Fabrication of nickel and chromium nanoparticles using the protein cage of apoferritin

被引:173
作者
Okuda, M
Iwahori, K
Yamashita, I
Yoshimura, H
机构
[1] Meiji Univ, Tama Ku, Kawasaki, Kanagawa 2148571, Japan
[2] Matsushita Elect Ind Co Ltd, Kyoto 6190237, Japan
关键词
nanoparticle; apoferritin; ferritin; biomineralization; nickel; chromium;
D O I
10.1002/bit.10748
中图分类号
Q81 [生物工程学(生物技术)]; Q93 [微生物学];
学科分类号
071005 ; 0836 ; 090102 ; 100705 ;
摘要
The iron storage protein, apoferritin, has a cavity in which iron is oxidized and stored as a hydrated oxide core. The size of the core is about 7 nm in diameter and is regulated by the cavity size. The cavity can be utilized as a nanoreactor to grow inorganic crystals. We incubated apoferritin in nickel or chromium salt solutions to fabricate hydroxide nanoparticles in the cavity. By using a solution containing dissolved carbon dioxide and by precisely controlling the pH, we succeeded in fabricating nickel and chromium cores. During the hydroxylation process of nickel ions a large portion of the apoferritin precipitated through bulk precipitation of nickel hydroxide. Bulk precipitation was suppressed by adding ammonium ions. However, even in the presence of ammonium ions the core did not form using a degassed solution. We concluded that carbonate ions were indispensable for core formation and that the ammonium ions prevented precipitation in the bulk solution. The optimized condition for nickel core formation was 0.3 mg/ mL horse spleen apoferritin and 5 mM ammonium nickel sulfate in water containing dissolved carbon dioxide. The pH was maintained at 8.65 using two buffer solutions: 150 mM HEPES (pH 7.5) and 195 mIVI CAPSO (pH 9.5) with 20 mM ammonium at 23degreesC. The pH had not changed after 48 h. After 24 h of incubation, all apoferritins remained in the supernatant and all of them had cores. Recombinant L-ferritin showed less precipitation even above a pH of 8.65. A chromium core was formed under the following conditions: 0.1 mg/mL apoferritin, 1 mM ammonium chromium sulfate, 100 mM HEPES (pH 7.5) with a solution containing dissolved carbon dioxide. About 80% of the supernatant apoferritin (0.07 mg/mL) formed a core. In nickel and chromium core formation, carbonate ions would play an important role in accelerating the hydroxylation in the apoferritin cavity compared to the bulk solution outside. (C) 2003 Wiley Periodicals.
引用
收藏
页码:187 / 194
页数:8
相关论文
共 13 条
  • [1] COWAN JA, 1996, INORGANIC BIOCH INTR, P133
  • [2] Calculated electrostatic gradients in recombinant human H-chain ferritin
    Douglas, T
    Ripoll, DR
    [J]. PROTEIN SCIENCE, 1998, 7 (05) : 1083 - 1091
  • [3] Nanophase cobalt oxyhydroxide mineral synthesized within the protein cage of ferritin
    Douglas, T
    Stark, VT
    [J]. INORGANIC CHEMISTRY, 2000, 39 (08) : 1828 - 1830
  • [4] CARBONATE AND BICARBONATE TRACE-METAL COMPLEXES - CRITICAL REEVALUATION OF STABILITY-CONSTANTS
    FOUILLAC, C
    CRIAUD, A
    [J]. GEOCHEMICAL JOURNAL, 1984, 18 (06) : 297 - 303
  • [5] Ferritins: Molecular properties, iron storage function and cellular regulation
    Harrison, PM
    Arosio, P
    [J]. BIOCHIMICA ET BIOPHYSICA ACTA-BIOENERGETICS, 1996, 1275 (03): : 161 - 203
  • [6] THE ROLE OF THE L-CHAIN IN FERRITIN IRON INCORPORATION - STUDIES OF HOME AND HETEROPOLYMERS
    LEVI, S
    SANTAMBROGIO, P
    COZZI, A
    ROVIDA, E
    CORSI, B
    TAMBORINI, E
    SPADA, S
    ALBERTINI, A
    AROSIO, P
    [J]. JOURNAL OF MOLECULAR BIOLOGY, 1994, 238 (05) : 649 - 654
  • [7] MASSOVER WH, 1990, IRON BIOMINERALS
  • [8] RECONSTITUTION OF MANGANESE OXIDE CORES IN HORSE SPLEEN AND RECOMBINANT FERRITINS
    MELDRUM, FC
    DOUGLAS, T
    LEVI, S
    AROSIO, P
    MANN, S
    [J]. JOURNAL OF INORGANIC BIOCHEMISTRY, 1995, 58 (01) : 59 - 68
  • [9] RICE DW, 1983, SPECIAL HORSE SPLEEN, P39
  • [10] Functional properties of threefold and fourfold channels in ferritin deduced from electrostatic calculations
    Takahashi, T
    Kuyucak, S
    [J]. BIOPHYSICAL JOURNAL, 2003, 84 (04) : 2256 - 2263