Evolution of surface roughness of some metallic materials in cavitation erosion

被引:69
作者
Chiu, KY [1 ]
Cheng, FT
Man, HC
机构
[1] Hong Kong Polytech Univ, Dept Appl Phys, Kowloon, Hong Kong, Peoples R China
[2] Hong Kong Polytech Univ, Dept Ind & Syst Engn, Kowloon, Hong Kong, Peoples R China
关键词
cavitation erosion; surface roughness; profilometry; incubation period; erosion rate;
D O I
10.1016/j.ultras.2005.03.009
中图分类号
O42 [声学];
学科分类号
070206 ; 082403 ;
摘要
The evolution of surface roughness of three common metallic materials (316L stainless steel, CP titanium, and brass) in ultrasonic vibratory cavitation tests was monitored using profilometric measurements. Three stages of roughness change, based on the rate of change of the mean surface roughness d(R-a)/dt, may be identified. In stage I (initial stage), R-a increases almost linearly with the test time; in stage II (transition stage), the rate decreases until stage III (steady-state stage) is reached, in which R, remains unchanged. Concurrent measurements of mass loss in the ultrasonic cavitation test indicated that stage I approximately coincides with the incubation stage, stage II approximately coincides with the acceleration stage, and stage III approximately coincides with the maximum erosion rate stage as defined by ASTM Standard G 32. Compared with conventional mass loss measurements in assessing material degradation in cavitation erosion, surface roughness measurements provide an alternative and convenient method which possesses several advantages. In the first place, change in surface roughness provides information of material response before mass loss is detected. Secondly, there is no restriction of the size of the component, while weighing is suitable for small samples only. Thirdly, mass loss reflects erosion of the whole surface under cavitation attack, and the mean depth of penetration or erosion only gives an average loss, while in roughness measurement, damage in specific locations may be studied. The present study indicates that roughness measurement may constitute a practical method for monitoring damage in industrial ultrasonic cleaners. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:713 / 716
页数:4
相关论文
共 50 条
[31]   Cavitation erosion of electrostatic spray polyester coatings with different surface finish [J].
Szala, Miroslaw ;
Swietlicki, Aleksander ;
Sofinska-Chmiel, Weronika .
BULLETIN OF THE POLISH ACADEMY OF SCIENCES-TECHNICAL SCIENCES, 2021, 69 (04)
[32]   Cavitation erosion behaviour of Zr-based bulk metallic glasses [J].
Drozdz, D. ;
Wunderlich, R. K. ;
Fecht, H. -J. .
WEAR, 2007, 262 (1-2) :176-183
[33]   Investigation on Cavitation-Erosion Damage with the Cavitation Amplitude of Al Alloy Materials in Seawater [J].
Yang, Ye-Jin ;
Kim, Seong-Jong .
CORROSION SCIENCE AND TECHNOLOGY-KOREA, 2020, 19 (05) :250-258
[34]   Formation and progression of cavitation erosion surface for long exposure [J].
Hattori, Shuji ;
Ogiso, Takaaki ;
Minami, Yusuke ;
Yamada, Ikuo .
WEAR, 2008, 265 (11-12) :1619-1625
[35]   Formation and progression of cavitation erosion surface for long exposure [J].
Hattori, Shuji ;
Ogiso, Takaaki ;
Minami, Yusuke ;
Yamada, Ikuo .
Nihon Kikai Gakkai Ronbunshu, A Hen/Transactions of the Japan Society of Mechanical Engineers, Part A, 2007, 73 (08) :912-917
[36]   Cavitation erosion in waters having different surface tensions [J].
Iwai, Y ;
Li, SC .
WEAR, 2003, 254 (1-2) :1-9
[37]   Combined wear of slurry erosion, cavitation erosion, and corrosion on the simulated ship surface [J].
Liang, Liang ;
Pang, Youxia ;
Tang, Yong ;
Zhang, Hao ;
Liu, Hui ;
Liu, Yu .
ADVANCES IN MECHANICAL ENGINEERING, 2019, 11 (03)
[38]   The influence of alumina crystal structures on the morphology and surface erosion of PMMA composite materials exposed to cavitation testing [J].
Vuksanovic, Marija M. ;
Tomic, Natasa Z. ;
Gajic-Kvascev, Maja ;
Djokic, Veljko R. ;
Dojcinovic, Marina ;
Husovic, Tatjana Volkov ;
Heinemann, Radmila Jancic .
WEAR, 2019, 436
[39]   The Synergistic Effects of Cavitation Erosion–Corrosion in Ship Propeller Materials [J].
Basumatary J. ;
Nie M. ;
Wood R.J.K. .
Journal of Bio- and Tribo-Corrosion, 2015, 1 (2)
[40]   A systematic study into the cavitation erosion test for marine propeller materials by cavitating jet technique [J].
Usta, Onur ;
Koksal, Cagatay Sabri ;
Korkut, Emin .
OCEAN ENGINEERING, 2023, 284