Influence of green inhibitor on flow-accelerated corrosion of API X70 line pipe steel in synthetic oilfield water

被引:11
作者
Ajmal, T. S. [1 ]
Arya, Shashi Bhushan [1 ]
Thippeswamy, L. R. [2 ]
Quraishi, M. A. [3 ,4 ]
Haque, Jiyaul [3 ]
机构
[1] Natl Inst Technol Karnataka, Dept Met & Mat Engn, Mangalore 575025, India
[2] Natl Inst Technol Karnataka, Dept Mech Engn, Mangalore, India
[3] Banaras Hindu Univ, Dept Chem, Indian Inst Technol, Varanasi, Uttar Pradesh, India
[4] King Fahd Univ Petr & Minerals, Res Inst, Ctr Res Excellence Corros, Dhahran, Saudi Arabia
关键词
Flow-accelerated corrosion (FAC); carbon steel pipe; oleic acid hydrazide (OAH) inhibitor; electrochemical impedance spectroscopy; CARBON-DIOXIDE CORROSION; MILD-STEEL; BEHAVIOR; IMIDAZOLINE; HYDRODYNAMICS; PERFORMANCE; METHIONINE; MECHANISM; ACID;
D O I
10.1080/1478422X.2020.1745355
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Inhibition effect of oleic acid hydrazide (OAH), a green corrosion inhibitor on API X70 steel in an Indian oilfield produced water was investigated for the first time under flow condition. The test was carried out at a more critical location (90-degree pipe elbow) in a circulating loop system with the fixed flow velocity. This location is deliberately chosen because, at this location, catastrophic failure of a low alloy steel piping system usually takes place under highly corrosive turbulent flow with higher wall shear stress and flow velocity. The corrosion examination was carried out by varying the concentrations (0.05, 0.15, 0.30 g L-1) of the OAH inhibitor under flow condition. The maximum inhibitor efficiency is found 87.7% at 0.30 g L-1 concentration. The formation of protective film was confirmed by SEM, XPS, Raman spectroscopy and FTIR spectra.
引用
收藏
页码:487 / 496
页数:10
相关论文
共 50 条
[1]  
Ahmed W. H., 2012, NUCL POWER PRACTICAL, DOI [10.5772/51346, DOI 10.5772/51346]
[2]   Experimental investigation of flow accelerated corrosion under two-phase flow conditions [J].
Ahmed, Wael H. ;
Bello, Mufatiu M. ;
El Nakla, Meamer ;
Al Sarkhi, Abdelsalam ;
Badr, Hassan M. .
NUCLEAR ENGINEERING AND DESIGN, 2014, 267 :34-43
[3]   Effect of hydrodynamics on the flow accelerated corrosion (FAC) and electrochemical impedance behavior of line pipe steel for petroleum industry [J].
Ajmal, T. S. ;
Arya, Shashi Bhushan ;
Udupa, K. Rajendra .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2019, 174 :42-53
[4]   Corrosion inhibition and adsorption mechanism studies of Hunteria umbellata seed husk extracts on mild steel immersed in acidic solutions [J].
Alaneme, Kenneth Kanayo ;
Olusegun, Sunday Joseph ;
Adelowo, Oluwabunkunmi Tomi .
ALEXANDRIA ENGINEERING JOURNAL, 2016, 55 (01) :673-681
[5]  
Ameh P.O., 2017, J. Ind. Environ. Chem., V1, P15
[6]  
[Anonymous], 2014, ASTM Int, V97, P1, DOI [DOI 10.1520/G0059-97R14.2, DOI 10.1520/G0059-97R14]
[7]   Effect of hydrodynamic conditions on the inhibition performance of L-methionine as a "green" inhibitor [J].
Ashassi-Sorkhabi, H. ;
Asghari, E. .
ELECTROCHIMICA ACTA, 2008, 54 (02) :162-167
[8]  
Bruice PY., 2014, ORGANIC CHEM, P594
[9]   Effects of Microstructure on Corrosion of X70 Pipe Steel in an Alkaline Soil [J].
Du, C. W. ;
Li, X. G. ;
Liang, P. ;
Liu, Z. Y. ;
Jia, G. F. ;
Cheng, Y. F. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2009, 18 (02) :216-220
[10]   Development of a structure-activity relationship for oil field corrosion inhibitors [J].
Durnie, W ;
De Marco, R ;
Jefferson, A ;
Kinsella, B .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1999, 146 (05) :1751-1756