Microstructure and mechanical behaviour of the isothermally forged Ti-6Al-7Nb alloy

被引:6
作者
Barbosa, PF [1 ]
Button, ST [1 ]
机构
[1] UNICAMP, DEMA,FEM, Sch Mech Engn, Dept Mat Engn,Met Forming Lab, BR-13083970 Campinas, SP, Brazil
关键词
titanium alloys; microstructural changes; isothermal forging;
D O I
10.1243/1464420001544708
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The mechanical properties of the Ti-6Al-7Nb alloy, used to manufacture high-strength prostheses, are highly dependent on its microstructure. This work presents the microstructural changes of this alloy under isothermal hot working. It is shown that the microstructure is strongly affected by the strain rate, temperature and strain. The possible precipitation of intermetallic phases is also evaluated. To define the best processing conditions, compression tests were performed at temperatures varying from 750 to 1030 degreesC and deformation speeds of 0.01, 0.1 and 1 mm/s. Tests were carried out in the (alpha+beta) and beta -phase regions. Experimental results showed that the best microstructure (recrystallized with equiaxial refined white alpha grains and acicular dark grains within a beta -transformed matrix) was obtained in tests at 950 degreesC and 0.01 mm/s.
引用
收藏
页码:23 / 31
页数:9
相关论文
共 21 条
[11]  
Murray J.L., 1987, PHASE DIAGRAM BINARY, P188
[12]   Mechanical properties of biomedical titanium alloys [J].
Niinomi, M .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 243 (1-2) :231-236
[13]  
PRANGNELL PB, 1992, MAT SCI ENG A-STRUCT, V159, P51
[14]   Processing maps for hot working of titanium alloys [J].
Prasad, YVRK ;
Seshacharyulu, T .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1998, 243 (1-2) :82-88
[15]  
RAVEH A, 1983, ADV XRAY ANAL, P25
[16]  
SCHEPP PP, 1990, TITANIUM 1990 PRODUC, P646
[17]  
SCHEY JA, 1987, INTRO MANUFACTURING, P222
[18]  
Semlitsch M., 1987, CLIN MATER, V2, P1, DOI DOI 10.1016/0267-6605(87)90015-1
[19]   JOINT REPLACEMENT COMPONENTS MADE OF HOT-FORGED AND SURFACE-TREATED TI-6AL-7NB ALLOY [J].
SEMLITSCH, MF ;
WEBER, H ;
STREICHER, RM ;
SCHON, R .
BIOMATERIALS, 1992, 13 (11) :781-788
[20]  
Semlitsch MF, 1986, BIOL BIOMECHANICAL P, P69