摘要
Wood fiber-reinforced polylactic acid (PLA) composites (WFRPCs) were used as a filament to manufacture the unidirectional WFRPC components by means of fused deposition modeling (FDM). The physico-mechanical properties of the WFRPC components printed at different extrusion temperatures (200, 210, 220, and 230 degrees C) were determined. The results revealed that most of the physical properties (moisture content, surface roughness, water absorption rate, and thickness swelling rate) of the printed WFRPC component were not significantly influenced by extrusion temperature, while its density and color difference increased as the extrusion temperature increased. Additionally, the tensile and flexural properties of the FDM-printed WFRPC component decreased when the extrusion temperature was more than 200 degrees C, whereas the compressive strength and internal bond strength increased by 15.1% and 24.3%, respectively, when the extrusion temperature was increased from 200 to 230 degrees C. Furthermore, scanning electronic microscopy (SEM) demonstrated that the fracture surface of the tensile component printed at a higher extrusion temperature exhibited a better compatibility at fiber/PLA interfaces and good adhesion between the extruded filament segments. These results indicate that the FDM printing process using different extrusion temperatures has a substantial impact on the surface color, density, and mechanical properties of the printed WFRPC component.
引用
收藏
页数:11
相关论文
共 43 条
[1]   Hybrid composites made from recycled materials: Moisture absorption and thickness swelling behavior [J].
Ashori, Alireza ;
Sheshmani, Shabnam .
BIORESOURCE TECHNOLOGY, 2010, 101 (12) :4717-4720
[2]   Thermorheological and mechanical properties of cellulose reinforced PLA bio-composites [J].
Awal, A. ;
Rana, M. ;
Sain, M. .
MECHANICS OF MATERIALS, 2015, 80 :87-95
[3]   Heat treated wood-nylon 6 composites [J].
Aydemir, Deniz ;
Kiziltas, Alper ;
Kiziltas, Esra Erbas ;
Gardner, Douglas J. ;
Gunduz, Gokhan .
COMPOSITES PART B-ENGINEERING, 2015, 68 :414-423
[4]  
Ayrilmis N, 2011, J TROP FOR SCI, V23, P10
[5]   Effect of thermal-treatment of wood fibres on properties of flat-pressed wood plastic composites [J].
Ayrilmis, Nadir ;
Jarusombuti, Songklod ;
Fueangvivat, Vallayuth ;
Bauchongkol, Piyawade .
POLYMER DEGRADATION AND STABILITY, 2011, 96 (05) :818-822
[6]   Effect of high temperature on the change in color, dimensional stability and mechanical properties of spruce wood [J].
Bekhta, P ;
Niemz, P .
HOLZFORSCHUNG, 2003, 57 (05) :539-546
[7]   Mechanical performance of biocomposites based on PLA and PHBV reinforced with natural fibres - A comparative study to PP [J].
Bledzki, A. K. ;
Jaszkiewicz, A. .
COMPOSITES SCIENCE AND TECHNOLOGY, 2010, 70 (12) :1687-1696
[8]   Mechanical properties of PLA composites with man-made cellulose and abaca fibres [J].
Bledzki, Andrzej K. ;
Jaszkiewicz, Adam ;
Scherzer, Dietrich .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2009, 40 (04) :404-412
[9]   THE COLOR MEASUREMENT - A FAST METHOD TO STUDY AND TO OPTIMIZE THE CHEMICAL-TRANSFORMATIONS UNDER-GONE IN THE THERMICALLY TREATED WOOD [J].
BOURGOIS, J ;
JANIN, G ;
GUYONNET, R .
HOLZFORSCHUNG, 1991, 45 (05) :377-382
[10]   Fused deposition modeling with polypropylene [J].
Carneiro, O. S. ;
Silva, A. F. ;
Gomes, R. .
MATERIALS & DESIGN, 2015, 83 :768-776