Interface characteristics in diffusion bonding of Fe3Al with Cr18-Ni8 stainless steel

被引:7
|
作者
Wang, J [1 ]
Li, YJ
Yin, YS
机构
[1] Shandong Univ, Sch Mat Sci & Engn, Key Lab Liquid Struct & Hered Mat, Jinan 250061, Peoples R China
[2] Harbin Inst Technol, Natl Key Lab Adv Welding Prod Technol, Harbin 150001, Peoples R China
基金
中国国家自然科学基金;
关键词
Fe3Al/Cr18-Ni8; interface; diffusion bonding; reaction layer; characteristics;
D O I
10.1016/j.jcis.2004.10.071
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Fe3Al and Cr18-Ni8 stainless steel were diffusion-bonded in vacuum and a Fe3Al/Cr18-Ni8 interface with reaction layer was formed. Microstructure in the reaction layer at Fe3Al/Cr18-Ni8 interface was analyzed by means of scanning electron microscope (SEM) and electron probe micro-analyzer (EPMA). The growth of reaction layer with heating temperature (T) and holding time (t) was researched. The results indicate that FeAl, Fe3Al, Ni3Al, and alpha-Fe (Al) solid solution are formed in the reaction layer. These phases are favorable to promote the element diffusion and to accelerate the formation of the reaction layer at Fe3Al/Cr18-Ni8 interface. The growth of reaction layer obeys the parabolic law and its thickness (X) is expressed by X-2 = 7.5 x 10(-4) exp(-83.59/RT)(t - t(0)). (c) 2004 Elsevier Inc. All rights reserved.
引用
收藏
页码:201 / 205
页数:5
相关论文
共 50 条
  • [1] Stress distribution near the diffusion bonding interface of Fe3Al and Cr18-Ni8 stainless steel
    Li, Y.
    Xia, C.
    Wang, J.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2012, 50 (03): : 193 - 197
  • [2] Stress distribution at diffusion-bonded interface of Fe3Al with Cr18-Ni8 steel
    王娟
    李亚江
    夏春智
    China Welding, 2008, (03) : 46 - 50
  • [3] A study of crack and fracture on the welding joint of Fe3Al and Cr18-Ni8 stainless steel
    Li Yajiang
    Ma Haijun
    Wang Juan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (13-14): : 4343 - 4347
  • [4] Element diffusion near the interface of diffusion bonding for Fe3Al and stainless steel 18-8
    Li, YJ
    Wang, J
    Yin, YS
    Ma, HJ
    ACTA METALLURGICA SINICA, 2005, 41 (02) : 150 - 156
  • [5] Microstructure characteristics near the interface of vacuum brazing of Al/Cr18-Ni8 stainless steel
    Li, Y.
    Wang, J.
    Wu, N.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2013, 51 (02): : 129 - 133
  • [6] Effect of Cr and Ni on diffusion bonding of Fe3Al with steel
    Wang, J
    Li, YJ
    Ma, HJ
    BULLETIN OF MATERIALS SCIENCE, 2005, 28 (01) : 63 - 67
  • [7] Effect of Cr and Ni on diffusion bonding of Fe3Al with steel
    Wang Juan
    Li Yajiang
    Ma Haijun
    Bulletin of Materials Science, 2005, 28 (1) : 63 - 67
  • [8] Effect of heat treatment on microstructure near diffusion bonding interface of Fe3Al/18-8 stainless steel
    Ma, H. J.
    Li, Y. J.
    Wang, J.
    Yin, Y. S.
    MATERIALS SCIENCE AND TECHNOLOGY, 2006, 22 (12) : 1499 - 1502
  • [9] Microstructure and diffusion kinetics at the bonded Fe-16Al/Cr18-Ni8 interface
    Wang, J
    Li, YJ
    Ma, HJ
    Yin, YS
    REACTION KINETICS AND CATALYSIS LETTERS, 2005, 87 (01): : 67 - 75
  • [10] XRD and TEM analysis on the Fe3Al/18-8 stainless steel diffusion bonded interface
    Wang, J
    Li, YJ
    Liu, P
    MATERIALS LETTERS, 2003, 57 (26-27) : 4323 - 4327