Silanization of adhesively bonded aluminum alloy AA6060 with γ-glycidoxypropyltrimethoxysilane.: II.: Stability in degrading environments

被引:5
作者
Johnsen, BB
Olafsen, K
Stori, A
Vinje, K
机构
[1] SINTEF Mat Technol, Dept Polymers & Composit, NO-0314 Oslo, Norway
[2] Norwegian Univ Sci & Technol, Dept Machine Design & Mat Technol, NO-7491 Trondheim, Norway
关键词
adhesive bonding; aluminum; gamma-glycidoxypropyltrimethoxysilane; reflection-absorption infrared spectroscopy; durability;
D O I
10.1163/156856103322114589
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Alkaline etched aluminum alloy AA6060 treated with of gamma-glycidoxypropyltrimethoxysilane was investigated. The stability of the silane films in degrading environments was investigated by exposing them to acidic and alkaline solutions at 40degreesC, followed by analysis with reflection-absorption infrared spectroscopy. Desorption of the silane from the surface occurred at pH 4, and at a much slower rate at pH 7, while the silane film was stable at pH 8. Two models for the degradation of the silanized aluminum surface in an acidic environment were proposed: one involving simultaneously hydrolysis of the siloxane network and corrosion of the underlying aluminum surface, and the other involving only corrosion of the aluminum surface. The durability of the silane treated surface was determined using wedge tests on joints made with XD4600 one-component epoxy adhesive. The durability was significantly reduced in highly acidic environment (pH 2), but no significant differences in durability were observed in the pH range from 4 to 11, except that the durability was slightly higher in higher alkaline environment during the initial period of testing. Better durability in an alkaline environment is connected to a better stability of both the siloxane network and the aluminum surface in this environment.
引用
收藏
页码:1283 / 1298
页数:16
相关论文
共 30 条
[21]   The interaction of a commercial dry film adhesive with aluminium and organosilane treated aluminium surfaces: a study by XPS and ToF-SIMS [J].
Rattana, A ;
Hermes, JD ;
Abel, ML ;
Watts, JF .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2002, 22 (03) :205-218
[22]  
RATTANA A, 2001, P 24 ANN M ADH SOC, P202
[23]   INFLUENCE OF SIMPLE SURFACE TREATMENTS ON THE DURABILITY OF BONDED ALUMINUM-ALLOY PLATES [J].
RIDER, AN ;
ARNOTT, DR ;
WILSON, AR ;
VARGAS, O .
INTERFACES II, 1995, 189- :235-240
[24]   Boiling water and silane pre-treatment of aluminium alloys for durable adhesive bonding [J].
Rider, AN ;
Arnott, DR .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2000, 20 (03) :209-220
[25]   SILANE COUPLING AGENTS AS ADHESION PROMOTERS FOR AEROSPACE STRUCTURAL FILM ADHESIVES [J].
THIEDMAN, W ;
TOLAN, FC ;
PEARCE, PJ ;
MORRIS, CEM .
JOURNAL OF ADHESION, 1987, 22 (03) :197-210
[26]   A study of the curing of 3-glycidoxypropyltrimethoxy silane films on aluminum [J].
Underhill, PR ;
Goring, G ;
DuQuesnay, DL .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 1998, 18 (05) :313-317
[27]   The drying of 3-glycidoxypropyltrimethoxy silane [J].
Underhill, PR ;
Goring, G ;
DuQuesnay, DL .
APPLIED SURFACE SCIENCE, 1998, 134 (1-4) :247-253
[28]   A study of the deposition of 3-glycidoxypropyltrimethoxysilane on aluminum [J].
Underhill, PR ;
Goring, G ;
DuQuesnay, DL .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 1998, 18 (05) :307-311
[29]   The effect of humidity on the curing of 3-glycidoxypropyltrimethoxy silane [J].
Underhill, PR ;
Goring, G ;
DuQuesnay, DL .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2000, 20 (03) :195-199
[30]   Modelling the interaction of hybrid inorganic-organic molecules on oxide surfaces:: glycidyl isopropyl ether and epoxyhexane on a γ-Al2O3(111) mimic [J].
Woods, GA ;
Haq, S ;
Richardson, NV ;
Shaw, S ;
Digby, R ;
Raval, R .
SURFACE SCIENCE, 1999, 433 :199-204