Optimization of Acid Leaching of Rare-Earth Elements from Mongolian Apatite-Based Ore

被引:51
作者
Kim, Rina [1 ]
Cho, Heechan [1 ]
Han, Kenneth N. [2 ]
Kim, Kihong [1 ]
Mun, Myoungwook [1 ]
机构
[1] Seoul Natl Univ, Dept Energy Resources Engn, Seoul 08826, South Korea
[2] South Dakota Sch Mines & Technol, Dept Mat & Met Engn, Rapid City, SD 57701 USA
关键词
rare-earth element; acid leaching; apatite; magnetic separation; two-stage leaching; Ca removal; PHOSPHORIC-ACID; PHOSPHATE ROCK; RECOVERY; LANTHANIDES; SOLUBILITY; SYSTEMS;
D O I
10.3390/min6030063
中图分类号
P3 [地球物理学]; P59 [地球化学];
学科分类号
0708 ; 070902 ;
摘要
Optimization of the acid leaching process for Mongolian apatite-based ore containing rare-earth elements (REEs) was studied. The ore contained approximately 10% of REEs as total rare earth oxides, and the major impurities were Ca (33% as CaO) and Fe (23% as Fe2O3). Fe bearing minerals could be removed by passing the sample through a wet high-intensity magnetic separator before leaching. After magnetic separation, basic leaching tests were conducted to investigate the influence of the acid type and concentration, temperature, and the pH on the REE leaching level and kinetics. Hydrochloric acid was found to be the most effective leaching agent, leaching more than 90% of REEs in an hour. However, the concentrations of Ca ions in the leachate were also high, which would complicate recovery of the REEs. Therefore, to reduce the amount of Ca ions in the leachate, a two-stage leaching procedure was attempted. In stage 1, the sample was preleached using 1.0 M hydrochloric acid to dissolve Ca. In stage 2, the solid residue of stage 1 was leached using 2.0 M hydrochloric acid to dissolve REEs. Consequently, this two-stage leaching significantly reduced the Ca concentration in the final leachate without affecting the leaching levels of REEs.
引用
收藏
页数:15
相关论文
共 27 条
[1]  
Altangerel T, RARE EARTH DEPOSITS
[2]   Recovery of lanthanides from Abu Tartur phosphate rock, Egypt [J].
Aly, MM ;
Mohammed, NA .
HYDROMETALLURGY, 1999, 52 (02) :199-206
[3]  
[Anonymous], GEOLOGICAL SOC AM AB
[4]   The solubility of gypsum and anhydrite in simulated laterite pressure acid leach solutions up to 250 °C [J].
Azimi, G. ;
Papangelakis, V. G. .
HYDROMETALLURGY, 2010, 102 (1-4) :1-13
[5]   Kinetics of rare earth leaching from a mangnese-removed weathered rare-earth mud in hydrochloric acid solutions [J].
Chi, R ;
Tian, J ;
Zhu, G ;
Wu, Y ;
Li, S ;
Wang, C ;
Zhou, ZA .
SEPARATION SCIENCE AND TECHNOLOGY, 2006, 41 (06) :1099-1113
[6]  
Daly J.C.K., 2011, CENTR ASIA CAUC ANAL, V13, P6
[7]  
Enkhbayar D., 2016, INT J GEOSCI, V07, P20, DOI [10.4236/ijg.2016.71003, DOI 10.4236/IJG.2016.71003]
[8]   SOLUBILITY PRODUCTS OF THE TRIVALENT RARE-EARTH PHOSPHATES [J].
FIRSCHING, FH ;
BRUNE, SN .
JOURNAL OF CHEMICAL AND ENGINEERING DATA, 1991, 36 (01) :93-95
[9]  
Gangolli S., 1999, DICT SUBSTANCES THEI
[10]  
HABASHI F, 1985, J CHEM TECH BIOT A, V35, P5