摘要
Pit nucleation and metastable growth on microelectrodes of aluminium and some Al alloys in chloride solution below the pitting potential are described by recurring current transients. Pit nucleation is a sharp, violent event and is observed repeatedly on all materials tested: pure aluminium, titanium and iron binary aluminium alloys, and alloy 1050A. At the imposed electrode potential, current transients due to pit nucleation recorded for pure aluminium and a solid solution titanium binary alloy are exclusively anodic. Those from alloys containing iron intermetallics sometimes exhibit both anodic and cathodic wings. The cathodic wing is due to transient hydrogen evolution at sites which border iron-rich intermetallic particles: these are preferred pit nucleation sites. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:534 / 539
页数:6
相关论文
共 27 条
[1]   Effect of iron-containing intermetallic particles on the corrosion behaviour of aluminium [J].
Ambat, Rajan ;
Davenport, Alison J. ;
Scamans, Geoff M. ;
Afseth, Andreas .
CORROSION SCIENCE, 2006, 48 (11) :3455-3471
[2]   Nano-scale dissolution phenomena in Al-Cu-Mg alloys [J].
Birbilis, N. ;
Cavanaugh, M. K. ;
Kovarik, L. ;
Buchheit, R. G. .
ELECTROCHEMISTRY COMMUNICATIONS, 2008, 10 (01) :32-37
[3]   Electrochemical characteristics of intermetallic phases in aluminum alloys - An experimental survey and discussion [J].
Birbilis, N ;
Buchheit, RG .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2005, 152 (04) :B140-B151
[4]   MICROSEGREGATION AND TENDENCY FOR PITTING CORROSION IN HIGH-PURITY ALUMINUM [J].
BOND, AP ;
BOLLING, GF ;
DOMIAN, HA ;
BILONI, H .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1966, 113 (08) :773-&
[5]   Investigation of the initiation of localized corrosion on aluminum alloys by using fluorescence microscopy [J].
Büchler, M ;
Watari, T ;
Smyrl, WH .
CORROSION SCIENCE, 2000, 42 (09) :1661-1668
[6]   The effect of temperature on the nucleation of corrosion pits on titanium in Ringer's physiological solution [J].
Burstein, GT ;
Liu, C ;
Souto, RM .
BIOMATERIALS, 2005, 26 (03) :245-256
[7]   THE NUCLEATION AND GROWTH OF CORROSION PITS ON STAINLESS-STEEL [J].
BURSTEIN, GT ;
PISTORIUS, PC ;
MATTIN, SP .
CORROSION SCIENCE, 1993, 35 (1-4) :57-62
[8]   Electrochemical reactions of freshly bared metal surfaces using the fluid impacted guillotined electrode [J].
Burstein, GT ;
Sasaki, K .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2001, 148 (07) :B282-B287
[9]   TRANSPORT PROCESSES AND MECHANISM OF PITTING OF METALS [J].
GALVELE, JR .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1976, 123 (04) :464-474
[10]   Imaging metastable pits on austenitic stainless steel in situ at the open-circuit corrosion potential [J].
González-García, Y ;
Burstein, GT ;
González, S ;
Souto, RM .
ELECTROCHEMISTRY COMMUNICATIONS, 2004, 6 (07) :637-642