Fatigue behaviors of AISI 316L stainless steel with a gradient nanostructured surface layer

被引:465
作者
Huang, H. W. [1 ]
Wang, Z. B. [1 ]
Lu, J. [2 ]
Lu, K. [1 ,3 ]
机构
[1] Chinese Acad Sci, Inst Met Res, Shenyang Natl Lab Mat Sci, Shenyang 110016, Peoples R China
[2] City Univ Hong Kong, Dept Mfg Engn & Engn Management, Hong Kong, Hong Kong, Peoples R China
[3] Nanjing Univ Sci & Technol, Herbert Gleiter Inst Nanosci, Nanjing 210094, Jiangsu, Peoples R China
基金
中国国家自然科学基金;
关键词
Gradient nanostructures; Surface mechanical rolling treatment; AISI 316L stainless steel; Fatigue; Strain localization; HIGH-CYCLE FATIGUE; MECHANICAL ATTRITION TREATMENT; SEVERE PLASTIC-DEFORMATION; INDUCED RESIDUAL-STRESSES; NANOCRYSTALLINE METALS; GRINDING TREATMENT; GRAINED COPPER; ALLOY; RESISTANCE; STABILITY;
D O I
10.1016/j.actamat.2014.12.057
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
By means of surface mechanical rolling treatment (SMRT), a gradient nanostructured (GNS) surface layer was formed on AISI 316L stainless steel. The mean grain size is similar to 30 nm in the topmost surface layer and increases with depth. Tension compression fatigue measurements were performed on the SMRT sample under the stress-controlled mode. In comparison with the coarse-grained sample, the fatigue strength of the SMRT sample is significantly enhanced in both the low- and high-cycling fatigue regimes. Meanwhile, the fatigue ratio is evidently elevated with an increasing tensile strength in the SMRT sample. The initiation and growth of cracks, the cyclic deformation behaviors, as well as effects of strength and residual stresses, have been investigated to clarify the fatigue mechanism of the SMRT sample. The results emphasized the GNS surface layer enhances the fatigue property by suppressing the initiation of cracks and accommodating a remarkable cyclic plastic strain amplitude. (C) 2015 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:150 / 160
页数:11
相关论文
共 60 条
  • [1] Cyclic deformation and near surface microstructures of shot peened or deep rolled austenitic stainless steel AISI 304
    Altenberger, I
    Scholtes, B
    Martin, U
    Oettel, H
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1999, 264 (1-2): : 1 - 16
  • [2] The effect of shot peening on fatigue and corrosion behavior of 316L stainless steel in Ringer's solution
    Azar, V.
    Hashemi, B.
    Yazdi, Mahboobeh Rezaee
    [J]. SURFACE & COATINGS TECHNOLOGY, 2010, 204 (21-22) : 3546 - 3551
  • [3] Fatigue properties of nanocrystallized surfaces obtained by high energy shot peening
    Bagherifard, S.
    Fernandez Pariente, I.
    Ghelichi, R.
    Guagliano, M.
    [J]. FATIGUE 2010, 2010, 2 (01): : 1683 - 1690
  • [4] FUNDAMENTAL-ASPECTS OF LOW AMPLITUDE CYCLIC DEFORMATION IN FACE-CENTERED CUBIC-CRYSTALS
    BASINSKI, ZS
    BASINSKI, SJ
    [J]. PROGRESS IN MATERIALS SCIENCE, 1992, 36 : 89 - 148
  • [5] Bassler H-J, 1997, 24 ANN REV PROGR QUA
  • [6] Influence of martensitic transformation on the low-cycle fatigue behaviour of 316LN stainless steel at 77 K
    Botshekan, M
    Degallaix, S
    Desplanques, Y
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1997, 234 : 463 - 466
  • [7] Crack tip plasticity in plastically graded Ni-W electrodeposited nanocrystalline alloys
    Cavaliere, P.
    [J]. COMPUTATIONAL MATERIALS SCIENCE, 2008, 41 (04) : 440 - 449
  • [8] Cavaliere P., 2009, J FATIGUE, V31, P1476
  • [9] Tensile properties of a nanocrystalline 316L austenitic stainless steel
    Chen, XH
    Lu, J
    Lu, L
    Lu, K
    [J]. SCRIPTA MATERIALIA, 2005, 52 (10) : 1039 - 1044
  • [10] Analysis of fatigue resistance improvements via surface severe plastic deformation
    Dai, K.
    Shaw, L.
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2008, 30 (08) : 1398 - 1408