Study on Formation Mechanism by Monitoring the Morphology and Structure Evolution of Nearly Monodispersed Fe3O4 Submicroparticles with Controlled Particle Sizes

被引:143
作者
Fan, Ting [1 ]
Pan, Dengke [1 ]
Zhang, Hui [1 ]
机构
[1] Beijing Univ Chem Technol, State Key Lab Chem Resource Engn, Beijing 100029, Peoples R China
关键词
COATED MAGNETITE NANOPARTICLES; IRON-OXIDES; HYDROTHERMAL SYNTHESIS; SHELL STRUCTURE; MICROSPHERES; GAMMA-FE2O3; OXIDATION; CORE; NANOCRYSTALS; ACETATE;
D O I
10.1021/ie200970j
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
We present a facile surfactant-free solvothermal method for the fabrication of nearly monodispersed Fe3O4 submicroparticles with tunable particle sizes ranging from 130 to 420 nm by varying the concentration of single iron source FeCl3 center dot 6H(2)O in initial solutions. The morphology and crystal structure of the as-prepared Fe3O4 submicroparticles have been well characterized by using SEM/TEM/HRTEM, XRD, FT-IR, Raman spectroscopy, and XPS methods. It is found that the Fe3O4 particles present single-crystal nature and strong ferromagnetic property with magnetization saturation values ranged in 54.3-88.7 emu . g(-f). A complexation-aggregation-phase transformation formation mechanism was first proposed for the nearly monodispersed single-crystal Fe3O4 submicroparticles based upon the quasi-in situ monitoring of the morphology and structure evolution of the samples during the synthesis process. These size-tunable nearly monodispersed Fe3O4 submicroparticles are expected to have promising applications in wide research fields such as bioseparation, targeted drug delivery, and catalysis.
引用
收藏
页码:9009 / 9018
页数:10
相关论文
共 60 条
[1]  
[Anonymous], 1996, The Iron Oxides
[2]   Shape-tuned synthesis of dispersed magnetite submicro particles with good magnetic properties [J].
Bai, Wei ;
Meng, Xiangjian ;
Zhu, Xia ;
Jing, Chengbin ;
Gao, Cheng ;
Chu, Junhao .
PHYSICA E-LOW-DIMENSIONAL SYSTEMS & NANOSTRUCTURES, 2009, 42 (02) :141-145
[3]   Influence of grain size, oxygen stoichiometry, and synthesis conditions on the γ-Fe2O3 vacancies ordering and lattice parameters [J].
Belin, T ;
Guigue-Millot, N ;
Caillot, T ;
Aymes, D ;
Niepce, JC .
JOURNAL OF SOLID STATE CHEMISTRY, 2002, 163 (02) :459-465
[4]   CORE AND VALENCE LEVEL PHOTOEMISSION STUDIES OF IRON-OXIDE SURFACES AND OXIDATION OF IRON [J].
BRUNDLE, CR ;
CHUANG, TJ ;
WANDELT, K .
SURFACE SCIENCE, 1977, 68 (01) :459-468
[5]   FTIR and NMR study of poly(lactide-co-glycolide) and hydroxyapatite implant degradation under in vivo conditions [J].
Chlopek, J. ;
Morawska-Chochol, A. ;
Paluszkiewicz, C. ;
Jaworska, J. ;
Kasperczyk, J. ;
Dobrzynski, P. .
POLYMER DEGRADATION AND STABILITY, 2009, 94 (09) :1479-1485
[6]   Topotactic transformations of goethite and lepidocrocite into hematite and maghemite [J].
Cudennec, Y ;
Lecerf, A .
SOLID STATE SCIENCES, 2005, 7 (05) :520-529
[7]  
Cullity B. D., 1978, ELEMENTS XRAY DIFFRA
[8]   Hydrothermal synthesis of monodisperse magnetite nanoparticles [J].
Daou, T. J. ;
Pourroy, G. ;
Begin-Colin, S. ;
Greneche, J. M. ;
Ulhaq-Bouillet, C. ;
Legare, P. ;
Bernhardt, P. ;
Leuvrey, C. ;
Rogez, G. .
CHEMISTRY OF MATERIALS, 2006, 18 (18) :4399-4404
[9]  
deFaria DLA, 1997, J RAMAN SPECTROSC, V28, P873, DOI 10.1002/(SICI)1097-4555(199711)28:11<873::AID-JRS177>3.0.CO
[10]  
2-B