Structural, morphological, optical and luminescence investigations of chemical bath deposited Ni:ZnS thin films

被引:3
作者
Jrad, Abdelhak [1 ,2 ]
Naouai, Manel [3 ]
Ammar, Souad [2 ]
Turki-Kamoun, Najoua [1 ]
机构
[1] Univ Tunis El Manar, Fac Sci Tunis, Dept Phys, LR99ES13 Lab Phys Mat Condensee LPMC, Tunis 2092, Tunisia
[2] Univ Paris Diderot, ITODYS, CNRS UMR 7086, Sorbonne Paris Cite, F-75013 Paris, France
[3] Fac Sci Tunis, Dept Phys, Lab Spect Atom Mol & Applicat, Campus Univ Farhat Hached, Tunis El Manar 2092, Tunisia
来源
MATERIALS TODAY COMMUNICATIONS | 2021年 / 29卷
关键词
CBD; ZnS; Ni dopant; XPS; SEM; FTIR; PHYSICAL-PROPERTIES; PHOTOCATALYTIC ACTIVITY; MAGNETIC-PROPERTIES; ZNS; NI; TEMPERATURE; FERROMAGNETISM; GROWTH;
D O I
10.1016/j.mtcomm.2021.102746
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Nickel doped zinc sulfide (Ni:ZnS) thin films are deposited on glass substrates by chemical bath deposition (CBD) for different Ni concentrations (0, 6, 12 and 18 at%). X-ray diffraction (XRD) patterns of undoped and Ni doped layers show a cubic structure with (111) preferred orientation. For the highest Ni concentration an impurity phase is detected and assigned to NiS compound. Fourier transform infrared (FTIR) analysis proves the existence of some residues in the films. X-ray photoelectron spectroscopy (XPS) reveals the formation of ZnS. The morphological study by scanning electron microscopy (SEM) shows important changes in layers topography. Transmittance (T) and reflectance (R) data reveal an enhancement for 6 at% and 12 at% dopant concentrations. Finally, photoluminescence (PL) properties show a decrease of the emission intensity with an increment of Ni content until 12 at%. Then, an increase of the PL intensity is observed with further increase of Ni amount.
引用
收藏
页数:8
相关论文
共 50 条
  • [41] Structural, morphological and optical studies on chemically deposited nanocrystalline CdZnSe thin films
    Deo, Soumya R.
    Singh, Ajaya K.
    Deshmukh, Lata
    Paliwal, L. J.
    Singh, R. S.
    Adhikari, Rameshwar
    JOURNAL OF SAUDI CHEMICAL SOCIETY, 2014, 18 (04) : 327 - 339
  • [42] Synthesizing of ZnS and ZnO nanotubes films deposited by thermal evaporation: morphological, structural and optical properties
    Abdallah, B.
    Kakhia, M.
    Zetoune, W.
    Alkafri, N.
    MATERIALS RESEARCH EXPRESS, 2019, 6 (11)
  • [43] Structural, morphological, and optical properties of AgxO thin films deposited via obliquely angle deposition
    Ben Soltane, H.
    Akkari, F. Chaffar
    Gallas, B.
    Kanzari, M.
    MATERIALS SCIENCE-POLAND, 2023, 41 (01) : 27 - 41
  • [44] EFFECT OF THE pH ON CRYSTAL STRUCTURAL, OPTICAL AND SURFACE MORPHOLOGICAL PROPERTIES OF THE CdS FILMS DEPOSITED BY CHEMICAL BATH DEPOSITION
    Aybek, A. S.
    Ruzgar, H.
    CHALCOGENIDE LETTERS, 2016, 13 (08): : 339 - 350
  • [45] Solution-processed NiS thin films: structural, morphological, compositional and optical analysis
    Suresh, Kumar
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2024, 115 (09) : 700 - 708
  • [46] Influence of humidity on the growth characteristics and properties of chemical bath-deposited ZnS thin films
    Lin, Yi-Cheng
    Chao, Yen-Tai
    Yao, Pin-Chuan
    APPLIED SURFACE SCIENCE, 2014, 307 : 724 - 730
  • [47] Electrochemical Synthesis of In2Se3 Thin Films from Citrate Bath. Structural, Optical and Morphological Investigations
    Dilmi, Oualid
    Benaicha, Mohamed
    RUSSIAN JOURNAL OF ELECTROCHEMISTRY, 2021, 57 (05) : 462 - 470
  • [48] Structural, morphological, optical and diode properties of chemical bath deposited nano-structured CdS thin films using EDTA as a complexing agent
    Vidhya, S. N.
    Karunakaran, R. T.
    MATERIALS SCIENCE-POLAND, 2019, 37 (03): : 317 - 323
  • [49] Effect of Ni incorporation on structural, optical and magnetic properties of electron beam evaporated ZnS thin films
    Kumar, K. Chaitanya
    Kaleemulla, S.
    JOURNAL OF PHYSICS AND CHEMISTRY OF SOLIDS, 2019, 135
  • [50] STUDY OF CHEMICAL BATH DEPOSITION OF ZnS THIN FILMS WITH SUBSTRATE VIBRATION
    Bian, Z. Q.
    Xu, X. B.
    Chu, J. B.
    Sun, Z.
    Chen, Y. W.
    Huang, S. M.
    SURFACE REVIEW AND LETTERS, 2008, 15 (06) : 821 - 827