Wear Behavior and Hardening Mechanism of Novel Lightweight Fe-25.1Mn-6.6Al-1.3C Steel Under Impact Abrasion Conditions

被引:21
作者
Peng, Shi-guang [1 ]
Song, Ren-bo [1 ]
Sun, Ting [2 ]
Pei, Zhong-zheng [1 ]
Cai, Chang-hong [1 ]
Feng, Yi-fan [1 ]
Tan, Zhi-dong [1 ]
机构
[1] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
[2] Cent Iron & Steel Res Inst, Beijing 100081, Peoples R China
关键词
Novel lightweight; Fe-25.1Mn-6.6Al-1.3C cast steel; Impact abrasive wear; Nano-size carbides; Lomer-Cottrell locks; Dislocation walls; HADFIELD MANGANESE STEEL; HIGH-STRENGTH; ALLOYS; DUCTILITY; DEFORMATION; ALUMINUM; MICROSTRUCTURES; TEMPERATURE;
D O I
10.1007/s11249-016-0751-2
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The aim of the present work was to reveal the wear behavior and hardening mechanism of novel lightweight Fe-25.1Mn-6.6Al-1.3C cast steel under abrasive impact wear with different heat treatments. The impact wear tests were carried out by using MLD-10 abrasive wear testing tester under the same impact wear condition. For this purpose, the cast steel upon quenching (Q) and quenching (1050 degrees C) + aging (Q-A) at 550 degrees C for a different time from 1 to 4 h was chosen to conduct impact abrasive wear tests. It was shown that the best wear resistance of Fe-25.1Mn-6.6Al-1.3C steel under Q-A (2 h) process was about 2.29 times higher than that of under Q process, which results from the fact that the fine nano-size second-phase (Fe, Mn)(3)A1C kappa-carbides tend to precipitate coherently within the austenite matrix under the additional aging treatment. In consequence, the fine nanosize kappa-carbides improved both the initial hardness and wear resistance of the substrate. However, when the specimen was treated at 550 degrees C for longer aging time (4 h), coarse kappa-carbides would precipitate around the grain boundaries, which made the material extremely brittle and decreased the wear resistance. The surface hardening showed Lomer-Cottrell locks, high density of dislocation tangles and dislocation walls; neither martensite nor mechanical twins were observed under the low impact energy condition for both heat treatment processes.
引用
收藏
页数:10
相关论文
共 30 条
[1]   On the comparison of the abrasive wear behavior of aluminum alloyed and standard Hadfield steels [J].
Abbasi, Majid ;
Kheirandish, Shahram ;
Kharrazi, Yousef ;
Hejazi, Jalal .
WEAR, 2010, 268 (1-2) :202-207
[2]   The fracture and plastic deformation of aluminum alloyed Hadfield steels [J].
Abbasi, Majid ;
Kheirandish, Shahram ;
Kharrazi, Yosef ;
Hejazi, Jalal .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 513-14 :72-76
[3]   A first evaluation of the abrasive wear of an austenitic FeMnAlC steel [J].
Acselrad, O ;
de Souza, AR ;
Kalashnikov, IS ;
Camargo, SS .
WEAR, 2004, 257 (9-10) :999-1005
[4]  
Allahkaram SR, 2008, INT J ENG-IRAN, V21, P55
[5]  
Buckholz S., 2013, The Influence of Aluminum and Carbon on the Abrasion Resistance of High Manganese Steels
[6]   The role of dense dislocation walls on the deformation response of aluminum alloyed hadfield steel polycrystals [J].
Canadinc, D. ;
Sehitoglu, H. ;
Maier, H. J. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 454 :662-666
[7]   Excellent combination of strength and ductility in an Fe-9Al-28Mn-1.8C alloy [J].
Chang, K. M. ;
Chao, C. G. ;
Liu, T. F. .
SCRIPTA MATERIALIA, 2010, 63 (02) :162-165
[8]   Effects of C and Cr content on high-temperature microstructures of Fe-9Al-30Mn-xC-yCr alloys [J].
Chen, May-Show ;
Cheng, Hsin-Chung ;
Huang, Chiung-Fang ;
Chao, Chih-Yeh ;
Ou, Keng-Liang ;
Yu, Chih-Hua .
MATERIALS CHARACTERIZATION, 2010, 61 (02) :206-211
[9]  
Choi K., 2013, SCRIPTA MATER, V63, P1028
[10]   MECHANISM OF WORK-HARDENING IN HADFIELD MANGANESE STEEL [J].
DASTUR, YN ;
LESLIE, WC .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1981, 12 (05) :749-759