Effect of deformation twinning on dissolution corrosion of 316L stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °C

被引:42
|
作者
Klok, Oksana [1 ,2 ]
Lambrinou, Konstantina [2 ]
Gavrilov, Serguei [2 ]
Stergar, Erich [2 ]
Lim, Jun [2 ]
Van der Donck, Tom [3 ]
Van Renterghem, Wouter [2 ]
De Graeve, Iris [1 ]
机构
[1] VUB, Electrochem & Surface Engn SURF, Pl Laan 2, B-1050 Brussels, Belgium
[2] SCK CEN, Boeretang 200, B-2400 Mol, Belgium
[3] Katholieke Univ Leuven, Dept Mat Engn, Kasteelpk Arenberg 44, B-3001 Leuven, Belgium
关键词
Stainless steel; Plastic deformation; Twinning; De-alloying; Liquid metal corrosion; STACKING-FAULT ENERGY; LONG-TERM CORROSION; AUSTENITIC STEELS; PLASTIC-DEFORMATION; OXYGEN; BEHAVIOR; T91; TEMPERATURES; MECHANISMS; STRENGTH;
D O I
10.1016/j.jnucmat.2018.08.030
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This work addresses the effect of deformation twinning on the dissolution corrosion behaviour of 316 L austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE). For this purpose, plastically deformed 316 L steel specimens with distinctly different deformation twin densities were simultaneously exposed to oxygen-poor (<10(-13) mass%) static liquid LBE for 1000 hat 500 degrees C. The variation in deformation twin density was achieved by loading in uniaxial tension to similar degrees of plastic deformation (8-10%) specimens made of the same 316 L steel heat. Tensile loading was carried out at -150,25 and 150 degrees C so as to affect the twin density, which increased as the temperature of plastic deformation decreased. Dissolution corrosion was the only liquid metal corrosion mechanism observed in the LBE-exposed steel specimens. The thickness of the dissolution-affected zone increased with the deformation twin density, which was highest in the 316 L steel specimen deformed at -150 degrees C and lowest in the one deformed at 150 degrees C. As deformation twin boundaries accelerated the LBE ingress into the steel bulk, their local orientation with respect to the steel specimen surface affected the thickness of the dissolution-affected zone. (C) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:556 / 567
页数:12
相关论文
共 50 条
  • [41] Low-temperature oxy-nitriding of 316 L austenitic stainless steel for improved corrosion resistance in liquid lead-bismuth eutectic
    Chen, Guang
    Wang, Jun
    Zhang, Hongtao
    Li, Longyi
    Fan, Hongyuan
    SCRIPTA MATERIALIA, 2021, 202
  • [42] Insights into the effect of plasma nitriding on corrosion behavior of 304 stainless steel in liquid lead-bismuth eutectic
    Sun, Bihan
    Liu, Sirui
    Xiao, Changquan
    Zhu, Wenjian
    Wang, Da
    Ma, Xianfeng
    MATERIALS CHEMISTRY AND PHYSICS, 2025, 339
  • [43] Growth and Exfoliation Behavior of the Oxide Scale on 316L and T91 in Flowing Liquid Lead-Bismuth Eutectic at 480 °C
    Tian, S. J.
    OXIDATION OF METALS, 2020, 93 (1-2): : 183 - 194
  • [44] Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels
    Wu Xinqiang
    Rong Lijian
    Tan Jibo
    Chen Shenghu
    Hu Xiaofeng
    Zhang Yangpeng
    Zhang Ziyu
    ACTA METALLURGICA SINICA, 2023, 59 (04) : 502 - 512
  • [45] Creep of 316L austenitic steel at 450-550 °C in static lead-bismuth eutectic covered by argon-hydrogen gas
    Yurechko, Mariya
    Skrypnik, Aleksandr
    Wedemeyer, Olaf
    Konys, Jurgen
    Schroer, Carsten
    JOURNAL OF NUCLEAR MATERIALS, 2022, 558
  • [46] Corrosion behavior of Cr coating on ferritic/martensitic steels in liquid lead-bismuth eutectic at 600 °C and 700 °C
    Wang, Li
    Liao, Qing
    Zhang, Jintao
    Liu, Sijie
    Gan, Shuyun
    Wang, Renda
    Ge, Fangfang
    Chen, Liming
    Xu, Shuai
    Polcar, T.
    Daghbouj, N.
    Li, Bingsheng
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 29 : 3958 - 3966
  • [47] Corrosion Behavior of Ti3SiC2 in Flowing Liquid Lead-Bismuth Eutectic at 500 °C
    Lyu, Liangliang
    Qiu, Xi
    Yue, Huifang
    Zhou, Mingyang
    Zhu, Huiping
    MATERIALS, 2022, 15 (21)
  • [48] TWIN ASTIR: First tensile results of T91 and 316L steel after neutron irradiation in contact with liquid lead-bismuth eutectic
    Van den Bosch, J.
    Coen, G.
    Bosch, R. W.
    Almazouzi, A.
    JOURNAL OF NUCLEAR MATERIALS, 2010, 398 (1-3) : 68 - 72
  • [49] Corrosion behavior of 304L stainless steel by wire arc additive manufacturing in liquid lead-bismuth eutectic at 550 °C
    Zhang, Libo
    Wang, Hao
    Zhao, Ke
    Ning, Fangqiang
    Xu, Tianyi
    Liu, Jia
    Yan, Hong
    Zhang, Qiang
    JOURNAL OF NUCLEAR MATERIALS, 2025, 605
  • [50] Corrosion kinetics and mechanisms of 15-15Ti steel in flowing liquid lead-bismuth eutectic at 500°C
    Tian, Shujian
    Zhu, Ge
    Jiang, Zhizhong
    Luo, Lin
    Zhang, Min
    Liu, Jing
    JOURNAL OF NUCLEAR MATERIALS, 2024, 601