Effects of artificial aging on microstructure, mechanical properties and stress corrosion cracking of a novel high strength 7A99 Al alloy

被引:60
作者
Hou, Yuzhu [1 ]
Chen, Liang [1 ,2 ]
Li, Zhigang [1 ]
Zhao, Guoqun [1 ]
Zhang, Cunsheng [1 ]
机构
[1] Shandong Univ, Minist Educ, Key Lab Liquid Solid Struct Evolut & Proc Mat, Jinan 250061, Shandong, Peoples R China
[2] Shandong Univ, Suzhou Inst, Suzhou 215123, Jiangsu, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2020年 / 780卷
基金
中国国家自然科学基金;
关键词
7A99; Al; Aging; Precipitation; Mechanical properties; Stress corrosion cracking; MG-CU ALLOY; HEAT-TREATMENT; HOT EXTRUSION; ZR ALLOYS; GP-ZONES; EVOLUTION; PRECIPITATION; BEHAVIOR; PHASES; RESISTANCE;
D O I
10.1016/j.msea.2020.139217
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A recently developed 7A99 Al alloy was subjected to hot extrusion, solid solution and artificial aging. The microstructure evolution and precipitation behavior were examined, and their effects on mechanical properties and stress corrosion cracking were analyzed. The results showed that the coarse Mg(Zn, Cu) 2 phases were broken and refined by hot extrusion. Most of the phases dissolved into Al matrix during solution, and only insoluble Al7Cu2Fe phase was remained. GPI zones and eta' appeared in the under-aged and peak-aged samples. With the extension of aging time, stable. phase with large size formed and became the dominant precipitate in the over-aged sample. It was concluded that the precipitation of 7A99 Al during aging at 150 degrees C followed the sequence of solid solution -> GPI zones -> metastable eta' stable eta. The peak-aged sample owned the high yield and ultimate tensile strength of 588 MPa and 622 MPa, and a low elongation of 10.2%. The under-aged and over-aged samples exhibited relatively lower strength and higher elongations. 2% pre-stretching prior to aging could further improve the tensile properties. Both the under-aged and peak-aged samples were susceptible to the stress corrosion cracking, and the intergranular cracking was observed. In contrary, the over-aged sample showed much better corrosion resistance with a typical ductile fracture, due to the coarsening and separation of grain boundary precipitations.
引用
收藏
页数:14
相关论文
共 46 条
[1]   Microstructure and mechanical properties of a large billet of spray formed Al-Zn-Mg-Cu alloy with high Zn content [J].
Bai Pucun ;
Hou Xiaohu ;
Zhang Xiuyun ;
Zhao Chunwang ;
Xing Yongming .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 508 (1-2) :23-27
[2]   GP-zones in Al-Zn-Mg alloys and their role in artificial aging [J].
Berg, LK ;
Gjonnes, J ;
Hansen, V ;
Li, XZ ;
Knutson-Wedel, M ;
Waterloo, G ;
Schryvers, D ;
Wallenberg, LR .
ACTA MATERIALIA, 2001, 49 (17) :3443-3451
[3]   Dispersoid composition in zirconium containing Al-Zn-Mg-Cu (AA7010) aluminium alloy [J].
Cassell, A. M. ;
Robson, J. D. ;
Race, C. P. ;
Eggeman, A. ;
Hashimoto, T. ;
Besel, M. .
ACTA MATERIALIA, 2019, 169 :135-146
[4]   Microstructures and mechanical properties of age-formed 7050 aluminum alloy [J].
Chen, J. F. ;
Zhen, L. ;
Jiang, J. T. ;
Yang, L. ;
Shao, W. Z. ;
Zhang, B. Y. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 539 :115-123
[5]   Effect of recrystallization and heat treatment on strength and SCC of an Al-Zn-Mg-Cu alloy [J].
Chen, Songyi ;
Chen, Kanghua ;
Dong, Pengxuan ;
Ye, Shengping ;
Huang, Lanping .
JOURNAL OF ALLOYS AND COMPOUNDS, 2013, 581 :705-709
[6]   Enhanced Fatigue Crack Propagation Resistance in an Al-Zn-Mg-Cu Alloy by Retrogression and Reaging Treatment [J].
Chen, Xu ;
Liu, Zhiyi ;
Lin, Mao ;
Ning, Ailin ;
Zeng, Sumin .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2012, 21 (11) :2345-2353
[7]   The effect of Cu on mechanical and precipitation properties of AI-Zn-Mg alloys [J].
Chinh, NQ ;
Lendvai, J ;
Ping, DH ;
Hono, K .
JOURNAL OF ALLOYS AND COMPOUNDS, 2004, 378 (1-2) :52-60
[8]   Effect of hot extrusion and optimal solution treatment on microstructure and properties of spray-formed Al-11.3Zn-2.65Mg-1Cu alloy [J].
Ditta, Allah ;
Wei, Lijun ;
Xu, Yanjin ;
Wu, Sujun .
JOURNAL OF ALLOYS AND COMPOUNDS, 2019, 797 :558-565
[9]   Quantitative metallography of precipitating and secondary phases after strengthening treatment of net shaped casting of Al-Zn-Mg-Cu (7000) alloys [J].
Ghiaasiaan, Reza ;
Amirkhiz, Babak Shalchi ;
Shankar, Sumanth .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 698 :206-217
[10]   Controlled Diffusion Solidification (CDS) of Al-Zn-Mg-Cu (7050): Microstructure, heat treatment and mechanical properties [J].
Ghiaasiaan, Reza ;
Zeng, Xiaochun ;
Shankar, Sumanth .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 594 :260-277