Friction and wear behaviors of biodegradable Mg-6Gd-0.5Zn-0.4Zr alloy under simulated body fluid condition

被引:27
|
作者
Dai, Jianwei [1 ,2 ]
Zhang, Xiaobo [1 ,2 ]
Yin, Qiao [1 ]
Ni, Shengnan [1 ]
Ba, Zhixin [1 ,2 ]
Wang, Zhangzhong [1 ,2 ]
机构
[1] Nanjing Inst Technol, Sch Mat Sci & Engn, 1 Hongjing Rd, Nanjing 211167, Jiangsu, Peoples R China
[2] Jiangsu Key Lab Adv Struct Mat & Applicat Technol, Nanjing, Jiangsu, Peoples R China
关键词
Biodegradable Mg alloy; SBF; Friction coefficient; Wear behavior; CORROSION BEHAVIOR; MAGNESIUM ALLOYS; MG; DEGRADATION; IMPLANTS;
D O I
10.1016/j.jma.2017.11.002
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The friction and wear behaviors of biodegradable Mg-6Gd-0.5Zn-0.4Zr (wt%, GZ60K) alloy were evaluated under simulated body fluid (SBF) condition using ball-on-disk configuration and compared with those under dry sliding condition. The results show that under dry sliding and SBF conditions, the friction coefficient declines with increasing applied load and keeps stable with prolonging sliding time. The friction coefficient of the alloy effectively decreases in SBF as compared to dry sliding due to lubrication caused by SBF. The real wear rates under SBF condition are lower than those under dry sliding condition for each parameter. Nevertheless, the nominal wear rates are higher in SBF which are attributed to the more mass loss caused by corrosion but not wear. Both the nominal wear rate in SBF and the dry sliding wear rate increase with increasing applied load, and they decline firstly and then keep stable with prolonging sliding time. It is concluded that the wear of the alloy is restricted by the SBF, but the corrosion of the alloy is aggravated by the wear. (c) 2017 Production and hosting by Elsevier B.V. on behalf of Chongqing University. This is an open access article under the CC BY-NC-ND license.
引用
收藏
页码:448 / 453
页数:6
相关论文
共 50 条
  • [31] Microstructure, mechanical and biodegradable properties of a Mg-2Zn-1Gd-0.5Zr alloy with different solution treatments
    Chen, Jun-Xiu
    Gao, Ming
    Tan, Li-Li
    Yang, Ke
    RARE METALS, 2019, 38 (06) : 532 - 542
  • [32] Friction and wear behavior of Mg–11Y–5Gd–2Zn–0.5Zr (wt%) alloy with oil lubricant
    Li-Jie Cao
    Qu-Dong Wang
    Yu-Juan Wu
    Bing Ye
    Rare Metals, 2013, 32 : 453 - 458
  • [33] Investigation of corrosion behaviors of Mg-6Gd-3Y-0.4Zr alloy in NaCl aqueous solutions
    Guo, Xing-Wu
    Chang, Jian-Wei
    He, Shang-Ming
    Ding, Wen-Jiang
    Wang, Xishu
    ELECTROCHIMICA ACTA, 2007, 52 (07) : 2570 - 2579
  • [34] Biocorrosion of Biodegradable Implant Mg-xCa-4Zn Alloy in Simulated Body Fluid with the Addition of Ca
    Wang, Jijie
    Feng, Yuejiao
    Cui, Tong
    Jiang, Da
    Li, Na
    Wang, Yanjing
    FUNCTIONAL MATERIALS AND NANOTECHNOLOGY, 2012, 496 : 181 - +
  • [35] Effect of isothermal homogenization on microstructure and mechanical properties of the Mg-5Y-4Gd-0.5Zn-0.4Zr alloy
    Liu, Ke
    Wang, Xudong
    Wen, Kai
    MATERIALS & DESIGN, 2013, 52 : 1035 - 1042
  • [36] Effect of Heat Treatment on Microstructures and Mechanical Properties of Mg-5.5Gd-3.5Nd-0.5Zn-0.4Zr Alloy
    Li, Zhengqiu
    Zhang, Deming
    Zhao, Zhihao
    Xia, Chunyang
    Zhu, Yijun
    Liu, Ziqi
    TRANSACTIONS OF THE INDIAN INSTITUTE OF METALS, 2022, 75 (11) : 2883 - 2890
  • [37] Fatigue behaviors of HP-Mg, Mg-Ca and Mg-Zn-Ca biodegradable metals in air and simulated body fluid
    Bian, Dong
    Zhou, Weirui
    Liu, Yang
    Li, Nan
    Zheng, Yufeng
    Sun, Zhili
    ACTA BIOMATERIALIA, 2016, 41 : 351 - 360
  • [38] Corrosion and wear behavior of an Mg–2Zn–0.2Mn alloy in simulated body fluid
    De-Bao Liu
    Bo Wu
    Xiao Wang
    Min-Fang Chen
    Rare Metals, 2015, 34 : 553 - 559
  • [39] Effect of solution treatment on microstructure and corrosion resistance of biodegradable Mg-2.0Zn-0.5Zr-3.0Gd magnesium alloy
    Yao H.
    Wen J.-B.
    Xiong Y.
    He J.-G.
    Liu Y.
    Li X.-Y.
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2019, 29 (03): : 498 - 507
  • [40] Corrosion and wear behavior of an Mg–2Zn–0.2Mn alloy in simulated body fluid
    De-Bao Liu
    Bo Wu
    Xiao Wang
    Min-Fang Chen
    RareMetals, 2015, 34 (08) : 553 - 559