Selective adsorption mechanism of salicylic acid on pyrite surfaces and its application in flotation separation of chalcopyrite from pyrite

被引:121
作者
Han, Guang [1 ]
Wen, Shuming [1 ]
Wang, Han [1 ]
Feng, Qicheng [1 ]
机构
[1] Kunming Univ Sci & Technol, State Key Lab Complex Nonferrous Met Resources Cl, Fac Land Resource Engn, Kunming 650093, Yunnan, Peoples R China
基金
中国国家自然科学基金;
关键词
Salicylic acid; Pyrite; Chalcopyrite; Flotation separation; Low alkalinity; MACROMOLECULAR DEPRESSANT; ORGANIC DEPRESSANTS; FLOATABILITY; SPHALERITE; OXIDATION; SULFIDE; ASPIRIN; DEXTRIN; XPS; DFT;
D O I
10.1016/j.seppur.2020.116650
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
In the flotation process of copper sulfide, traditional inorganic depressants used for pyrite often cause environmental problems and difficulty in treatment of the tailings and waste water. Therefore, it is necessary to explore non-polluting and efficient flotation reagents to make mineral processing environmentally friendly and sustainable. In this work, salicylic acid (SA) has been studied for adsorption on pyrite and chalcopyrite surfaces by surface-adsorption experiments. The interaction mechanism of SA with pyrite surfaces was demonstrated by zeta potential measurements, infrared spectroscopy, time-of-flight secondary-ion mass spectrometry (ToF-SIMS), and X-ray photoelectron spectroscopy (XPS). The impact of SA on the flotation behavior of chalcopyrite and pyrite was further verified by microflotation experiments. Adsorption experiments indicated that SA dramatically reduced the adsorption amounts of xanthate on pyrite surfaces, yet it exhibited a weaker impact on adsorption of xanthate on chalcopyrite surfaces. The zeta potential results showed that the potential of pyrite increased among an extensive pH range after treatment of SA. a new characteristic peak appeared in the pyrite SA infrared spectrum. ToF-SIMS and XPS analysis of the pyrite SA surfaces revealed a strong interaction between SA and Fe sites. Microflotation tests confirmed that SA had an obvious depression effect on pyrite, yet no clear depression effect on chalcopyrite. These results verified that selective adsorption of SA on pyrite weaken the floatability of pyrite, thereby enabling separation of chalcopyrite from pyrite at low alkalinity.
引用
收藏
页数:9
相关论文
共 45 条
[1]   Synthesis, structural, hirshfeld surface, spectroscopic studies and quantum chemical calculation of the proton transfer complex between 2-amino-4-hydroxy-6-methylpyrimidine and salicylic acid [J].
Afroz, Ziya ;
Faizan, Mohd ;
Alam, Mohammad Jane ;
Nunes Rodrigues, Vitor Hugo ;
Ahmad, Shabbir ;
Ahmad, Afaq .
JOURNAL OF MOLECULAR STRUCTURE, 2018, 1171 :438-448
[2]   Effects of type and dosages of organic depressants on pyrite floatability in microflotation system [J].
Ahmadi, Mehran ;
Gharabaghi, Mahdi ;
Abdollahi, Hadi .
ADVANCED POWDER TECHNOLOGY, 2018, 29 (12) :3155-3162
[3]   Adsorption of guar gum and CMC on pyrite [J].
Bicak, O. ;
Ekmekci, Z. ;
Bradshaw, D. J. ;
Harris, P. J. .
MINERALS ENGINEERING, 2007, 20 (10) :996-1002
[4]   Metal ions and dextrin adsorption on pyrite [J].
Bogusz, E ;
Brienne, SR ;
Butler, I ;
Rao, SR ;
Finch, JA .
MINERALS ENGINEERING, 1997, 10 (04) :441-445
[5]   Comparative XPS study between experimentally and naturally weathered pyrites [J].
Cai, Yuanfeng ;
Pan, Yuguan ;
Xue, Jiyue ;
Sun, Qingfeng ;
Su, Guizhen ;
Li, Xiang .
APPLIED SURFACE SCIENCE, 2009, 255 (21) :8750-8760
[6]   The role of sodium sulfide in the flotation of pyrite depressed in chalcopyrite flotation [J].
Cao, Zhao ;
Chen, Xumeng ;
Peng, Yongjun .
MINERALS ENGINEERING, 2018, 119 :93-98
[7]   Selective separation of pyrite from chalcopyrite and arsenopyrite by biomodulation using Acidithiobacillus ferrooxidans [J].
Chandraprabha, MN ;
Natarajan, KA ;
Somasundaran, P .
INTERNATIONAL JOURNAL OF MINERAL PROCESSING, 2005, 75 (1-2) :113-122
[8]   Molecular structures and activity of organic depressants for marmatite, jamesonite and pyrite flotation [J].
Chen Jian-hua ;
Li Yu-qiong ;
Long Qiu-rong .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2010, 20 (10) :1993-1999
[9]   Importance of oxidation during regrinding of rougher flotation concentrates with a high content of sulfides [J].
Chen, Xumeng ;
Seaman, David ;
Peng, Yongjun ;
Bradshaw, Dee .
MINERALS ENGINEERING, 2014, 66-68 :165-172
[10]   Investigation of pyrite oxidation by hexavalent chromium: Solution species and surface chemistry [J].
Demoisson, Frederic ;
Mullet, Martine ;
Humbert, Bernard .
JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2007, 316 (02) :531-540