Durability of PSS-supported Pd-membranes under mixed gas and water-gas shift conditions

被引:31
作者
Augustine, Alexander S. [1 ]
Mardilovich, Ivan P. [1 ]
Kazantzis, Nikolaos K. [1 ]
Ma, Yi Hua [1 ]
机构
[1] Worcester Polytech Inst, Dept Chem Engn, Ctr Inorgan Membrane Studies, Worcester, MA 01609 USA
关键词
Pd-membrane reactor; Water-gas-shift reaction; Long-term testing; Mixed-gas testing; Reactor performance assessment; LONG-TERM STABILITY; COMPOSITE MEMBRANES; HYDROGEN-PRODUCTION; CARBON-MONOXIDE; THIN PD/AG; REACTORS; STEAM; SIMULATION; MORPHOLOGY; SEPARATION;
D O I
10.1016/j.memsci.2012.05.001
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The palladium-based catalytic membrane reactor (Pd-CMR) as well as the palladium-based membrane separator have demonstrated a wide ranging applicability to the fields of H-2 production and clean power generation. One of the key requirements in these two application fields remains the synthesis of robust, composite, dense metal membranes which exhibit high H-2 permeance as well as long-term selectivity stability. Within such a context, a porous stainless steel supported thin Pd-membrane with an H-2 permeance of 34 m(3)/m(2)-h-bar(0.5) (400 degrees C) has been prepared and tested under H-2/H2O(10-37%) mixed gas conditions, 2.6-6.1 bar and 400-450 degrees C for up to 190 h. Two similar membranes with H-2 permeance of 23 and 28 m(3)/m(2)-h-bar(0.5), were also tested under water-gas-shift (WGS) reaction conditions (42% CO, 40% H-2, 18% CO2), H2O/CO ratio of 2-3, 7.9-14.7 bar, 400 degrees C and 2700 h(-1) for up to 1000 h. At the highest pressure level a stable CO conversion and H-2 recovery of 97 and 88% respectively were achieved for 900 h which is indicative of the overall system stability. All the membranes exhibited leak growth under mixed and WGS conditions at similar rates (3.1 x 10(-7)-2.2 x 10(-5) m(3)/m(2)-h-bar) as those measured during pure H-2 testing, suggesting that the reactive atmosphere did not permanently harm the dense Pd-layer. Additionally, a significant part of the leak growth that was experimentally observed during the 1000 hour WGS test can be reasonably attributed to defects inherent to the welded regions of the PSS316L supports utilized in the present research study. (c) 2012 Elsevier B.V. All rights reserved.
引用
收藏
页码:213 / 220
页数:8
相关论文
共 40 条
[31]  
Perry R., 1997, PERRYS CHEM ENG HDB, V7th
[32]   Thin Pd-23%Ag/stainless steel composite membranes: Long-term stability, life-time estimation and post-process characterisation [J].
Peters, T. A. ;
Tucho, W. M. ;
Ramachandran, A. ;
Stange, M. ;
Walmsley, J. C. ;
Holmestad, R. ;
Borg, A. ;
Bredesen, R. .
JOURNAL OF MEMBRANE SCIENCE, 2009, 326 (02) :572-581
[33]   Effect of H2S on the Performance and Long-Term Stability of Pd/Cu Membranes [J].
Pomerantz, Natalie ;
Ma, Yi Hua .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2009, 48 (08) :4030-4039
[34]   Influence of alloy composition and membrane fabrication on the pressure dependence of the hydrogen flux of palladium-copper membranes [J].
Roa, F ;
Way, JD .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2003, 42 (23) :5827-5835
[35]   Development of membrane reformer system for highly efficient hydrogen production from natural gas [J].
Shirasaki, Y. ;
Tsuneki, T. ;
Ota, Y. ;
Yasuda, I. ;
Tachibana, S. ;
Nakajima, H. ;
Kobayashi, K. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2009, 34 (10) :4482-4487
[36]   CATALYTIC PALLADIUM-BASED MEMBRANE REACTORS - A REVIEW [J].
SHU, J ;
GRANDJEAN, BPA ;
VANNESTE, A ;
KALIAGUINE, S .
CANADIAN JOURNAL OF CHEMICAL ENGINEERING, 1991, 69 (05) :1036-1060
[37]  
Torkelson J., 2008, DOEDEFC2605NT42452
[38]   The solubility and diffusion of carbon in palladium [J].
Yokoyama, H ;
Numakura, H ;
Koiwa, M .
ACTA MATERIALIA, 1998, 46 (08) :2823-2830
[39]   FORMATION OF INTERSTITIAL PD-C PHASE BY INTERACTION OF ETHYLENE, ACETYLENE, AND CARBON-MONOXIDE WITH PALLADIUM [J].
ZIEMECKI, SB ;
JONES, GA ;
SWARTZFAGER, DG ;
HARLOW, RL .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1985, 107 (15) :4547-4548
[40]  
2000, Patent No. 6152987