The Clathrate Ba8-xSi46 Revisited: Preparation Routes, Electrical and Thermal Transport Properties

被引:21
作者
Castillo, Rodrigo [1 ]
Schnelle, Walter [1 ]
Bobnar, Matej [1 ]
Burkhardt, Ulrich [1 ]
Boehme, Bodo [1 ]
Baitinger, Michael [1 ]
Schwarz, Ulrich [1 ]
Grin, Yuri [1 ]
机构
[1] Max Planck Inst Chem Phys Fester Stoffe, D-01187 Dresden, Germany
来源
ZEITSCHRIFT FUR ANORGANISCHE UND ALLGEMEINE CHEMIE | 2015年 / 641卷 / 02期
关键词
Intermetallic clathrate; Barium; Silicon; Superconductivity; Electrical conductivity; Seebeck coefficient; Thermal conductivity; HIGH-PRESSURE; SUPERCONDUCTIVITY; LOCALIZABILITY; DECOMPOSITION; BA8SI46;
D O I
10.1002/zaac.201500001
中图分类号
O61 [无机化学];
学科分类号
070301 ; 081704 ;
摘要
The clathrate-I Ba8-xSi46 was manufactured from BaSi2 and a-Si by high-pressure high-temperature synthesis at 5 GPa and 900 degrees C and by redox reaction from Ba4Li2Si6. The transport properties were measured on specimens from the high-pressure high-temperature synthesis. The composition of the Ba8-xSi46 phase [space group Pm (3) over bar n, a = 10.3051(1)angstrom] corresponds to x = 0.8(2) according to the refined lattice parameter, the value determined from full-profile refinement of powder X-ray diffraction data amounts to x = 0.73(1), and the chemical analysis results in x = 1.0(1), yielding the average composition Ba7.2(2)Si46. The electrical transport properties of the phase with x = 0.8 were determined in the temperature range 2-300 K using a polycrystalline bulk specimen. The material is a metallic conductor with rho(300 K) = 3.3 mu Omega m and S(300 K) = -6.8 mu V K-1. The thermal conductivity shows a relatively large -for an intermetallic clathrate value of about 8 W.K-1 m(-1).
引用
收藏
页码:206 / 213
页数:8
相关论文
共 44 条
  • [1] WinCSD: software package for crystallographic calculations (Version 4)
    Akselrud, Lev
    Grin, Yuri
    [J]. JOURNAL OF APPLIED CRYSTALLOGRAPHY, 2014, 47 : 803 - 805
  • [2] LINEAR METHODS IN BAND THEORY
    ANDERSEN, OK
    [J]. PHYSICAL REVIEW B, 1975, 12 (08): : 3060 - 3083
  • [3] Thermoelectric properties of Ba8AuxGe46-x clathrate compounds
    Anno, H
    Hokazono, M
    Takakura, H
    Matsubara, K
    [J]. ICT: 2005 24TH INTERNATIONAL CONFERENCE ON THERMOELECTRICS, 2005, : 102 - 105
  • [4] Baitinger M, 2014, SPRINGER SER MATER S, V199, P35, DOI 10.1007/978-94-017-9127-4_2
  • [5] Intrinsic Electrical and Thermal Properties from Single Crystals of Na24Si136
    Beekman, M.
    Schnelle, W.
    Borrmann, H.
    Baitinger, M.
    Grin, Yu.
    Nolas, G. S.
    [J]. PHYSICAL REVIEW LETTERS, 2010, 104 (01)
  • [6] ESDS AND ESTIMATED PROBABLE-ERROR OBTAINED IN RIETVELD REFINEMENTS WITH LOCAL CORRELATIONS
    BERAR, JF
    LELANN, P
    [J]. JOURNAL OF APPLIED CRYSTALLOGRAPHY, 1991, 24 : 1 - 5
  • [7] Bhattacharya A., 2014, VERH DTSCH PHYS GES
  • [8] High temperature thermoelectric properties of the type-I clathrate Ba8AuxSi46-x
    Candolfi, C.
    Aydemir, U.
    Baitinger, M.
    Oeschler, N.
    Steglich, F.
    Grin, Yu
    [J]. JOURNAL OF APPLIED PHYSICS, 2012, 111 (04)
  • [9] Cros C., 1970, J SOLID STATE CHEM, V2, P570, DOI [DOI 10.1016/0022-4596(70)90053-8, 10.1016/0022-4596(70)90053-8]
  • [10] de Boissieu M., 2014, PHYS REV LETT, V113