The fracture properties of a fibre-metal laminate based on magnesium alloy

被引:137
|
作者
Cortés, P [1 ]
Cantwell, WJ [1 ]
机构
[1] Univ Liverpool, Dept Engn, Liverpool L69 3GH, Merseyside, England
关键词
fatigue; fibre-metal laminates;
D O I
10.1016/j.compositesb.2005.06.002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A range of fibre-metal laminates (FML) based on a lightweight magnesium alloy have been manufactured and tested. Two types of composite reinforcement have been investigated, a woven carbon fibre reinforced epoxy and a unidirectional glass fibre reinforced polypropylene. Initial tests using the single cantilever beam geometry (SCB) have shown that little or no surface treatment is required to achieve a relatively strong bond between the composite plies and the magnesium alloy. Tests on both types of laminate indicated that increasing the volume fraction of composite, V-C in the FML resulted in a significant increase in its tensile strength. Similar tests showed that the addition of the woven carbon fibre/epoxy plies did not have any effect on the Young's modulus of the FML whereas increasing the V-C of the glass/polypropylene plies resulted in a continuous decrease in the modulus of these thermoplastic-matrix systems. Fatigue tests on both types of laminate highlighted the positive contribution of the composite plies in the FMLs. Here, the crack growth rates in centre-notched tension specimens were significantly lower in the FMLs than in the plain magnesium alloy system. Low velocity impact tests on the FMLs highlighted their excellent energy-absorbing characteristics relative to two aluminium-based FMLs. The specific perforation energy of the glass fibre/PP laminate was higher than that offered by a similar aluminium alloy FML and significantly higher than that for a glass reinforced epoxy/aluminium FML. Here, extensive delamination and shear fracture in the outer magnesium alloy plies were found to contribute to the energy-absorbing capacity of these laminates. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:163 / 170
页数:8
相关论文
共 50 条
  • [1] The influence of cooling rate on the fracture properties of a thermoplastic-based fibre-metal laminate
    Guillén, JF
    Cantwell, WJ
    JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 2002, 21 (08) : 749 - 772
  • [2] The fracture properties of fibre-metal laminates based on glass fibre reinforced polyamide
    Guillen, F
    Cantwell, WJ
    ADVANCED COMPOSITES LETTERS, 2000, 9 (03) : 211 - 216
  • [3] Static pressure loading of fibre-metal laminate plates
    Simmons, MC
    Schleyer, G
    Cantwell, WJ
    Birch, RS
    IMPACT LOADING OF LIGHTWEIGHT STRUCTURES, 2005, 49 : 481 - 493
  • [4] Interfacial fracture of the fibre-metal laminates based on fibre reinforced thermoplastics
    Abdullah, M. R.
    Prawoto, Y.
    Cantwell, W. J.
    MATERIALS & DESIGN, 2015, 66 : 446 - 452
  • [5] Interfacial fracture in fibre-metal laminates based on glass fibre reinforced polypropylene
    Reyes, G.
    Cantwell, W.J.
    Advanced Composites Letters, 7 (04): : 97 - 102
  • [6] Interfacial fracture in fibre-metal laminates based on glass fibre reinforced polypropylene
    Reyes, G
    Cantwell, WJ
    ADVANCED COMPOSITES LETTERS, 1998, 7 (04) : 97 - 103
  • [7] Fatigue crack initiation in fibre-metal laminate GLARE 2
    Vasek, A
    Polak, J
    Kozak, V
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 234 : 621 - 624
  • [8] Effect of surface treatment on the corrosion properties of magnesium-based fibre metal laminate
    Zhang, X.
    Zhang, Y.
    Ma, Q. Y.
    Dai, Y.
    Hu, F. P.
    Wei, G. B.
    Xu, T. C.
    Zeng, Q. W.
    Wang, S. Z.
    Xie, W. D.
    APPLIED SURFACE SCIENCE, 2017, 396 : 1264 - 1272
  • [9] Fatigue failure analysis of riveted fibre-metal laminate lap joints
    Tarpani, A. C. S. P.
    Barreto, T. A.
    Tarpani, J. R.
    ENGINEERING FRACTURE MECHANICS, 2020, 239
  • [10] The static and fatigue response of metal laminate and hybrid fibre-metal laminate doublers joints under tension loading
    Sugiman, S.
    Crocombe, A. D.
    COMPOSITE STRUCTURES, 2012, 94 (09) : 2937 - 2951