Superplastic deformation in W-0.5 wt.% TiC with approximately 0.1 μm grain size

被引:67
作者
Kurishita, H. [1 ]
Matsuo, S. [1 ]
Arakawa, H. [1 ]
Kobayashi, S. [2 ]
Nakai, K. [2 ]
Takida, T. [3 ]
Takebe, K. [3 ]
Kawai, M. [4 ]
机构
[1] Tohoku Univ, IMR, Int Res Ctr Nucl Mat Sci, Oarai, Ibaraki 3111313, Japan
[2] Ehime Univ, Dept Mat Sci & Biotechnol, Matsuyama, Ehime 7908577, Japan
[3] ALMT Corp, Toyama 9318543, Japan
[4] High Energy Accelerator Res Org, Inst Mat Struct Sci, Tsukuba, Ibaraki 3050801, Japan
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2008年 / 477卷 / 1-2期
关键词
tungsten; TiC dispersoids; mechanical alloying atmosphere; superplasticity; deformation mechanism;
D O I
10.1016/j.msea.2007.05.009
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In order to reveal the occurrence of superplasticity in ultra-fine grained W-TiC, W-0.5 wt. % TiC consolidates were fabricated utilizing mechanical alloying (MA) in purified H, (W-0.5TiC-H-2) or Ar (W-0.5TiC-Ar) and hot isostatic pressing. The W-0.5TiC-H-2 and W-0.5TiC-Ar feature equiaxed ultra-fine grains with average diameters of 150 and 70 nm, respectively, and W-0.5TiC-Ar contains a high density of nano-sized Ar bubbles. Tensile tests were conducted at 1673-1973 K (0.45-0.54T(m), T-m: melting point of W) at initial strain rates from 5 x 10(-5) to 5 x 10(-3) s(-1). It is found that W-0.5TiC-H-2 exhibits a large strain rate sensitivity of flow stress, m, of 0.5-0.6, which is a feature of superplastic materials, whereas W-0.5TiC-Ar exhibits a smaller m value of approximately 0.2. This suggests that the Ar bubbles cause an adverse effect on superplastic deformation. The activation energy for deformation is 300 kJ mol(-1) for W-0.5TiC-H-2 and 570 kJ mol(-1) for W-0.5TiC-Ar, corresponding to those for grain boundary diffusion and lattice diffusion in W, respectively. Each deformation controlling mechanism is discussed. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:162 / 167
页数:6
相关论文
共 16 条
[1]  
BENJAMIN JS, 1970, METALL TRANS, V1, P2943
[2]   Microstructure and bend ductility of W-0.3 mass% TiC alloys fabricated by advanced powder-metallurgical processing [J].
Ishijima, Y ;
Kurishita, H ;
Arakawa, H ;
Hasegawa, M ;
Hiraoka, Y ;
Takida, T ;
Takebe, K .
MATERIALS TRANSACTIONS, 2005, 46 (03) :568-574
[3]   Current status of ductile tungsten alloy development by mechanical alloying [J].
Ishijima, Y ;
Kurishita, H ;
Yubuta, K ;
Arakawa, H ;
Hasegawa, M ;
Hiraoka, Y ;
Takida, T ;
Takebe, K .
JOURNAL OF NUCLEAR MATERIALS, 2004, 329 :775-779
[4]  
*JAP I MET, 1993, MET DAT BOOK, P24
[5]   Microstructure and impact properties of ultra-fine grained tungsten alloys dispersed with TiC [J].
Kitsunai, Y ;
Kurishita, H ;
Kayano, H ;
Hiraoka, Y ;
Igarashi, T ;
Takida, T .
JOURNAL OF NUCLEAR MATERIALS, 1999, 271 :423-428
[6]  
KURISHITA H, 2006, PHYS SCR T, V128, P76
[7]  
KURISHITA H, 2006, UNPUB J NUCL MAT
[8]  
Kurishita H., 1999, J PLASMA FUSION RES, V75, P594
[9]  
KURISHITA H, 2005, IN PRESS J NUCL MAT
[10]   Development of an ultra-fine grained V-1.7 mass% Y alloy dispersed with yttrium compounds having superior ductility and high strength [J].
Kuwabara, T ;
Kurishita, H ;
Hasegawa, M .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2006, 417 (1-2) :16-23