High temperature oxidation and γ′ depletion in the single-crystal superalloy PWA 1484

被引:10
作者
Amaro, Robert L. [1 ]
Antolovich, Stephen D. [2 ,3 ,4 ,5 ,6 ]
Neu, Richard W. [2 ,3 ,4 ,5 ]
Singh, Preet M. [4 ,5 ]
机构
[1] Colorado Sch Mines, Dept Mech Engn, Boulder, CO 80303 USA
[2] Georgia Inst Technol, George W Woodruff Sch Mech Engn, 801 Ferst Dr, Atlanta, GA 30332 USA
[3] Georgia Inst Technol, Mech Properties Res Lab, 801 Ferst Dr, Atlanta, GA 30332 USA
[4] Georgia Inst Technol, Sch Mat Sci & Engn, 771 Ferst Dr, Atlanta, GA 30332 USA
[5] Georgia Inst Technol, Mech Properties Res Lab, 771 Ferst Dr, Atlanta, GA 30332 USA
[6] Washington State Univ, Sch Mech & Mat Engn, POB 642920, Pullman, WA 99164 USA
关键词
Oxidation kinetics; gamma ' depletion; Surface roughness; PWA; 1484; NI-BASE SUPERALLOY; THERMOMECHANICAL FATIGUE; CRACK INITIATION; GROWTH-KINETICS; PURE NICKEL; DEGREES-C; AIR; BEHAVIOR; METALS; MICROSTRUCTURE;
D O I
10.1080/09603409.2016.1180276
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Single-crystal Ni-base superalloys are a favoured material for blades in the hot section of aero turbines. These materials exhibit excellent dimensional stability, deformation response and oxidation behaviour at higher temperatures, relative to other metals. Due to the high service temperatures and fluctuating loads experienced by turbine blades, a complete understanding of the material's oxidation and.' depletion kinetics is sought to characterise this aspect of the material's deformation response. This work provides the results and subsequent analysis of stress-free gamma' depletion tests performed on the single-crystal Ni-base superalloy PWA 1484. It was determined that the gamma' depletion kinetics of this material followed a sub-parabolic rate law. Furthermore, gamma' depletion kinetics were dependent upon surface roughness. Surface roughness can be an issue in practical application of oxidation principles and data. A relationship is developed, based on the literature and current work, which relates the stress-free gamma' depletion kinetics to exposure temperature, time and surface roughness.
引用
收藏
页码:476 / 488
页数:13
相关论文
共 30 条
[1]   Mechanism-based life model for out-of-phase thermomechanical fatigue in single crystal Ni-base superalloys [J].
Amaro, R. L. ;
Antolovich, S. D. ;
Neu, R. W. .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2012, 35 (07) :658-671
[2]  
Amaro R. L., 2010, THERMOMECHANICAL FAT, P321
[3]   INTERGRANULAR CRACK TIP OXIDATION MECHANISM IN A NICKEL-BASED SUPERALLOY [J].
ANDRIEU, E ;
MOLINS, R ;
GHONEM, H ;
PINEAU, A .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1992, 154 (01) :21-28
[4]   High temperature oxidation of single-crystal Ni-base superalloys [J].
Bouhanek, K ;
Oquab, D ;
Pieraggi, B .
HIGH TEMPERATURE CORROSION AND PROTECTION OF MATERIALS 4, PTS 1 AND 2, 1997, 251-2 :33-40
[5]  
Cetel A. D., 1988, SUPERALLOYS, V21, P235
[6]   High temperature oxidation behaviour of directionally solidified nickel base superalloy CM-247LC [J].
Das, DK ;
Singh, V ;
Joshi, SV .
MATERIALS SCIENCE AND TECHNOLOGY, 2003, 19 (06) :695-708
[7]  
DeHoff Robert., 2006, Thermodynamics in Materials Science, P605
[8]   A multiscale approach for coupled phenomena in fcc materials at high temperatures [J].
Dumoulin, S ;
Busso, EP ;
O'Dowd, NP ;
Allen, D .
PHILOSOPHICAL MAGAZINE, 2003, 83 (31-34) :3895-3916
[9]  
Fleury E., 1991, ENDOMMAGEMENT SUPERA
[10]   OXIDATION OF NI-CR-AL ALLOYS BETWEEN 1000 DEGREES AND 1200 DEGREES C [J].
GIGGINS, CS ;
PETTIT, FS .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1971, 118 (11) :1782-&