Cavitation Erosion on Solid Polymers of Polytetrafluoroethelyene

被引:11
作者
Liu, Caiyun [2 ]
Li, Jiang [2 ]
Chen, Haosheng [1 ]
机构
[1] Tsinghua Univ, State Key Lab Tribol, Beijing 100084, Peoples R China
[2] Univ Sci & Technol Beijing, Sch Mech Engn, Beijing 100083, Peoples R China
关键词
Polymers (solid); Cavitation erosion; Erosive wear; PTFE; CORROSION;
D O I
10.1007/s11249-012-9953-4
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
A 100-h-long cavitation erosion experiment was performed on a sample of polytetrafluoroethelyene (PTFE). The weight loss curve of PTFE was different from that of metals, and the erosion process was characterized by two stages, each with a distinct erosion rate. Morphology studies on the erosion pits and X-ray diffraction analysis of the eroded surfaces revealed that brittle fracture was the main reason for the higher erosion rate at the beginning of the erosion process, while ductile fracture dominated the weight loss process later in the erosion process, thereby reducing the erosion rate. Based on these results, we consider that this transition from brittle to ductile fracture was responsible for the different erosion rates at the two different erosion stages.
引用
收藏
页码:17 / 20
页数:4
相关论文
共 12 条
[1]  
[Anonymous], 1961, FORTSCHR HOCHPOLYMER, DOI DOI 10.1007/BFB0050504
[2]  
Blackley D.C., 1983, SYNTHETIC RUBBERS TH, P283
[3]   Spherical dendritic particles formed in cavitation erosion [J].
Chen Haosheng ;
Liu Shihan ;
Wang Jiadao ;
Chen Darong .
MATERIALS LETTERS, 2008, 62 (17-18) :2707-2709
[4]   Experimental and numerical investigations on development of cavitation erosion pits on solid surface [J].
Chen Haosheng ;
Li Yongjian ;
Chen Darong ;
Wang Jiadao .
TRIBOLOGY LETTERS, 2007, 26 (02) :153-159
[5]   The molecular conformations of polytetrafluoroethylene: forms II and IV [J].
Clark, ES .
POLYMER, 1999, 40 (16) :4659-4665
[6]  
Franta I., 1989, ELASTOMERS RUBBER CO, P294
[7]   RIPPLE FORMATION IN SOLID LIQUID EROSION [J].
KARIMI, A ;
SCHMID, RK .
WEAR, 1992, 156 (01) :33-47
[8]  
Knapp R.T., 1970, Cavitation
[9]   Synergistic effect of cavitation erosion and corrosion of various engineering alloys in 3.5% NaCl solution [J].
Kwok, CT ;
Cheng, FT ;
Man, HC .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2000, 290 (1-2) :145-154
[10]   Deformation, yielding, fracture and fatigue behavior of conventional and highly cross-linked ultra high molecular weight polyethylene [J].
Pruitt, LA .
BIOMATERIALS, 2005, 26 (08) :905-915