Surface and line-edge roughness in acid-breakable resin-based positive resist

被引:3
作者
Sakamizu, T [1 ]
Shiraishi, H [1 ]
机构
[1] Hitachi Ltd, Cent Res Lab, Tokyo 1858601, Japan
来源
ADVANCES IN RESIST TECHNOLOGY AND PROCESSING XX, PTS 1 AND 2 | 2003年 / 5039卷
关键词
positive resist; acid-breakable resin; line-edge roughness; surface roughness;
D O I
10.1117/12.483773
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A positive chemical amplification resist based on acid-catalyzed fragmentation of acetal groups in its main-chain has been developed as a means for reducing line-edge roughness. The resist consists of an acid-generator, an. acid-diffusion controller and an acid-breakable (AB) resin that is synthesized through a co-condensation reaction between polyphenol and aromatic multi-functional vinylether compound. The effects of the fractionation of AB resins on resin properties and line-edge roughness (LER) are evaluated. Although AB resins have wide molecular-weight distributions, the density of acetal groups in this AB resin is found to be almost constant except in the lower molecular-weight components. The resist with a fractionated resin from which such components removed provides the high resolution of 60-nm line-and-space (US) patterns with fairly low LER. AFM analysis shows the surface roughness (SR) for the resist with the fractionated resin is smaller than that for a resist using non-fractionated AB resin, and that the SR value is not altered throughout the range of exposure doses up to just below the beginning of dissolution. By using the fractionated AB resin, the AB resin-based resist (ABR) is capable of forming sub-100 nm US patterns with less than 5 nm of LER (3sigma).
引用
收藏
页码:492 / 501
页数:10
相关论文
共 20 条
  • [1] ARAI T, 1997, J PHOTOPOLYM SCI TEC, V10, P625
  • [2] Process dependence of roughness in a positive-tone chemically amplified resist
    He, D
    Cerrina, F
    [J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 1998, 16 (06): : 3748 - 3751
  • [3] TETRAHYDROPYRANYL-PROTECTED AND FURANYL-PROTECTED POLYHYDROXYSTYRENE IN CHEMICAL AMPLIFICATION SYSTEMS
    HESP, SAM
    HAYASHI, N
    UENO, T
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 1991, 42 (04) : 877 - 883
  • [4] Deep-ultraviolet interferometric lithography as a tool for assessment of chemically amplified photoresist performance
    Hinsberg, W
    Houle, FA
    Hoffnagle, J
    Sanchez, M
    Wallraff, G
    Morrison, M
    Frank, S
    [J]. JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, 1998, 16 (06): : 3689 - 3694
  • [5] Fine pit pattern formation by EB-writing for a high density optical recording
    Hosaka, S
    Koyanagi, H
    Katoh, K
    Isshiki, F
    Suzuki, T
    Miyamoto, M
    Arimoto, A
    Maeda, T
    [J]. MICROELECTRONIC ENGINEERING, 2001, 57-8 : 223 - 230
  • [6] Creation of low molecular-weight organic resists for nanometer lithography
    Kadota, T
    Yoshiiwa, M
    Kageyama, H
    Wakaya, F
    Gamo, K
    Shirota, Y
    [J]. ADVANCES IN RESIST TECHNOLOGY AND PROCESSING XVIII, PTS 1 AND 2, 2001, 4345 : 891 - 902
  • [7] Novel molecular resists based on inclusion complex of cyclodextrin
    Kim, JB
    Kwon, YG
    Yun, HJ
    Choi, JH
    [J]. ADVANCES IN RESIST TECHNOLOGY AND PROCESSING XIX, PTS 1 AND 2, 2002, 4690 : 837 - 845
  • [8] Effect of process parameters on pattern edge roughness of chemically-amplified resists
    Koh, HP
    Lin, QY
    Hu, X
    Chan, L
    [J]. ADVANCES IN RESIST TECHNOLOGY AND PROCESSING XVII, PTS 1 AND 2, 2000, 3999 : 240 - 251
  • [9] Line edge roughness in positive-tone chemically amplified resists: Effect of additives and processing conditions
    Lin, QH
    Goldfarb, DL
    Angelopoulos, M
    Sriram, SR
    Moore, JS
    [J]. ADVANCES IN RESIST TECHNOLOGY AND PROCESSING XVIII, PTS 1 AND 2, 2001, 4345 : 78 - 86
  • [10] Toward controlled resist line edge roughness: Material origin of line edge roughness in chemically amplified positive-tone resists
    Lin, QH
    Sooriyakumaran, R
    Huang, WS
    [J]. ADVANCES IN RESIST TECHNOLOGY AND PROCESSING XVII, PTS 1 AND 2, 2000, 3999 : 230 - 239