Characterization and Properties of Reactive Poly (Lactic Acid)/Ethylene-Vinyl Alcohol Copolymer Blends with Chain-Extender

被引:9
作者
Wu, Jyh-Horng [1 ]
Wu, Chien-Pang [1 ]
Kuo, M. C. [2 ]
Tsai, Yuhsin [3 ]
机构
[1] Ind Technol Res Inst, Mat & Chem Res Labs, Tainan 73445, Taiwan
[2] Kun Shan Univ, Dept Mat Engn, 195 Kunda Rd, Tainan 71003, Taiwan
[3] China Med Univ, Sch Chinese Med, 91 Hsueh Shih Rd, Taichung 40402, Taiwan
关键词
Poly (lactic acid); Ethylene-vinyl alcohol copolymer; Chain extender; Biaxially stretching; POLY(LACTIC ACID); CRYSTALLIZATION BEHAVIOR; PHYSICAL-PROPERTIES; LACTIC-ACID; COMPATIBILIZATION; POLY(L-LACTIDE); PLASTICIZERS;
D O I
10.1007/s10924-016-0755-x
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
A hydrophilic copolymer, ethylene-vinyl alcohol (EVOH), was incorporated into the poly(lactic acid) (PLA) matrix to improve the barrier property of PLA through twin-screw extrusion rather than the typical coextrusion process. A chain extender, poly[(ethylene)-co-(methyl acrylate)-co-(glycidyl methacrylate)] (PEMG), was used to reduce the probability of the thermal degradation of PLA during melt compounding. Biaxial stretching was used to enhance the microstructure and barrier property of PLA-PEMG/EVOH films. Experimentally, PEMG considerably reduced the probability of the thermal degradation of the PLA-PEMG sample. Biaxial stretching increased the tensile strength and decreased the value of elongation at break of the PLA-PEMG/EVOH80 (PLA/EVOH 100/80) film. Because of the efficient blending of PLA/EVOH in the twin-screw extruder, the dispersion of EVOH in the PLA matrix revealed homogeneous dispersion with a domain size of 1-5 mu m. EVOH effectively improved the water vapour transmission rate (WVTR) of PLA through melt blending. Blending PLA-PEMG with EVOH substantially decreased the WVTR from 250 cc-20 mu m/m(2)-day-atm for neat PLA to approximately 65 cc-20 mu m/m(2)-day-atm for the PLA-PEMG/EVOH80 film, a decrease of approximately 74 % compared with neat PLA. Moreover, the WVTR decreased further from 65 cc-20 mu m/m(2)-day-atm for the unstretched PLA-PEMG/EVOH80 film to 6.3 cc-20 mu m/m(2)-day-atm for the film stretched at a stretch ratio of 3.5 x 3.5 and at 100 %/s, a decrease of approximately 90 % compared with neat PLA.
引用
收藏
页码:129 / 138
页数:10
相关论文
共 31 条
  • [21] Ruckenstein E, 1998, J APPL POLYM SCI, V69, P1429, DOI 10.1002/(SICI)1097-4628(19980815)69:7<1429::AID-APP18>3.0.CO
  • [22] 2-O
  • [23] Tsuji H, 1996, J APPL POLYM SCI, V60, P2367, DOI 10.1002/(SICI)1097-4628(19960627)60:13<2367::AID-APP8>3.0.CO
  • [24] 2-C
  • [25] Reactive compatibilization of biodegradable blends of poly(lactic acid) and poly(ε-caprolactone)
    Wang, L
    Ma, W
    Gross, RA
    McCarthy, SP
    [J]. POLYMER DEGRADATION AND STABILITY, 1998, 59 (1-3) : 161 - 168
  • [26] Polyethylene-poly(L-lactide) diblock copolymers: Synthesis and compatibilization of poly(L-lactide)/polyethylene blends
    Wang, YB
    Hillmyer, MA
    [J]. JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 2001, 39 (16) : 2755 - 2766
  • [27] Physical properties and crystallization behavior of silica particulates reinforced poly(lactic acid) composites
    Wu, Jyh-Hong
    Yen, Ming-Shien
    Kuo, M. C.
    Chen, Bo-Hua
    [J]. MATERIALS CHEMISTRY AND PHYSICS, 2013, 142 (2-3) : 726 - 733
  • [28] Physical properties and crystallization behavior of poly(lactide)/poly(methyl methacrylate)/silica composites
    Wu, Jyh-Horng
    Kuo, M. C.
    Chen, Chien-Wen
    [J]. JOURNAL OF APPLIED POLYMER SCIENCE, 2015, 132 (32)
  • [29] Effect of Biaxial Stretching on Thermal Properties, Shrinkage and Mechanical Properties of Poly (Lactic Acid) Films
    Wu, Jyh-Horng
    Yen, Ming-Shien
    Wu, Chien-Pang
    Li, Chia-Hao
    Kuo, M. C.
    [J]. JOURNAL OF POLYMERS AND THE ENVIRONMENT, 2013, 21 (01) : 303 - 311
  • [30] Polyurethane toughened polylactide
    Yuan, YM
    Ruckenstein, E
    [J]. POLYMER BULLETIN, 1998, 40 (4-5) : 485 - 490