Microstructure, precipitates and hardness of selectively laser melted AlSi10Mg alloy before and after heat treatment

被引:228
作者
Zhou, Le [1 ,2 ]
Mehta, Abhishek [2 ]
Schulz, Esin [2 ]
McWilliams, Brandon [3 ]
Cho, Kyu [3 ]
Sohn, Yongho [1 ,2 ]
机构
[1] Univ Cent Florida, Adv Mat Proc & Anal Ctr, Orlando, FL 32816 USA
[2] Univ Cent Florida, Dept Mat Sci & Engn, Orlando, FL 32816 USA
[3] US Amy Res Lab, Weap & Mat Res Directorate, Aberdeen Proving Ground, MD 21005 USA
关键词
Selective laser melting; AlSi10Mg alloy; Precipitates; Microstructure; Hardness; MECHANICAL-PROPERTIES; TENSILE PROPERTIES; BETA-ALFESI; CRYSTAL-STRUCTURE; YIELD STRENGTH; SI; MG; PHASE; BEHAVIOR; ALPHA-AL(FEMN)SI;
D O I
10.1016/j.matchar.2018.04.022
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The microstructure and precipitates within selectively laser melted (SLM) AlSi10Mg alloys in the as-built state and after T6 heat treatment were examined and correlated to the hardness evolution. The as-built alloy exhibited columnar patterns perpendicular to the build-direction and fish-scale pattern along the build-direction originating from the melt pool. The microstructure consisted of fine Al cells and eutectic structure with up to 4 mu m in size. Tiny needle-like Si particles with highly faulted structure were identified within the Al cells and formed semi-coherent interface with the matrix. Nanoscale Si particles and pi-Al8Si6Mg3Fe phase were observed to segregate along the cell and grain boundary. Solution heat treatment (SHT) at 520 degrees C resulted in the dissolution of Al cellular microstructure. Precipitation and coarsening of the Si particles occurred, while the aspect ratio of Si particles remained nearly constant. The pi-Al8Si6Mg3Fe phase decomposed into plate-shaped beta-Al5SiFe. The artificial aging (AA) at 160 degrees C did not alter the microstructure but led to the formation of metastable Mg2Si precipitates. The GP zones and beta '' were identified through transmission electron microscopy after AA of 6 h, and beta '' existed up to AA of 24 h. The hardness decreased after SHT due to the coarsening of the microstructure and reduced solid solution hardening. Hardness reached maximum magnitude after AA of 6-10 h due to the precipitation hardening, and remained relatively unchanged up to AA of 24 h. Microstructure and/or hardness of gas atomized powders and bulk cast AlSi10Mg alloys were also examined as references.
引用
收藏
页码:5 / 17
页数:13
相关论文
共 51 条
[1]   The microstructure and mechanical properties of selectively laser melted AlSi10Mg: The effect of a conventional T6-like heat treatment [J].
Aboulkhair, Nesma T. ;
Maskery, Ian ;
Tuck, Chris ;
Ashcroft, Ian ;
Everitt, Nicola M. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 667 :139-146
[2]   On the Precipitation Hardening of Selective Laser Melted AlSi10Mg [J].
Aboulkhair, Nesma T. ;
Tuck, Chris ;
Ashcroft, Ian ;
Maskery, Ian ;
Everitt, Nicola M. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (08) :3337-3341
[3]   The crystal structure of the β" phase in Al-Mg-Si alloys [J].
Andersen, SJ ;
Zandbergen, HW ;
Jansen, J ;
Traeholt, C ;
Tundal, U ;
Reiso, O .
ACTA MATERIALIA, 1998, 46 (09) :3283-3298
[4]  
[Anonymous], 2014, P SOL FREEF FABR SFF
[5]   Effect of Er additions on ambient and high-temperature strength of precipitation-strengthened Al-Zr-Sc-Si alloys [J].
Booth-Morrison, Christopher ;
Seidman, David N. ;
Dunand, David C. .
ACTA MATERIALIA, 2012, 60 (08) :3643-3654
[6]   Additive manufactured AlSi10Mg samples using Selective Laser Melting (SLM): Microstructure, high cycle fatigue, and fracture behavior [J].
Brandl, Erhard ;
Heckenberger, Ulrike ;
Holzinger, Vitus ;
Buchbinder, Damien .
MATERIALS & DESIGN, 2012, 34 :159-169
[7]  
CAHOON JR, 1971, METALL TRANS, V2, P1979
[8]   Predictive equations of the tensile properties based on alloy hardness and microstructure for an A356 gravity die cast cylinder head [J].
Ceschini, L. ;
Morri, Alessandro ;
Morri, Andrea ;
Pivetti, G. .
MATERIALS & DESIGN, 2011, 32 (03) :1367-1375
[9]   Strength and strain hardening of a selective laser melted AlSi10Mg alloy [J].
Chen, B. ;
Moon, S. K. ;
Yao, X. ;
Bi, G. ;
Shen, J. ;
Umeda, J. ;
Kondoh, K. .
SCRIPTA MATERIALIA, 2017, 141 :45-49
[10]   Precipitation phenomena in ultrafine grained Al-Mg-Si alloy with heterogeneous microstructure [J].
Chrominski, Witold ;
Lewandowska, Malgorzata .
ACTA MATERIALIA, 2016, 103 :547-557