8% of theoretical density, Vickers hardness of about 14.4 GPa, fracture toughness of 7.8 MPam(1/2) and exhibited fine equiaxed tetragonal grain size of below 0.25 mu m. In contrast, the addition of 1 wt% CuO was detrimental and the samples exhibited about 50% monoclinic phase upon sintering coupled with poor bulk density and mechanical properties. The study also revealed that the addition of 0.2 wt% CuO and subjected to conventional sintering produced similar densification as that obtained for microwave sintering, thus indicating that the dopant played a more significant role than the sintering method.
引用
收藏
页码:19639 / 19645
页数:7
相关论文
共 40 条
  • [1] A review on the susceptor assisted microwave processing of materials
    Bhattacharya, Madhuchhanda
    Basak, Tanmay
    [J]. ENERGY, 2016, 97 : 306 - 338
  • [2] Microwave Sintering of Zirconia Materials: Mechanical and Microstructural Properties
    Borrell, Amparo
    Salvador, Maria D.
    Penaranda-Foix, Felipe L.
    Catala-Civera, Jose M.
    [J]. INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2013, 10 (02) : 313 - 320
  • [3] Impedance spectroscopy of CuO-doped Y-TZP ceramics
    Bowen, C
    Ramesh, S
    Gill, C
    Lawson, S
    [J]. JOURNAL OF MATERIALS SCIENCE, 1998, 33 (21) : 5103 - 5110
  • [4] Densification and microstructure evolution of Y-Tetragonal Zirconia Polycrystal powder during direct and hybrid microwave sintering in a single-mode cavity
    Charmond, Sylvain
    Carry, Claude Paul
    Bouvard, Didier
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2010, 30 (06) : 1211 - 1221
  • [5] Direct microwave sintering of yttria-stabilized zirconia at 2•45 GHz
    Goldstein, A
    Travitzky, N
    Singurindy, A
    Kravchik, M
    [J]. JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 1999, 19 (12) : 2067 - 2072
  • [6] Effect of strontium hexaaluminate addition on the damage-tolerance of yttria-stabilized zirconia
    Gottwik, L.
    Wippermann, A.
    Kuntz, M.
    Denkena, B.
    [J]. CERAMICS INTERNATIONAL, 2017, 43 (17) : 15891 - 15898
  • [7] EFFECT OF A LIQUID-PHASE ON SUPERPLASTICITY OF 2-MOL-PERCENT-Y2O3-STABILIZED TETRAGONAL ZIRCONIA POLYCRYSTALS
    HWANG, CMJ
    CHEN, IW
    [J]. JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1990, 73 (06) : 1626 - 1632
  • [8] Hydrothermal ageing of yttria-stabilised zirconia, sintered at 1300°C-1325°C:: the effects of copper oxide doping and sintering time variations
    Kanellopoulos, P
    Gill, C
    [J]. JOURNAL OF MATERIALS SCIENCE, 2002, 37 (23) : 5075 - 5082
  • [9] Effect of grain size on wear behavior in Y-TZP ceramics
    Kumar, B. Venkata Manoj
    Kim, Won-Sik
    Hong, Seong-Hyeon
    Bae, Hung-Tak
    Lim, Dae-Soon
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (03): : 474 - 479
  • [10] Kwa SM, 2015, J CERAM PROCESS RES, V16, P193