Effect of Al-Si Coating on Weldability of Press-Hardened Steels

被引:37
作者
Chen, RuiMing [1 ]
Zhang, ChaoQun [1 ]
Lou, Ming [1 ]
Li, YongBing [1 ]
Carlson, Blair E. [2 ]
机构
[1] Shanghai Jiao Tong Univ, Shanghai Key Lab Digital Manufacture Thin Walled, State Key Lab Mech Syst & Vibrat, Sch Mech Engn, 800 Dongchuan Rd, Shanghai 200240, Minhang, Peoples R China
[2] Gen Motors Res & Dev Ctr, Mfg Syst Res Lab, 30470 Harley Earl Blvd, Warren, MI 48092 USA
基金
中国国家自然科学基金;
关键词
Al-Si coating; press-hardened steel; resistance spot welding; ultrahigh-strength steel; FAILURE MODE TRANSITION; BORON STEEL; HOT; STRENGTH; SILICON; GROWTH; LAYER;
D O I
10.1007/s11665-020-04555-w
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Resistance spot welding (RSW) of Al-Si-coated PHS was undertaken, and the effect of Al-Si coating on nugget formation and mechanical properties was investigated. Press-hardened steel (PHS) has long been applied to automotive body structure construction to support mass and corresponding greenhouse gas emission reductions. PHS materials are often combined with an Al-Si coating applied as an oxidation barrier though unfortunately, the Al-Si coating poses a challenge to the resistance spot welding (RSW) of PHS containing stack-ups. As a newly developed coating for the hot stamping process, the property of Al-Si coating is different from base metal and traditional coatings, and the influence mechanism of Al-Si coating on the welding process is not clear. It would remain at nugget edge and might cause severe stress concentration. To investigate this problem, RSW of 1.5-mm Al-Si-coated PHS was undertaken, and the results indicate that a large portion of the Al-Si coating is extruded and forms a sharp notch close to the nugget edge during the welding process. During the post-weld cooling stage, a thin layer of residual coating is formed between the nugget and notch root. The mechanical performance of the welded joints is limited by the thin residual Al-Si layer which acts as a preexisting crack and supports the interfacial fracture. The presence of the Al-Si coating at the faying interface also significantly delays nugget formation, though it contributes to a larger nugget size by inhibiting expulsion events at the faying interface.
引用
收藏
页码:626 / 636
页数:11
相关论文
共 27 条
[1]   Microstructure-properties relationships in martensitic stainless steel resistance spot welds [J].
Alizadeh-Sh, M. ;
Marashi, S. P. H. ;
Pouranvari, M. .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2014, 19 (07) :595-602
[2]  
[Anonymous], 2009, STAHL AUT LEICHT SIC
[3]   Development of Cold-Rolled High-Strength Formable Steel for Automotive Applications [J].
Bhagat, A. N. ;
Singh, Avtar ;
Gope, N. ;
Venugopalan, T. .
MATERIALS AND MANUFACTURING PROCESSES, 2010, 25 (1-3) :202-205
[4]  
Chen Shu-jun, 2010, Electric Welding Machine, V40, P70
[5]   Microstructural evolution of intermetallic layer in hot-dipped aluminide mild steel with silicon addition [J].
Cheng, Wei-Jen ;
Wang, Chaur-Jeng .
SURFACE & COATINGS TECHNOLOGY, 2011, 205 (19) :4726-4731
[6]   Microstructure of liquid metal embrittlement cracks on Zn-coated 22MnB5 press-hardened steel [J].
Cho, Lawrence ;
Kang, Heeseung ;
Lee, Changwook ;
De Cooman, Bruno C. .
SCRIPTA MATERIALIA, 2014, 90-91 :25-28
[7]   Evaluation of weldability for resistance spot welded single-lap joint between GA780DP and hot-stamped 22MnB5 steel sheets [J].
Choi, Hong-Seok ;
Park, Geun-Hwan ;
Lim, Woo-Seung ;
Kim, Byung-min .
JOURNAL OF MECHANICAL SCIENCE AND TECHNOLOGY, 2011, 25 (06) :1543-1550
[8]  
Drillet P., 2013, METALL ITAL, V1
[9]   ON THE INFLUENCE OF SILICON ON THE GROWTH OF THE ALLOY LAYER DURING HOT DIP ALUMINIZING [J].
EGGELER, G ;
AUER, W ;
KAESCHE, H .
JOURNAL OF MATERIALS SCIENCE, 1986, 21 (09) :3348-3350
[10]   Plasticity and fracture modeling of quench-hardenable boron steel with tailored properties [J].
Eller, T. K. ;
Greve, L. ;
Andres, M. T. ;
Medricky, M. ;
Hatscher, A. ;
Meinders, V. T. ;
van den Boogaard, A. H. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2014, 214 (06) :1211-1227