Wear and corrosion characteristics of alumina dispersed Ni-P nanocomposite coating developed by electroless technique

被引:26
作者
Makkar, Preeti [1 ]
Agarwala, R. C. [1 ]
Agarwala, Vijaya [1 ,2 ]
机构
[1] Indian Inst Technol Roorkee, Dept Met & Mat Engn, Roorkee, Uttar Pradesh, India
[2] Indian Inst Technol Roorkee, Ctr Nanotechnol, Roorkee 247667, Uttar Pradesh, India
关键词
COMPOSITE COATINGS; ELECTROCHEMICAL IMPEDANCE; RESISTANCE; BEHAVIOR; NI-P-AL2O3; NANOPARTICLES; HARDNESS;
D O I
10.1007/s10853-015-8839-x
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Advances in materials performance require the development of nanocomposite coatings. The paper aims to study the comparative wear and corrosion performance of Ni-P and Ni-P-Al2O3 nanocomposite coatings developed by electroless technique. The effect of heat treatment (400 degrees C, 1 h) on the coating performance is also studied. The second-phase Al2O3 nanoparticles of average size 15 nm were synthesized by chemical precipitation route. The synthesized Al2O3 nanoparticles (4 g/l) were added into the alkaline Ni-P bath to develop Ni-P-Al2O3 nanocomposite coatings on the mild steel substrate. The coating thickness was found to be about 20 mu m. The phases and morphology of Al2O3 nanoparticles and coatings were examined by XRD and FESEM, respectively. Chemical composition of the coating was analysed by EDX. Wear and friction behaviour of the coatings were measured at different loads (1, 1.5 and 2 N) and velocities (0.1, 0.2 m/s) using ball-on-disc method. Tafel polarisation test was employed to evaluate corrosion behaviour of the coatings in acidic (pH 4.5) and alkaline (pH 8) environments. Ni-P-Al2O3 nanocomposite coatings showed higher hardness and wear and corrosion resistance compared with plane Ni-P coatings. An improvement in corrosion resistance was observed by Ni-P and Ni-P-Al2O3 coatings in both acidic and alkaline environments. Heat treatment significantly improves hardness and wear and corrosion resistance of the coatings.
引用
收藏
页码:2813 / 2823
页数:11
相关论文
共 31 条
[1]   Preparation of electroless Ni-P composite coatings containing nano-scattered alumina in presence of polymeric surfactant [J].
Afroukhteh, S. ;
Dehghanian, C. ;
Emamy, M. .
PROGRESS IN NATURAL SCIENCE-MATERIALS INTERNATIONAL, 2012, 22 (04) :318-325
[2]   Electroless Ni-P based nanocoating technology - A review [J].
Agarwala, Ramesh Chandra ;
Agarwala, Vijaya ;
Sharma, Rahul .
SYNTHESIS AND REACTIVITY IN INORGANIC METAL-ORGANIC AND NANO-METAL CHEMISTRY, 2006, 36 (06) :493-515
[3]   Wear behavior of Ni-P and Ni-P-Al2O3 electroless coatings [J].
Alirezaei, S. ;
Monirvaghefi, S. M. ;
Salehi, M. ;
Saatchi, A. .
WEAR, 2007, 262 (7-8) :978-985
[4]   Effect of alumina content on surface morphology and hardness of Ni-P-Al2O3(α) electroless composite coatings [J].
Alirezaei, S ;
Monirvaghefi, SM ;
Salehi, M ;
Saatchi, A .
SURFACE & COATINGS TECHNOLOGY, 2004, 184 (2-3) :170-175
[5]   Characterization and corrosion behavior of electroless Ni-P/nano-SiC coating inside the CO2 containing media in the presence of acetic acid [J].
Allahkaram, S. R. ;
Nazari, M. Honarvar ;
Mamaghani, S. ;
Zarebidaki, A. .
MATERIALS & DESIGN, 2011, 32 (02) :750-755
[6]   WEAR-MECHANISM MAPS [J].
ASHBY, MF ;
LIM, SC .
SCRIPTA METALLURGICA ET MATERIALIA, 1990, 24 (05) :805-810
[7]   Influence of particle size on the microstructure, hardness and corrosion resistance of electroless Ni-P-Al2O3 composite coatings [J].
Balaraju, JN ;
Kalavati ;
Rajam, KS .
SURFACE & COATINGS TECHNOLOGY, 2006, 200 (12-13) :3933-3941
[8]   Electroless Ni-P composite coatings [J].
Balaraju, JN ;
Narayanan, TSNS ;
Seshadri, SK .
JOURNAL OF APPLIED ELECTROCHEMISTRY, 2003, 33 (09) :807-816
[9]   Evaluation of the corrosion resistance of electroless Ni-P and Ni-P composite coatings by electrochemical impedance spectroscopy [J].
Balaraju, JN ;
Narayanan, TSNS ;
Seshadri, SK .
JOURNAL OF SOLID STATE ELECTROCHEMISTRY, 2001, 5 (05) :334-338
[10]   Electrochemical and X-ray photoelectron spectroscopy investigation into anodic behaviour of electroless Ni-9-5 wt-%P in acidic chloride environment [J].
Bozzini, B ;
Lenardi, C ;
Serra, M ;
Fanigliulo, A .
BRITISH CORROSION JOURNAL, 2002, 37 (03) :173-181