Synthesis and luminescent property of Sm3+ doped and (Sm3+, Zr4+) co-doped calcium stannate phosphors via co-precipitation and sintering

被引:7
作者
Zhu, Kun [1 ,2 ]
Lv, Haitao [1 ,3 ]
Wang, Yanmin [1 ]
Pan, Zhidong [1 ]
机构
[1] South China Univ Technol, Sch Mat Sci & Engn, Guangzhou 510640, Peoples R China
[2] Sci & Technol Bur Yun Fu, Yun Fu 527399, Peoples R China
[3] Guizhou Minzu Univ, Sch Mat Sci & Engn, Guiyang 550025, Peoples R China
基金
中国国家自然科学基金;
关键词
Phosphor; (Sm3+; Zr4+)-co-doped calcium stannate; Co-precipitation reaction; Afterglow; UP-CONVERSION LUMINESCENCE; MG CODOPED CASNO3; PHOTOLUMINESCENCE PROPERTIES; HYDROTHERMAL SYNTHESIS; OPTICAL-PROPERTIES; ANODE MATERIAL; SUBSTITUTION; TEMPERATURE; EFFICIENT; EMISSION;
D O I
10.1016/j.optmat.2021.111456
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Sm3+ doped calcium stannate (CaSnO3:Sm3+) and (Sm3+, Zr4+)-co-doped calcium stannate (CaSnO3:Sm3+, Zr4+) photoluminescent phosphors were synthesized via co-precipitation and subsequent sintering in oxidizing atmosphere at 1400 degrees C for 60 min with SnCl4.5H2O, CaCl2.2H2O, ZrO(NO3)(2.x)H2O and Sm2O3 as main raw materials. The synthesized samples were characterized by X-ray diffraction, scanning electron microscopy, energy dispersive spectroscopy, photoluminescent spectroscopy, luminescent decay curves, afterglow spectroscopy and thermo-luminescent glow curves. The results show that CaSnO3 pure phase is synthesized in co-precipitation reaction at an optimum molar ratio of CaCl2.2H2O:SnCl4.5H2O of 1.4:1.0 and subsequent sintering at 1400 degrees C for 60 min. Calcium stannate as a host matrix can be doped with Sm3+ ions or co-doped with Sm3+/Zr4+ ions for the formation of white photoluminescent phosphors. CaSnO3:0.03Sm(3+) phosphor has an optimum photo luminescent intensity. Also, the fluorescent emission intensity of CaSnO3:0.03Sm(3+),0.04Zr(4+) phosphor under excitation of 365 nm wavelength can be enhanced due to Zr4+ ions doping at an optimum doping amount y of 0.04. The CIE 1931 chromaticity coordinates change from (0.3600, 0.3535) for CaSnO3:0.03Sm(3+) phosphor to (0.3622, 0.3574) for CaSnO3:0.03Sm(3+), 0.04Zr(4+) phosphor as the average crystalline size decreases from 71.5 to 68.3 nm and the unit cell volume increases from 0.2686 to 0.2775 nm(3). In addition, the electron transition mechanism for the photoluminescent and long afterglow properties was also discussed.
引用
收藏
页数:12
相关论文
共 58 条
  • [1] Influence of the precursor salts in the synthesis of CaSnO3 by the polymeric precursor method
    Alves, Mary C. F.
    Souza, Soraia C.
    Lima, S. J. G.
    Longo, E.
    Souza, A. G.
    Santos, Ieda M. G.
    [J]. JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2007, 87 (03) : 763 - 766
  • [2] Investigations on the charge compensation on Ca and U substitution in CePO4 by using XPS, XRD and Raman spectroscopy
    Asuvathrarnan, R.
    Gnanasekar, K. I.
    Clinsha, P. C.
    Ravindran, T. R.
    Kutty, K. V. Govindan
    [J]. CERAMICS INTERNATIONAL, 2015, 41 (03) : 3731 - 3739
  • [3] Synthesis, processing and microstructural characterization of CaSnO3 and SrSnO3 ceramics
    Azad, AM
    Liew, L
    Shyan, W
    Yen, PT
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 1999, 282 (1-2) : 109 - 124
  • [4] Synthesis of calcium metastannate (CaSnO3) by solid state reactions in mechanically activated mixtures calcium citrate tetra hydrate [Ca3(C6H5O7)2•4H2O] - tin(II) oxalate (SnC2O4)
    Berbenni, Vittorio
    Milanese, Chiara
    Bruni, Giovanna
    Girella, Alessandro
    Marini, Amedeo
    [J]. THERMOCHIMICA ACTA, 2015, 608 : 59 - 64
  • [5] Catholuminescence properties of rare earth doped CaSnO3 phosphor
    Canimoglu, A.
    Garcia-Guinea, J.
    Karabulut, Y.
    Ayvacikli, M.
    Jorge, A.
    Can, N.
    [J]. APPLIED RADIATION AND ISOTOPES, 2015, 99 : 138 - 145
  • [6] Perovskite-type CaMnO3 anode material for highly efficient and stable lithium ion storage
    Chang, Limin
    Li, Jiahui
    Le, Zaiyuan
    Nie, Ping
    Guo, Yu
    Wang, Hairui
    Xu, Tianhao
    Xue, Xiangxin
    [J]. JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2021, 584 : 698 - 705
  • [7] ON CALCULATION OF ACTIVATION ENERGIES AND FREQUENCY FACTORS FROM GLOW CURVES
    CHEN, R
    [J]. JOURNAL OF APPLIED PHYSICS, 1969, 40 (02) : 570 - &
  • [8] Novel porous CaSnO3:Eu3+ and Ca2SnO4:Eu3+ phosphors by co-precipitation synthesis and postannealing approach: A general route to alkaline-earth stannates
    Chen, Xiang Ying
    Ma, Chao
    Bao, Shi Ping
    Zhang, Hai Yan
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 497 (1-2) : 354 - 359
  • [9] A host sensitized reddish-orange Gd2MoO6:Sm3+ phosphor for light emitting diodes
    Chen, Yan
    Wang, Jing
    Liu, Chunmeng
    Kuang, Xiaojun
    Su, Qiang
    [J]. APPLIED PHYSICS LETTERS, 2011, 98 (08)
  • [10] Electrocatalytically inactive SnS2 promotes water adsorption/dissociation on molybdenum dichalcogenides for accelerated alkaline hydrogen evolution
    Chen, Yaping
    Wang, Xingyong
    Lao, Mengmeng
    Rui, Kun
    Zheng, Xiaobo
    Yu, Haibo
    Ma, Jing
    Dou, Shi Xue
    Sun, Wenping
    [J]. NANO ENERGY, 2019, 64