A novel bilayered Sr0.6La0.4TiO3/La0.8Sr0.2MnO3 interconnector for anode-supported tubular solid oxide fuel cell via slurry-brushing and co-sintering process

被引:17
作者
Xu, Yanjie [1 ]
Wang, Shaorong [1 ]
Liu, Renzhu [1 ]
Wen, Tinglian [1 ]
Wen, Zhaoyin [1 ]
机构
[1] Chinese Acad Sci SICCAS, Shanghai Inst Ceram, CAS Key Lab Mat Energy Convers, Shanghai 200050, Peoples R China
关键词
Tubular solid oxide fuel cell; Anode-supported; Interconnector; Slurry-brushing; Co-sintering; DOPED LACRO3; SOFC; TEMPERATURE; FABRICATION; PEROVSKITE; EXPANSION; BEHAVIOR;
D O I
10.1016/j.jpowsour.2010.07.088
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Considering that conventional lanthanum chromate (LaCrO3) interconnector is hard to be co-sintered with green anode, we have fabricated a novel bilayered interconnector which consists of La-doped SrTiO3 (Sr0.6La0.4TiO3) and Sr-doped lanthanum manganite (La0.8Sr0.2MnO3). Sr0.6La0.4TiO3 is conductive and stable in reducing atmosphere, locating on the anode side; while La0.8Sr0.2MnO3 is on the cathode side. A slurry-brushing and co-sintering method is applied; the Sr0.6La0.4TiO3 and La0.8Sr0.2MnO3 slurries are successively brushed onto green anode specimen, followed by co-firing course to form a dense bilayered Sr0.6La0.4TiO3/La0.8Sr0.2MnO3 interconnector. For operating with humidified hydrogen and oxygen at 900 degrees C, the ohmic resistances between anode and cathode/interconnector are 0.33 Omega cm(2) and 0.186 Omega cm(2), respectively. The maximum power density is 290 mW cm(-2) for a cell with interconnector, and 420 mW cm(-2) for a cell without it, which demonstrates that nearly 70% of the power output can be achieved using this bilayered Sr0.6La0.4TiO3/La0.8Sr0.2MnO3 interconnector. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:1338 / 1341
页数:4
相关论文
共 50 条
[31]   Investigation of La0.6Sr0.4Co1-xNixO3-d (x1/40, 0.2, 0.4, 0.6, 0.8) catalysts on solid oxide fuel cells anode for biogas dry reforming [J].
Yao, Yao ;
Chen, Ting ;
Zhou, Zhihao ;
Huang, Zuzhi ;
Cai, Peijun ;
Xu, Lang ;
Wang, Shaorong .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (66) :28645-28654
[32]   Evaluation of La0.6Sr0.4Co0.2Fe0.8O3-δ as a Potential Cathode for Proton-Conducting Solid Oxide Fuel Cell [J].
Ismail, Ismariza ;
Osman, Nafisah ;
Jani, Abdul Mutalib Md .
SAINS MALAYSIANA, 2018, 47 (02) :387-391
[33]   Crystal Structure and Electrochemical Performance of La0.6Sr0.4Co0.2Fe0.8-xScxO3-δ Cathode Materials for Solid Oxide Fuel Cell [J].
Cai Changkun ;
Xie Manyi ;
Lin, Wang ;
Ke, Xue ;
Jun, Peng ;
Bao Jinxiao ;
An Shengli .
RARE METAL MATERIALS AND ENGINEERING, 2023, 52 (02) :601-608
[34]   A new symmetric solid-oxide fuel cell with La0.8Sr0.2Sc0.2Mn0.8O3-δ perovskite oxide as both the anode and cathode [J].
Zheng, Yao ;
Zhang, Chunming ;
Ran, Ran ;
Cai, Rui ;
Shao, Zongping ;
Farrusseng, D. .
ACTA MATERIALIA, 2009, 57 (04) :1165-1175
[35]   Improving La0.6Sr0.4Co0.8Fe0.2O3-δ infiltrated solid oxide fuel cell cathode performance through precursor solution desiccation [J].
Burye, Theodore E. ;
Nicholas, Jason D. .
JOURNAL OF POWER SOURCES, 2015, 276 :54-61
[36]   Effect of Sintering Temperature on the Behavior of Oxygen Permeation for La0.6Sr0.4Co0.2Fe0.8O3-δ Tubular Membraness [J].
Fan, Chuangang ;
Wu, Riming ;
Pei, Lizhai ;
Zhang, Qianfeng .
CHINESE CERAMICS COMMUNICATIONS, 2010, 105-106 :643-646
[37]   Silver infiltrated La0.6Sr0.4Co0.2Fe0.8O3 cathodes for intermediate temperature solid oxide fuel cells [J].
Sakito, Y. ;
Hirano, A. ;
Imanishi, N. ;
Takeda, Y. ;
Yamamoto, O. ;
Liu, Y. .
JOURNAL OF POWER SOURCES, 2008, 182 (02) :476-481
[38]   Magnetron-sputtered La0.6Sr0.4Co0.2Fe0.8O3 nanocomposite interlayer for solid oxide fuel cells [J].
Solovyev, A. A. ;
Ionov, I. V. ;
Shipilova, A. V. ;
Kovalchuk, A. N. ;
Syrtanov, M. S. .
JOURNAL OF NANOPARTICLE RESEARCH, 2017, 19 (03)
[39]   Fabrication and characterization of anode-supported single chamber solid oxide fuel cell based on La0.6Sr0.4Co0.2Fe0.8O3-δ-Ce0.9Gd0.1O1.95 composite cathode [J].
Sun, L. P. ;
Rieu, M. ;
Viricelle, J. P. ;
Pijolat, C. ;
Zhao, H. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2014, 39 (02) :1014-1022
[40]   Degradation Analysis of Long-Term Solid Oxide Fuel Cell Stacks with Respect to Chromium Poisoning in La0.58Sr0.4Co0.2Fe0.8O3-δ and La0.6Sr0.4CoO3-δ Cathodes [J].
Fang, Qingping ;
Menzler, Norbert H. ;
Blum, Ludger .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2021, 168 (10)