The slurry erosive wear of physically vapour deposited TiN and CrN coatings under controlled corrosion

被引:15
|
作者
Wang, HW [1 ]
Stack, MM [1 ]
机构
[1] Univ Manchester, Inst Sci & Technol, Ctr Corros & Protect, Manchester M60 1QD, Lancs, England
关键词
PVD coatings; TiN; CrN; erosion; corrosion; erosion-corrosion;
D O I
10.1023/A:1019186918225
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The erosion-corrosion of mild steel (BS6323), in the presence and absence of physically vapour deposited (PVD) TiN and CrN coatings, was studied, in comparison with that of AISI 304 stainless steel, in an aqueous alkaline slurry solution containing alumina particles. The influence of applied potential and particle velocity on the total erosion-corrosion loss was examined, and the respective corrosion and erosion damage (both contributing to the overall weight loss) then assessed by means of microscopical investigation of the morphology of the damaged surface, and subsequently evaluated quantitatively. The superior erosion-corrosion resistance of both the coatings compared to that of the uncoated mild and stainless steels was shown to be due to their resistance to both wear and corrosion. According to the detailed corrosion mechanisms revealed and different responses to wear, schematic diagrams were proposed to outline the main features of the corrosion-erosion process and the individual roles of erosion and corrosion. Discrete differences, in terms of the respective erosion and corrosion processes, between the TiN and CrN coatings, and between the mild and stainless steels, were also investigated and discussed.
引用
收藏
页码:23 / 36
页数:14
相关论文
共 50 条
  • [1] The slurry erosive wear of physically vapour deposited TiN and CrN coatings under controlled corrosion
    H.W. Wang
    M.M. Stack
    Tribology Letters, 1999, 6 : 23 - 36
  • [2] Erosive wear behaviour of thick chemical vapour deposited diamond coatings
    Wheeler, D.W.
    Wood, R.J.K.
    Wear, 1999, 225-229 (0I): : 523 - 536
  • [3] Erosive wear behaviour of thick chemical vapour deposited diamond coatings
    Wheeler, DW
    Wood, RJK
    WEAR, 1999, 225 : 523 - 536
  • [4] Wear of cermet cutting tools coated with physically vapour deposited TiN
    Novak, S
    Komac, M
    WEAR, 1997, 205 (1-2) : 160 - 168
  • [5] Corrosion and wear behavior of CAE deposited CrN-PVD coatings
    Montesano, L.
    Petrogalli, C.
    Pola, A.
    Gelfi, M.
    Sisti, V.
    La Vecchia, G. M.
    ADVANCES IN FRACTURE AND DAMAGE MECHANICS XII, 2014, 577-578 : 641 - +
  • [6] Evaluation of erosive wear resistance of TiN coatings by a slurry jet impact test
    Iwai, Y.
    Miyajima, T.
    Honda, T.
    Matsubara, T.
    Kanda, K.
    Hogmark, S.
    WEAR, 2006, 261 (01) : 112 - 118
  • [7] Corrosion Resistanne of the [TiN/CrN]n Coatings Deposited on Steel AISI 4140
    Aperador, W.
    Delgado, A.
    Duque, J.
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2013, 8 (08): : 10711 - 10719
  • [8] Mechanical, wear and corrosion behavior of CrN/TiN multilayer coatings deposited by low temperature unbalanced magnetron sputtering for biomedical applications
    Rabadzhiyska, Stanislava
    Kolaklieva, Lilyana
    Chitanov, Vasiliy
    Cholakova, Tetiana
    Kakanakov, Roumen
    Dimcheva, Nina
    Balashev, Konstantin
    MATERIALS TODAY-PROCEEDINGS, 2018, 5 (08) : 16012 - 16021
  • [9] Wear and corrosion resistance of CrN/TiN superlattice coatings deposited by a combined deep oscillation magnetron sputtering and pulsed dc magnetron sputtering
    Ou, Y. X.
    Lin, J.
    Tong, S.
    Che, H. L.
    Sproul, W. D.
    Lei, M. K.
    APPLIED SURFACE SCIENCE, 2015, 351 : 332 - 343
  • [10] Cavitation erosion of TiN and CrN coatings deposited on different substrates
    Krella, Alicja
    WEAR, 2013, 297 (1-2) : 992 - 997