Strengthening of iron aluminide alloys by atomic ordering and Laves phase precipitation for high-temperature applications

被引:71
作者
Risanti, DD [1 ]
Sauthoff, G [1 ]
机构
[1] Max Planck Inst Eisenforsch GmbH, D-40237 Dusseldorf, Germany
关键词
iron aluminides (based on Fe3Al); iron aluminides (based on FeAl); brittleness and ductility; mechanical properties at high temperatures;
D O I
10.1016/j.intermet.2004.12.029
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The ternary system Fe-Al-Ta allows the formation of the hard and brittle ternary Laves phase Ta(Fe0.5+x,Al0.5-x)(2) with hexagonal C14 structure. The present study concentrates on Fe-Al-Ta alloys with small Ta contents between 2 and 6 at.% and various Al contents between 0 and 45 at.%. The phase equilibria in the ternary Fe-Al-Ta system at 1000 degrees C are studied experimentally for determination of the solubility limits of Ta in iron aluminide matrices and types of phases and structures which may occur at high temperatures. It is observed that small amounts of Laves phase together with atomic ordering increase the yield stress and affect ductility in a complex way. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1313 / 1321
页数:9
相关论文
共 35 条
[1]   EFFECTS OF EARLY TRANSITION-METAL SOLUTES ON THE D0(3)-B2 CRITICAL-TEMPERATURE OF FE3AL [J].
ANTHONY, L ;
FULTZ, B .
ACTA METALLURGICA ET MATERIALIA, 1995, 43 (10) :3885-3891
[2]   Some aspects of rapid solidification processing of Fe-Al-X alloys [J].
Buckley, RA ;
Kaviani, S .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 258 (1-2) :173-180
[3]   Nickel and iron aluminides: An overview on properties, processing, and applications [J].
Deevi, SC ;
Sikka, VK .
INTERMETALLICS, 1996, 4 (05) :357-375
[4]   THE OXIDATION SULFIDATION BEHAVIOR OF IRON-ALLOYS CONTAINING 16-40 AT-DEGREES ALUMINUM [J].
DEVAN, JH ;
TORTORELLI, PF .
CORROSION SCIENCE, 1993, 35 (5-8) :1065-1071
[5]   Alloys based on Fe3Al or FeAl with strengthening Mo3Al precipitates [J].
Eumann, M ;
Palm, M ;
Sauthoff, G .
INTERMETALLICS, 2004, 12 (06) :625-633
[6]   Iron-rich iron-aluminium-molybdenum alloys with strengthening intermetallic μ phase and R phase precipitates [J].
Eumann, M ;
Palm, M ;
Sauthoff, G .
STEEL RESEARCH INTERNATIONAL, 2004, 75 (01) :62-73
[7]   Deformation behaviour of iron-rich iron-aluminium alloys at high temperatures [J].
Herrmann, J ;
Inden, G ;
Sauthoff, G .
ACTA MATERIALIA, 2003, 51 (11) :3233-3242
[8]  
Hertzberg RW., 2012, Deformation and fracture mechanics of engineering materials, copy right © 1976, 1983, V5th
[9]   MICROSTRUCTURE, ADHESION AND GROWTH-KINETICS OF PROTECTIVE SCALES ON METALS AND ALLOYS [J].
HINDAM, H ;
WHITTLE, DP .
OXIDATION OF METALS, 1982, 18 (5-6) :245-284
[10]  
HUNT CR, 1968, Z METALLKD, V59, P701