On the interface between porcelain and titanium

被引:3
|
作者
Guo, Litong [1 ]
Gao, Jiqiang [1 ]
Liu, Xiaochen [2 ]
Guo, Tianwen [3 ]
He, Zengying [1 ]
机构
[1] Xi An Jiao Tong Univ, State Key Lab Mech Behav Mat, Xian 710049, Peoples R China
[2] Zhejiang Univ, Affiliated Hosp Stomatol, Dept Prosthodent, Hangzhou PT-310006, Peoples R China
[3] Fourth Mil Med Univ, Xian 710032, Peoples R China
来源
HIGH-PERFORMANCE CERAMICS V, PTS 1 AND 2 | 2008年 / 368-372卷
关键词
porcelain-fused-to-metal; titanium; three-point flexure test; corrosion; ADHERENCE; ALLOY;
D O I
10.4028/www.scientific.net/KEM.368-372.1618
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Low-fusing dental porcelain was fused on titanium surface. The adhesion between the titanium and porcelain was evaluated by three-point flexure test. It was shown that the failure of the titanium-porcelain predominantly occurred at the alloy-oxide interface. Rutile phase was present on the interface debonding from porcelain. The influence of corrosion on bonding strength was also investigated. The results suggested that, after being immersed in artificial saliva with pH of 2.7, 5.4 and 7.0. no decreasing of the bonding strength of Ti-porcelain occurred.
引用
收藏
页码:1618 / +
页数:2
相关论文
共 50 条
  • [21] Synthesis and Characterization of Titanium Dentin Porcelain
    Guo, Litong
    Liu, Xuemei
    Zhang, Ye
    Guo, Lizhi
    Guo, Tianwen
    MATERIALS AND MANUFACTURING PROCESSES, 2011, 26 (10) : 1269 - 1272
  • [22] Chromatic behavior of porcelain fired on titanium
    Lakatos, Sorin
    Lakatos, Carmen
    Rominu, Mihai
    Florita, Zeno
    QUINTESSENCE INTERNATIONAL, 2007, 38 (07): : E368 - E373
  • [23] Preparation and Characterization of a Titanium Opaque Porcelain
    Guo, Litong
    Shi, Yao
    Guo, Lizhi
    Zhang, Qian
    Liu, Xuemei
    Xu, Cheng
    Guo, Tianwen
    MATERIALS AND MANUFACTURING PROCESSES, 2012, 27 (11) : 1189 - 1192
  • [24] Preparation of nanostructured Titanium surfaces for investigations of the interface between cell monolayers and Titanium
    Heeren, A.
    Burkhardt, C.
    Wolburg, H.
    Henschel, W.
    Nisch, W.
    Kern, D. P.
    MICROELECTRONIC ENGINEERING, 2006, 83 (4-9) : 1602 - 1604
  • [25] The Role of Oxygen at the Interface between Titanium and Carbon Nanotubes
    Felten, Alexandre
    Suarez-Martinez, Irene
    Ke, Xiaoxing
    Van Tendeloo, Gustaaf
    Ghijsen, Jacques
    Pireaux, Jean-Jacques
    Drube, Wolfgang
    Bittencourt, Carla
    Ewels, Christopher P.
    CHEMPHYSCHEM, 2009, 10 (11) : 1799 - 1804
  • [26] Influence of ultraviolet irradiation treatment on porcelain bond strength of titanium surfaces
    Kumasaka, Tomonari
    Ohno, Akinori
    Hori, Norio
    Hoshi, Noriyuki
    Maruo, Katsuichiro
    Kuwabara, Atsushi
    Seimiya, Kazuhide
    Toyoda, Minoru
    Kimoto, Katsuhiko
    DENTAL MATERIALS JOURNAL, 2018, 37 (03) : 422 - 428
  • [27] Effects of micro-arc oxidation on bond strength of titanium to porcelain
    Li, Jian-Xue
    Zhang, Yu-Mei
    Han, Yong
    Zhao, Yi-Min
    SURFACE & COATINGS TECHNOLOGY, 2010, 204 (08) : 1252 - 1258
  • [28] Shear bond strength and characterization of interfaces between electroformed gold substrates and porcelain
    Al Jabbari, Y. S.
    Barbagadaki, X.
    Al Wazzan, K. A.
    El-Danaf, E. A.
    Eliades, G.
    Zinelis, S.
    MATERIALS CHEMISTRY AND PHYSICS, 2013, 137 (03) : 825 - 833
  • [29] Determination of peeling plane of the fused porcelain to titanium
    Miura, E
    Jie, L
    Watanabe, I
    Tanaka, Y
    Shiraishi, T
    Hisatsune, K
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 2001, 65 (09) : 819 - 822
  • [30] Bond strength of binary titanium alloys to porcelain
    Yoda, M
    Konno, T
    Takada, Y
    Iijima, K
    Griggs, J
    Okuno, O
    Kimura, K
    Okabe, T
    BIOMATERIALS, 2001, 22 (12) : 1675 - 1681