Interlaminar fracture toughness of aerospace-grade carbon fibre reinforced plastics interleaved with thermoplastic veils

被引:59
|
作者
Quan, Dong [1 ]
Bologna, Francesca [1 ]
Scarselli, Gennaro [2 ]
Ivankovic, Alojz [1 ]
Murphy, Neal [1 ]
机构
[1] Univ Coll Dublin, Sch Mech & Mat Engn, Dublin, Ireland
[2] Univ Salento, Dept Innovat Engn, Lecce, Italy
关键词
Polymer-matrix composites (PMCs); Thermoplastic veils; Fracture toughness; Fractography; MODE-I; NONWOVEN VEILS; FIBER/EPOXY COMPOSITES; MECHANICAL-PROPERTIES;
D O I
10.1016/j.compositesa.2019.105642
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This work investigates the toughening performance of thermoplastic veils when used to interlay aerospace-grade CFRPs. Veils based on Polyethylene-terephthalate (PET), Polyphenylene-sulfide (PPS) and Polyamide-12 (PA) fibres (similar to 10 mu m in diameter) were used as interlayers of unidirectional (UD), non-crimp fabric (NCF) and 5-Harness satin weave (5H) carbon fibre/epoxy laminates. During a hot curing process of the laminates, the PET and PPS veils remained in a fibrous form, and the PA veils melted. This resulted in different toughening mechanisms, i.e. interlaying the PET and PPS veils introduced extensive thermoplastic fibre bridging, and adding the PA veils improved the fracture toughness of the epoxy matrix. The different toughening mechanisms of the veils, together with the different fracture mechanisms of the laminates, dramatically affected the toughening levels. In general, the PET and PPS veils were more effective for toughening the UD laminates, and the PA veils were superior for the NCF and 5H laminates.
引用
收藏
页数:11
相关论文
共 50 条
  • [31] Fracture toughness of fibre-reinforced plastics:: Effect of fibre type and temperature
    Ünal, A
    PROCESSING AND FABRICATION OF ADVANCED MATERIALS V, 1996, : 431 - 442
  • [32] Interlaminar fracture toughness of selectively stitched thick carbon fibre reinforced polymer fabric composite laminates
    Ishai, O
    PLASTICS RUBBER AND COMPOSITES, 2000, 29 (03) : 134 - 143
  • [33] A review on mode-I interlaminar fracture toughness of fibre reinforced composites
    Nasuha, N.
    Azmi, A. I.
    Tan, C. L.
    INTERNATIONAL CONFERENCE ON APPLICATIONS AND DESIGN IN MECHANICAL ENGINEERING (ICADME 2017), 2017, 908
  • [34] Influence of interlaminar fracture toughness on impact resistance of glass fibre reinforced polymers
    Kuboki, T
    Jar, PYB
    Forest, TW
    COMPOSITES SCIENCE AND TECHNOLOGY, 2003, 63 (07) : 943 - 953
  • [35] Determination of the interlaminar fracture toughness of glass-fiber-reinforced plastics on ring segments
    Solodilov, VI
    Bazhenov, SL
    Gorbatkina, YA
    Kuperman, AM
    MECHANICS OF COMPOSITE MATERIALS, 2003, 39 (05) : 407 - 414
  • [36] Determination of the Interlaminar Fracture Toughness of Glass-Fiber-Reinforced Plastics on Ring Segments
    V. I. Solodilov
    S. L. Bazhenov
    Yu. A. Gorbatkina
    A. M. Kuperman
    Mechanics of Composite Materials, 2003, 39 : 407 - 414
  • [37] Micromechanics of interlaminar fracture in carbon fibre reinforced plastics at multidirectional ply interfaces under static and cyclic loading
    Singh, S
    Greenhalgh, E
    PLASTICS RUBBER AND COMPOSITES PROCESSING AND APPLICATIONS, 1998, 27 (05): : 220 - 226
  • [38] Interlaminar fracture toughness behaviour of carbon fibre reinforced polymer with epoxy-dicarboxylic acid vitrimer matrix
    Tangthana-umrung, Kanokporn
    Gresil, Matthieu
    COMPOSITES COMMUNICATIONS, 2022, 32
  • [39] Study of Interlaminar Fracture Toughness and Flexural Properties of Carbon Fibre Composites Reinforced with Polyethersulfone/Graphene Oxide Films
    Wang, Gongdong
    Yu, Mingchi
    Wang, Meng
    Liu, Xueqing
    Zhang, Hongxiang
    He, Long
    COMPOSITES COMMUNICATIONS, 2024, 51
  • [40] Interlaminar Fracture Toughness of Carbon Fibre-Reinforced Polymer Laminates With Nano- and Micro-Fillers
    Kostopoulos, V.
    Karapappas, P.
    Loutas, T.
    Vavouliotis, A.
    Paipetis, A.
    Tsotra, P.
    STRAIN, 2011, 47 : E269 - E282