Failure of 2.25Cr-1Mo steel superheater tubes in a fluidized bed combustor due to fireside corrosion

被引:25
|
作者
Chandra, K. [1 ]
Kain, Vivekanand [1 ]
Dey, G. K. [1 ]
机构
[1] Bhabha Atom Res Ctr, Div Mat Sci, Bombay 400085, Maharashtra, India
关键词
Failure analysis; 2.25Cr-1Mo steel; Superheater tube; Creep; Oxidation; PERFORMANCE; BOILER;
D O I
10.1016/j.matchar.2010.10.012
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Repeated failures have been observed in a few superheater tubes made of 2.25Cr-1Mo steel at a localized region in a circulating fluidized bed combustion boiler. This paper reports the failure analysis of two affected tubes - the ruptured part of a failed tube and another tube with localized thinning in one region. Both the tubes had grayish, thick and hard deposits of calcium sulphate on the outer diameter surfaces beneath which thick oxide layer was present. A number of intergranular cracks and internal penetration of oxides along the grain boundaries in the base material were observed emanating from the oxides present on the fireside of the tubes. The longitudinal surface adjacent to the failed region showed typical features of intergranular creep. The primary reason of the failure was the continuing thinning of the tubes caused by the alternate cycle of formation of thick calcium sulphate deposit on the fireside of the tubes and its spallation. The spallation of calcium sulphate deposits occurred along with the metal oxide leading to the exposure of the bare material. This caused rapid growth of the less protective outer oxides on the base material. Intergranular creep led to the final rupture of the tube caused by increase in the hoop stress due to the thinning of the tube. (C) 2010 Elsevier Inc. All rights reserved.
引用
收藏
页码:62 / 69
页数:8
相关论文
共 50 条
  • [31] On fatigue-creep damage behaviour of 2.25Cr-1Mo steel
    Xinan Jiaotong Daxue Xuebao, 1 (30-34):
  • [32] Magnetic nondestructive evaluation of thermally degraded 2.25Cr-1Mo steel
    Byeon, JW
    Kwun, SI
    MATERIALS LETTERS, 2004, 58 (1-2) : 94 - 98
  • [33] Degradation evaluation of 2.25Cr-1Mo steel using electrical resistivity
    Nahm, SH
    Kim, JM
    Park, JS
    Yu, KM
    Kim, DK
    Kim, A
    Kim, DJ
    ADVANCES IN NONDESTRUCTIVE EVALUATION, PT 1-3, 2004, 270-273 : 1212 - 1217
  • [34] The influence of prior microstructure on tempering stages in 2.25Cr-1Mo steel
    Parameswaran, P
    Vijayalakshmi, M
    Raghunathan, VS
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2002, 21 (05) : 251 - 267
  • [35] Effect of microstructural features on the hot ductility of 2.25Cr-1Mo steel
    Chen, X. -M.
    Song, S. -H.
    Sun, Z. -C.
    Liu, S. -J.
    Weng, L. -Q.
    Yuan, Z. -X.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (10-11): : 2725 - 2732
  • [36] Young's modulus of a 2.25Cr-1Mo steel at elevated temperature
    Latella, BA
    Humphries, SR
    SCRIPTA MATERIALIA, 2004, 51 (07) : 635 - 639
  • [37] Prediction of welding residual stress in 2.25Cr-1Mo steel pipe
    School of Naval Architecture, Ocean and Civil Eng., Shanghai Jiaotong Univ., Shanghai 200030, China
    不详
    J. Shanghai Jiaotong Univ. Sci., 2006, 1 (77-83):
  • [38] STUDY ON THE HYDROGEN EFFECT ON THE TEMPER EMBRITTLEMENT OF 2.25Cr-1Mo STEEL
    Zhang Xiliang
    Zhou Changyu
    PROCEEDINGS OF THE 18TH INTERNATIONAL CONFERENCE ON NUCLEAR ENGINEERING 2010, VOL 5, 2011, : 179 - 184
  • [39] Microstructural modification in a laser-treated 2.25Cr-1Mo steel
    Rao, RVS
    Parameswaran, P
    Dayal, RK
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2001, 10 (05) : 515 - 520
  • [40] Creep property evaluation of a 2.25Cr-1Mo low alloy steel
    Song, S. -H.
    Wu, J.
    Wei, X. -J.
    Kumar, D.
    Liu, S. -J.
    Weng, L. -Q.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (09): : 2398 - 2403