The crystal structural evolution of nano-Si anode caused by lithium insertion and extraction at room temperature

被引:414
作者
Li, H
Huang, XJ
Chen, LQ
Zhou, GW
Zhang, Z
Yu, DP
Mo, YJ
Pei, N
机构
[1] Chinese Acad Sci, Inst Phys, Lab Solid State Ion, Beijing 100080, Peoples R China
[2] Chinese Acad Sci, Ctr Condensed Matter Phys, Beijing Lab Electron Microscopy, Beijing 100080, Peoples R China
[3] Peking Univ, Natl Key Lab Mesoscop Phys, Dept Phys, Beijing 100871, Peoples R China
[4] Henan Univ, Dept Phys, Kaifeng 475001, Peoples R China
关键词
nanosized Si; lithium ion battery; anode; electrochemical insertion; electron microscopy; Raman spectroscopy;
D O I
10.1016/S0167-2738(00)00362-3
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The crystal structure and morphology of nanosized Si particles and wires after Li-insertion/extraction electrochemically have been studied by ex-situ XRD, Raman spectroscopy and electronic microscopy. It is confirmed that the insertion of lithium ions at room temperature destroys the crystal structure of Si gradually and leads to the formation of metastable amorphous Li-Si alloy, Furthermore, local ordered structure of Si can be restored after the partial extraction of lithium ions, which indicates the extraction of lithium ions promoting the recrystallization of amorphous Li-inserted Si. It was also observed that nanosized Si particles and wires were merged together after the insertion/extraction of lithium ions. (C) 2000 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:181 / 191
页数:11
相关论文
共 25 条
[1]   Single-electrode Peltier heats of Li-Si alloy electrodes in LiCl-KCl eutectic melt [J].
Amezawa, K ;
Yamamoto, N ;
Tomii, Y ;
Ito, Y .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1998, 145 (06) :1986-1993
[2]   ALL-SOLID LITHIUM ELECTRODES WITH MIXED-CONDUCTOR MATRIX [J].
BOUKAMP, BA ;
LESH, GC ;
HUGGINS, RA .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1981, 128 (04) :725-729
[3]  
CHEN TD, 1995, J MATER RES, V10, P139
[4]   Electrochemical and in situ x-ray diffraction studies of the reaction of lithium with tin oxide composites [J].
Courtney, IA ;
Dahn, JR .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1997, 144 (06) :2045-2052
[5]  
Ichinose N., 1992, SUPERFINE PARTICLE T, P13
[6]   RAMAN-SCATTERING FROM HYDROGENATED MICROCRYSTALLINE AND AMORPHOUS-SILICON [J].
IQBAL, Z ;
VEPREK, S .
JOURNAL OF PHYSICS C-SOLID STATE PHYSICS, 1982, 15 (02) :377-392
[7]   SOLID LITHIUM-SILICON ELECTRODE [J].
LAI, SC .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1976, 123 (08) :1196-1197
[8]   Raman spectral study of silicon nanowires [J].
Li, BB ;
Yu, DP ;
Zhang, SL .
PHYSICAL REVIEW B, 1999, 59 (03) :1645-1648
[9]   A high capacity nano-Si composite anode material for lithium rechargeable batteries [J].
Li, H ;
Huang, XJ ;
Chen, LQ ;
Wu, ZG ;
Liang, Y .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 1999, 2 (11) :547-549
[10]  
Li H, 1998, ELECTROCHEM SOLID ST, V1, P241