pH-compensation effect of bioactive inorganic fillers on the degradation of PLGA

被引:134
作者
Li, HY
Chang, J
机构
[1] Chinese Acad Sci, Shanghai Inst Ceram, Biomat & Tissue Engn Res Ctr, Shanghai 200050, Peoples R China
[2] Chinese Acad Sci, Grad Sch, Shanghai 200050, Peoples R China
基金
中国国家自然科学基金;
关键词
PLGA; pH compensation; bioactive inorganic fillers; scaffolds; degradation;
D O I
10.1016/j.compscitech.2005.04.051
中图分类号
TB33 [复合材料];
学科分类号
摘要
It has been suggested that acidic degradation product of the poly (alpha-hydroxy acids) results in pH decrease in the vicinity of the scaffolds, which may be responsible for biocompatibility concerns rose recently about polylactide acid (PLA), polyglycolic acid (PGA) polymers and their copolymer poly (lactic acid-co glycolic acid) (PLGA). This in vitro study was performed to evaluate the pH-compensation ability of bioactive inorganic fillers (BIFs) such as wollastonite (W), bioglass 45S5 (BG 45S5) and hydroxyapatite (HA) on the acidic degradation products of PLGA. Three composite scaffolds of PLGA incorporated with BIFs were fabricated and immersed in phosphate buffered saline (PBS, pH 7.4) solution at 37 degrees C for 8 weeks to evaluate the pH changes of the PBS, the mass loss and water absorption of the scaffolds, and the molecular weight loss of the PLGA in the scaffolds. The results indicated that the pH of the PLGA group fell to a value of 4.3 in 8 weeks while the pH of the composite groups containing W and BG 45S5 was maintained between 7.7-7.3 and 8.15-7.1 throughout the soaking period, respectively. However, the pH of the composite group containing HA exhibited an almost linear decrease from 7.4 to 5.6 at an average rate of 0.05 per day. In addition, the incorporation of W and BG delayed the degradation of the PLGA in the composites while the incorporation of HA accelerated the degradation. Furthermore, the W and BG in the composite scaffolds accelerated weight loss of the scaffolds and increased their capacity to absorb water during the initial incubation period. All of these results suggested that incorporations of both W and BG 45S5 into PLGA strongly affected the degradation behavior of scaffolds and were effective in compensation of the pH decrease caused by the acidic degradation products of the PLGA. (c) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2226 / 2232
页数:7
相关论文
共 35 条
[1]  
Agrawal CM, 1997, J BIOMED MATER RES, V38, P105, DOI 10.1002/(SICI)1097-4636(199722)38:2<105::AID-JBM4>3.0.CO
[2]  
2-U
[3]   Effect of blending calcium compounds on hydrolytic degradation of poly(DL-lactic acid-co-glycolic acid) [J].
Ara, M ;
Watanabe, M ;
Imai, Y .
BIOMATERIALS, 2002, 23 (12) :2479-2483
[4]   Bioresorbable and bioactive polymer/Bioglass® composites with tailored pore structure for tissue engineering applications [J].
Boccaccini, AR ;
Maquet, V .
COMPOSITES SCIENCE AND TECHNOLOGY, 2003, 63 (16) :2417-2429
[5]   A novel porous cells scaffold made of polylactide-dextran blend by combining phase-separation and particle-leaching techniques [J].
Cai, Q ;
Yang, JA ;
Bei, JZ ;
Wang, SG .
BIOMATERIALS, 2002, 23 (23) :4483-4492
[6]  
Davies JE, 1997, J BIOMED MATER RES, V36, P429, DOI 10.1002/(SICI)1097-4636(19970915)36:4<429::AID-JBM1>3.0.CO
[7]  
2-G
[8]  
Gibbons D., 1992, DEGRADATION PHENOMEN, P97
[9]   pH-stabilization of predegraded PDLLA by an admixture of water-soluble sodiumhydrogenphosphate-results of an in vitro- and in vivo-study [J].
Heidemann, W ;
Jeschkeit-Schubbert, S ;
Ruffieux, K ;
Fischer, JH ;
Jung, H ;
Krueger, G ;
Wintermantel, E ;
Gerlach, KL .
BIOMATERIALS, 2002, 23 (17) :3567-3574
[10]  
Hench L.L., 1971, Journal of Biomedical Materials Research Symposium, V36, P117, DOI DOI 10.1002/JBM.820050611